Which material is suitable for working with hot H3PO4?
It attacks glass and most metals. Does it attack aluminum or copper?
|
|
Baphomet
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 211
Registered: 19-11-2006
Member Is Offline
Mood: No Mood
|
|
What about a crucible made of a refractory material like Al2O3?
|
|
Organikum
resurrected
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2334
Registered: 12-10-2002
Location: Europe
Member Is Offline
Mood: frustrated
|
|
Teflon. Several kinds of SS steel - the steel once passivied is mostly resistant against the acid.
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
Copper should be OK in the strict absense of oxygen. Aluminium might be a bit violent.
Al2O3 certainly should react, but it might be slow enough not to matter.
Aluminium phosphate is used as a ceramic but I think it might not stand up to the free acid.
|
|
Baphomet
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 211
Registered: 19-11-2006
Member Is Offline
Mood: No Mood
|
|
I like the Aluminium Phosphate idea. Just guessing but would the phosphate ions suppress the donation of protons from the acid due to being the same
as the acid's anion?
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
Actually, I suspect that you would get a whole mess of Al salts with
PO4---
HPO4--
H2PO4-
and lots of other things all of which would reduce the melting point of the AlPO4 untill it all turned into a liqid mess.
OTOH, I have't tried it; just don't try it with anything expensive first.
|
|
BromicAcid
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3237
Registered: 13-7-2003
Location: Wisconsin
Member Is Offline
Mood: Rock n' Roll
|
|
To some extent this question was tackled in the thread on making polyphosphoric acids as dehydrating agents:
http://www.sciencemadness.org/talk/viewthread.php?tid=4409
|
|
Eclectic
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 899
Registered: 14-11-2004
Member Is Offline
Mood: Obsessive
|
|
Well, after reading through the post linked to above, It doesn't look like anyone has actually tested an alumina crucible to see if a surface layer of
AlPO3 forms and protects the rest of the crucible.
Chloric1's breakage was likely due to thermal stress.
|
|