Author: Subject: HHO torch to melt gold
Chemgineer
Hazard to Others
***




Posts: 223
Registered: 25-5-2021
Member Is Offline


[*] posted on 1-8-2024 at 16:08
HHO torch to melt gold


I have refined some small amounts of gold and ended up with a precipitate powder.

Do you think one of the Amazon/Ebay HHO hydrogen oxygen torches would work well to melt this into a small bead?
View user's profile View All Posts By User
Sir_Gawain
Hazard to Others
***




Posts: 494
Registered: 12-10-2022
Location: [REDACTED]
Member Is Offline

Mood: Still in 2022

[*] posted on 1-8-2024 at 18:41


I would think so, because I’ve melted copper with a regular propane torch and copper’s melting point is slightly higher than gold.



“Alchemy is trying to turn things yellow; chemistry is trying to avoid things turning yellow.” -Tom deP.
View user's profile Visit user's homepage View All Posts By User
Keras
International Hazard
*****




Posts: 1017
Registered: 20-8-2018
Location: (48, 2)
Member Is Offline


[*] posted on 2-8-2024 at 00:50


Quote: Originally posted by Chemgineer  
I have refined some small amounts of gold and ended up with a precipitate powder.

Do you think one of the Amazon/Ebay HHO hydrogen oxygen torches would work well to melt this into a small bead?


I think NileRed (or NurdRage?) has a video about precipitating gold previously dissolved using aqua regis, and he uses a simple blow torch to do that. Gold powder is rather dull, IIRC. Not the bright shiny yellow colour we’re used to.
View user's profile View All Posts By User
Rainwater
National Hazard
****




Posts: 989
Registered: 22-12-2021
Member Is Offline

Mood: Break'n glass & kick'n a's

[*] posted on 2-8-2024 at 01:07


Mine is a jeweler's torch like this one (picture)HHO torches usually have a smaller flame made for cutting and welding. It will melt gold but not a large amount.
A propane oxygen flame is good. Acetylene oxygen flame is great.

Getting a batch to melt is really about keeping the heat where you want it. If you manage the losses, almost any heat source will work, even the knockoff mapp gas they sell now.




"You can't do that" - challenge accepted
View user's profile View All Posts By User
knowledgevschaos
Harmless
*




Posts: 41
Registered: 9-8-2023
Location: Sci-Hub and the hardware store
Member Is Offline

Mood: Hungry for information

[*] posted on 2-8-2024 at 02:04


With the right setup even a charcoal fire can do it.
Buying an HHO torch might be a waste of money unless you have other plans with it afterwards.