Cody's lab: 50lbs Al cans to thermite: pool of liquid Al2O3


https://youtu.be/N9rGAA6eF10

Really funny, he crushed 400 soft drink cans and a small part of it he converts to mid fine Al powder and mixes it with Fe3O4. He puts the thermite mixture (10lbs) on top of a pile of crushed cans and all the crushed cans take part of the reaction and at 17:30 you can see a pool of liquid Al2O3 (and some aluminum). After cooling overnight he gets a chunk of impure iron under the (now frozen) Al2O3 slag.
View user's profile View All Posts By User
Sir_Gawain
Hazard to Others
***




Posts: 317
Registered: 12-10-2022
Location: Due South of Due West
Member Is Offline

Mood: Way less sad

[*] posted on 13-5-2024 at 10:01


Cool video. It’s really interesting how the particle size scales up. There’s probably no limit to the particle size, as long as the reacting mass is large enough.



“Alchemy is trying to turn things yellow; chemistry is trying to avoid things turning yellow.” -Tom deP.