Cobalt oxide??
How can I prepare cobalt oxide "CoO" from cobalt II chloride??!!
|
|
Zinc
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 472
Registered: 10-5-2006
Member Is Offline
Mood: No Mood
|
|
I think that you can first make a solution of cobalt II chloride and then precipitate cobalt hydroxide by addition of NaOH. Then heat the hydroxide
until it dehydrates to CoO. I am not sure if this method works.
|
|
not_important
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3873
Registered: 21-7-2006
Member Is Offline
Mood: No Mood
|
|
make the carbonate or basic carbonate, using sodium carbonate or bicarbonate, filtter and wash well, heat to decompose. Overheating in air will
result in the formation of some Co(III) oxide.
|
|
woelen
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7997
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
The problem with all these precipitating alkaline methods is that contamination with cobalt (III) is very hard to avoid. In my experience, cobalt (II)
is EXTREMELY easily oxidized by oxygen from air, as soon as a precipitate is made at high pH, and also in the presence of many ligands. E.g. a
precipitate of Co(OH)2 is oxidized by air in a matter of seconds. Probably the same will happen with carbonate precipitates.
If you want to try the method of precipitating CoCO3, then try with bicarbonate, not with carbonate. But even then, you will have oxidized material. I
once purchased some CoCO3. This was a nice purple powder. Now it is dark brown, and quite a lot of it is oxidized to cobalt (III).
|
|
Dr. Beaker
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 132
Registered: 9-9-2005
Location: between the med red and dead
Member Is Offline
Mood: Shaken, not stirred
|
|
If O2 is such a problem then why not do it under inert conditions!?
|
|
Jome
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 154
Registered: 10-6-2004
Location: Soutwest sweden
Member Is Offline
Mood: desiccated
|
|
Tricky to heat stuff under inert gas. Perhaps try heating it (the carbonate) submerged in molten flux, so that the flux will form a molten layer
protecting it from atmospheric oxygen while it's being heated. To do this, you must find a substance that suits the following criterias:
1. It must be intert
2. It must melt near RT
3. It must stay molten (not boil before 2KK or something)
4. It must be less dense than the carbonate (4.5 ish at least)
Magnesium chloride? Table salt?
Better melt the flux first then add the carbonate.
|
|
not_important
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3873
Registered: 21-7-2006
Member Is Offline
Mood: No Mood
|
|
Tricky finding a flux that isn't going to react with the cobalt carbonate of oxide.
The carbonate does require quite strong heating to effect decomposition. Might be able to heat it in a ceramic tube with a slow flow of N2
This all assumes that you care if you have CoO or some mixed oxide.
|
|
12AX7
Post Harlot
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline
Mood: informative
|
|
Heat it with CO2, and maybe a dash of CO?
But all of this assumes Co(III) IS an intolerable impurity...which given the OP's brevity I would guess not...
Tim
|
|