Sir_Gawain
Hazard to Others
 
Posts: 488
Registered: 12-10-2022
Location: [REDACTED]
Member Is Offline
Mood: Still in 2022
|
|
Bromide in chlorate cell?
I recently constructed a sodium bromate cell and it went much better than I thought it would (video).
I next want to try a sodium chlorate cell, but it seems one of the problems a chlorate cell has that a bromate cell doesn’t is the release of
chlorine.
Would adding a small amount of bromide help prevent this? My idea is that any chlorine produced would immediately react with bromide to form bromine
which would stay in solution. The bromine would react with sodium hydroxide to re-form bromide.
Would this work, or would the bromide all convert to bromate and be useless?
“Alchemy is trying to turn things yellow; chemistry is trying to avoid things turning yellow.” -Tom deP.
|
|
bnull
National Hazard
  
Posts: 569
Registered: 15-1-2024
Location: Home
Member Is Offline
Mood: Sleepy
|
|
Let's see. The chlorine released reacts with bromide to make bromine. Bromine reacts with sodium hydroxide to form bromide and hypobromite.
Hypobromite disproportionates into bromide and bromate. You have a bromide-bromine cycle that converts eventually all bromide to bromate.
What happens when chlorine reacts with bromate?
|
|
Sir_Gawain
Hazard to Others
 
Posts: 488
Registered: 12-10-2022
Location: [REDACTED]
Member Is Offline
Mood: Still in 2022
|
|
That is my main question. My best guess is chloride, bromine, and oxygen, with possibly some chlorate.
“Alchemy is trying to turn things yellow; chemistry is trying to avoid things turning yellow.” -Tom deP.
|
|
yobbo II
National Hazard
  
Posts: 769
Registered: 28-3-2016
Member Is Offline
Mood: No Mood
|
|
According to Woelen here:
https://woelen.homescience.net/science/chem/exps/miniature_c...
bromide will dissolve Ti if using a Ti current runner or Ti is exposed to the liquid.
See near the bottom of the page.
You can make bromate using a lead dioxide anode (and Pt too I suppose).
Bromate from Bromide here:
http://www.chlorates.exrockets.com/further/bromates.pdf
Yob
|
|