ReconRabbit
Harmless
Posts: 6
Registered: 13-6-2024
Location: NYC
Member Is Offline
|
|
Solution strength for dissolving mineral impurities
Hi all,
A while back I had some rough quartz that I was intending to clean up but it had some soil stains that I couldn't remove with mechanical cleaning. A
rockhounding book I have recommends that muriatic acid be used, but I'm concerned about chlorides forming and staining the white quartz, plus having a
large container of hydrochloric acid is a significant hazard in my home due to the other people living here.
I was hoping I could use an oxidizing solution for this purpose. I have attempted soaking the sample in ~0.1M aq. oxalic acid; it may have been too
weak to have a visible effect. Should I try a stronger solution or a different species? Thanks!
|
|
Texium
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4546
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline
Mood: PhD candidate!
|
|
Oxalic acid can be good at dissolving iron and some other transition metals since it makes water soluble complexes. You might need to use a more
concentrated solution though, and apply some heat. If it doesn’t work, the “dirt” might be composed of more inert silicates, which would likely
not be touched by HCl either.
|
|
RU_KLO
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 175
Registered: 12-10-2022
Location: Argentina
Member Is Offline
|
|
Quote: Originally posted by ReconRabbit ![](images/xpblue/lastpost.gif) | Hi all,
A while back I had some rough quartz that I was intending to clean up but it had some soil stains that I couldn't remove with mechanical cleaning. A
rockhounding book I have recommends that muriatic acid be used, but I'm concerned about chlorides forming and staining the white quartz, plus having a
large container of hydrochloric acid is a significant hazard in my home due to the other people living here. |
Regretfully if you dont know the staining material, then HCl (muriatic acid or maybe Nitric Acid are your best bet. Most chlorides are soluble in
water, so are nitrates.
I think they wont stain your quartz (as soluble material can be washed away)
But I understand the hazzard of having strong acids in your house, and by large container, I think you have a big piece of quartz.)
If the container is in a ventilated area, maybe inside another container. CAREFULLY labeling and advising your family, the risk will be reduced.
HCl and nitric acid are volatille acids, meaning that they will produce some fumes with time, try not to have metal tools nearby or they will get
rusty.
try not to use concentrated acids but diluted. (common muriatic acid is 20% aprox HCL - depends on brands- so diluting by 1 part of acid + 2 parts
water can be use. Heating increases attack time, but should be done outside (because of fumes) and in a glass heating resistant container - not
directly from heat, but in a water bath.
Do not use stainless steel or other material for heating acids.
Go SAFE, because stupidity and bad Luck exist.
|
|
ReconRabbit
Harmless
Posts: 6
Registered: 13-6-2024
Location: NYC
Member Is Offline
|
|
Quote: Originally posted by Texium ![](images/xpblue/lastpost.gif) | Oxalic acid can be good at dissolving iron and some other transition metals since it makes water soluble complexes. You might need to use a more
concentrated solution though, and apply some heat. If it doesn’t work, the “dirt” might be composed of more inert silicates, which would likely
not be touched by HCl either. |
The sample crystal is fairly large (roughly 5x5x6 inches) and as RU_KLO stated it's inadvisable to use a stainless steel heating vessel, so what
works? Wide bottomed beaker? I'd like to go as far as I can without heating, so I'll look for a stronger solution. The stains are the orange-brown
color characteristic of iron deposits around here.
|
|
Rainwater
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 850
Registered: 22-12-2021
Member Is Offline
Mood: indisposition to activity
|
|
If using HCl solution, the reaction can be accelerated with H2O2
This doesn't really help with the hazards involved, as it makes the solution more dangerous, but should allow the job to be completed much sooner.
If your primary stain is metal based, a few drops of HCl applied directly to the sample should produce an immediate result. Informing you if this
method would work.
I have soaking samples in warm sodium bicarbonate solution and removed many organic surfaces stains.
Sulfide stains are the hardest to remove, because they are usually part of the sample.
About 1000mi south of nyc, white quarts is colored by water inclusions in the crystal. Boiling is not recommended as you can end up with sand.
"You can't do that" - challenge accepted
|
|
Deathunter88
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 512
Registered: 20-2-2015
Location: Beijing, China
Member Is Offline
Mood: No Mood
|
|
Just use muratic acid, you likely have more dangerous chemical under the kitchen sink. The new "green" product already comes prediluted to 20% so you
don't even have to worry about fumes anymore.
|
|
bnull
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 280
Registered: 15-1-2024
Location: Between the Atlantic and the Pacific Ocean
Member Is Offline
Mood: Sleepy (again)
|
|
Quote: Originally posted by ReconRabbit ![](images/xpblue/lastpost.gif) | I'm concerned about chlorides forming and staining the white quartz, plus having a large container of hydrochloric acid is a significant hazard in my
home due to the other people living here. |
The only problem I see is health hazard. Chlorides won't be a problem since they are soluble.
If you're still wary or using good old HCl, try citric acid and a toothbrush. Rubber gloves are good but not essential. Make a solution of citric
acid, put it on a cup, and dip the toothbrush every now and then while scrubbing the stains. It is a really boring task but it is safe. And wear an
apron or a dark colored shirt.
It may also happen that the stains are really part of the quartz. I have some small crystals somewhere that are naturally stained.
Edit: A wire brush is even better. Toothbrush...
[Edited on 15-6-2024 by bnull]
Quod scripsi, scripsi.
B. N. Ull
P.S.: Did you know that we have a Library?
|
|
ReconRabbit
Harmless
Posts: 6
Registered: 13-6-2024
Location: NYC
Member Is Offline
|
|
Thanks for the suggestions. I'll get some muriatic from the hardware store and hopefully something HDPE I can use for mixing/combining materials. I'll
also try the citric acid with a wire brush as I have plenty of that.
Edit: It is harder to find muriatic acid than I thought. All of the easily available pool chemicals for chlorinating water are sodium hypochlorite
tablets.
[Edited on 15-6-2024 by ReconRabbit]
|
|
charley1957
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 153
Registered: 18-2-2012
Location: Texas
Member Is Online
Mood: Extracted
|
|
In my part of the US muriatic acid is found in most hardware stores in the paint section and at most lumber yards. I pay about $8 for a gallon of
very clean HCl. It comes in a white container with a yellow label. I believe the name brand is Sunnyside.
You can’t claim you drank all day if you didn’t start early in the morning.
|
|
Twospoons
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1306
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline
Mood: A trace of hope...
|
|
Its frequently used to etch concrete to expose the aggregate. Check that section of your hardware store.
Helicopter: "helico" -> spiral, "pter" -> with wings
|
|
ReconRabbit
Harmless
Posts: 6
Registered: 13-6-2024
Location: NYC
Member Is Offline
|
|
So, after abrading the surface and leaving the rock in a saturated citric acid solution, I didn't see a change. I'll try to find stronger solutions,
but even after checking the section for concrete etchant (I was specifically told that I would find muriatic acid there) the only thing I could find
was urea monohydrochloride.
Someone on another forum recommended "Calcium-Lime-Rust CLR" (Lauric acid). I will report anything that happens using that. The presence of sulfides