Any advice on preparing supported catalysts?


I have been reading way too many patents. All of hte latest ones seem to deal with both PTC (sorta gettting dealt with in teh org.chem part) and the use of supported catalysts (MnO2, etc.). I was wondering, does anybody have any suggestions, preferably considered, on how one would go about preparing such catalysts?
View user's profile View All Posts By User
solo
International Hazard
*****




Posts: 3972
Registered: 9-12-2002
Location: Estados Unidos de La Republica Mexicana
Member Is Offline

Mood: ....getting old and drowning in a sea of knowledge

[*] posted on 29-1-2007 at 03:51
Reference Information


Environmentally Friendly Catalytic Methods
James H. Clark and Duncan J. Macquarrie
Chem. Soc. Rev., 1996, 25, 303 - 310

Excerp
..........This review will focus on supported reagent type catalysts based
on porous inorganic support materials, and liquid phase organic
reactions in which they are used.

Attachment: Environmentally friendly catalytic methods.pdf (1.1MB)
This file has been downloaded 876 times





It's better to die on your feet, than live on your knees....Emiliano Zapata.
View user's profile View All Posts By User
Baphomet
Hazard to Others
***




Posts: 211
Registered: 19-11-2006
Member Is Offline

Mood: No Mood

[*] posted on 1-2-2007 at 18:57


hey dude check out this:

http://www.gracedavison.com/davicat/index.htm

the paper about is nice, a good intro to the topic, and this site will help you choose your support using a wizard interface




\"Who ARE you? You\'re like the drummer from REO Speedwagon - nobody knows who you are\" from \'Employee of the Month\'
View user's profile View All Posts By User
Ozone
International Hazard
*****




Posts: 1269
Registered: 28-7-2005
Location: Good Olde USA
Member Is Offline

Mood: Integrated

[*] posted on 1-2-2007 at 21:36


Thanks Baphomet!

That's F'n awesome. I am impressed that the company would go so far!

Cheers,

O3

OTT, use dry substrate under inert atmosphere with *very* pure proto-catalyst reagents; except in *very* special cases, S8 and CO2 are a no-no. Pay special attention to "particle-size reduction" and slurry techniques.




-Anyone who never made a mistake never tried anything new.
--Albert Einstein
View user's profile View All Posts By User
Baphomet
Hazard to Others
***




Posts: 211
Registered: 19-11-2006
Member Is Offline

Mood: No Mood

[*] posted on 4-2-2007 at 22:50


You're welcome :) I hope you find it useful.

If anyone finds a way to make microspheres in the kitchen please let me know :p