Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Nitrocellulose won't ignite..
Maui3
Hazard to Self
**




Posts: 70
Registered: 9-9-2024
Member Is Offline


[*] posted on 25-10-2024 at 03:52
Nitrocellulose won't ignite..


My nitrocellulose just gets burnt.. I tested the normal cotton too, and this burned quite nicely. I am quite new to energetics, so this might be stupid question, but could it have something to do with the pH being too low or high? I think my nitrocellulose was still quite acidic, even after the washings.. Also, my nitrate salt didn't dissolve in all the sulfruic acid, so there is some nitrate salt of the outside of the cotton, which even after scraping off, still doesn't make the cotton ignite..
View user's profile View All Posts By User
Keras
National Hazard
****




Posts: 942
Registered: 20-8-2018
Location: (48, 2)
Member Is Offline


[*] posted on 25-10-2024 at 05:00


I hope this is not your last post… :/
View user's profile View All Posts By User
fx-991ex
Hazard to Others
***




Posts: 101
Registered: 20-5-2023
Member Is Online


[*] posted on 25-10-2024 at 05:06


Make sure to clean residue correctly, use medium/warm water and work it more.
Also make sure its very completely dry before testing.
View user's profile View All Posts By User
Maui3
Hazard to Self
**




Posts: 70
Registered: 9-9-2024
Member Is Offline


[*] posted on 25-10-2024 at 08:05


Haha! Definitely not my last pos-


.. Thank you fx-991ex for the tips.. Will try!
View user's profile View All Posts By User
Sturge11
Harmless
*




Posts: 18
Registered: 4-9-2019
Member Is Offline


[*] posted on 25-10-2024 at 08:27


Metallica said it best. GASOLINE!
View user's profile View All Posts By User
Laboratory of Liptakov
International Hazard
*****




Posts: 1415
Registered: 2-9-2014
Location: Technion Haifa
Member Is Offline

Mood: old jew

[*] posted on 25-10-2024 at 10:14


Your nitrocellulose is not dry. The looks a like dry between fingers, but isnt. There is about 10 - 15 % water. You set hot airgun on 50 Celsia on 30 minute for 1g NC distance 5 cm.....:cool:



Development of primarily - secondary substances CHP (2015) Lithex (2022) Brightelite (2023) Nitrocelite and KC primer (2024)
View user's profile View All Posts By User
Sir_Gawain
Hazard to Others
***




Posts: 460
Registered: 12-10-2022
Location: [REDACTED]
Member Is Offline

Mood: Stable

[*] posted on 25-10-2024 at 10:20


Could you post some pictures? That might help.
The nitrate salt should dissolve completely. Which nitrate is it?




“Alchemy is trying to turn things yellow; chemistry is trying to avoid things turning yellow.” -Tom deP.
View user's profile Visit user's homepage View All Posts By User

  Go To Top