Chemgineer
Hazard to Others
 
Posts: 223
Registered: 25-5-2021
Member Is Offline
|
|
Clean burnt/melted plastic off concrete.
So I have a garden fire to et rid of some stuff, there was evidently some plastic that ended up going on there. When everything was cooled down I've
noticed plastic has melted into the concrete.
I've tried scraping, burning with a torch etc. and it's not perfect.
My next idea is to try some nitric acid since this does terrible things to most plastics!
Any other ideas?
|
|
fx-991ex
Hazard to Others
 
Posts: 109
Registered: 20-5-2023
Member Is Offline
|
|
dissolve with acetone?
|
|
Jenks
Hazard to Others
 
Posts: 163
Registered: 1-12-2019
Member Is Offline
|
|
Maybe it would burn off cleanly if supplied with a stream of oxygen.
|
|
Chemgineer
Hazard to Others
 
Posts: 223
Registered: 25-5-2021
Member Is Offline
|
|
So i've had some success, every now and again I have a suck back incident with my nitric acid and I end up with sulfate contamination.
I know I could distil it but since I have my plastic problem i've poured about 200ml of this onto the concrete where is bubbles and reacts with
something.
It now seems to have much less integrity and I bet a jet wash will be able to lift it now!
**Failing that I suppose thermite might help! lol
[Edited on 20-2-2024 by Chemgineer]
|
|
Sir_Gawain
Hazard to Others
 
Posts: 493
Registered: 12-10-2022
Location: [REDACTED]
Member Is Offline
Mood: Still in 2022
|
|
The nitric acid is probably reacting with the concrete. If any acid gets under the plastic, it should help loosen it by etching the concrete.
“Alchemy is trying to turn things yellow; chemistry is trying to avoid things turning yellow.” -Tom deP.
|
|
Rainwater
National Hazard
  
Posts: 988
Registered: 22-12-2021
Member Is Offline
Mood: Break'n glass & kick'n a's
|
|
I recommend a steal wire brush attached to a drill. Works for unwanted tattoos amd silver nitrate stains
"You can't do that" - challenge accepted
|
|
averageaussie
Hazard to Self

Posts: 93
Registered: 30-4-2023
Location: Right behind you
Member Is Offline
Mood: school
|
|
considering your signature, this is a very concerning statement. care to share the story?
|
|
Rainwater
National Hazard
  
Posts: 988
Registered: 22-12-2021
Member Is Offline
Mood: Break'n glass & kick'n a's
|
|
There was some alcohol and a divorce and a name and an arm. If it works it ant stupid
"You can't do that" - challenge accepted
|
|
averageaussie
Hazard to Self

Posts: 93
Registered: 30-4-2023
Location: Right behind you
Member Is Offline
Mood: school
|
|
arm + angle grinder doesn't seem like the smartest idea...
just because it works doesn't mean there aren't better methods, for all the new guys reading this thinking just because something works, there isn't
another method that not only works better, but is a LOT safer.
if you are going to do something stupid, do it safely please.
|
|
Rainwater
National Hazard
  
Posts: 988
Registered: 22-12-2021
Member Is Offline
Mood: Break'n glass & kick'n a's
|
|
thats why i used a drill, you would have to be
insane to use a grinder. But all jokes aside, it was perty stupid and resulted in scars and infection. Next time ill use more alcohol
"You can't do that" - challenge accepted
|
|
j_sum1
Administrator
      
Posts: 6373
Registered: 4-10-2014
Location: At home
Member Is Offline
Mood: Most of the ducks are in a row
|
|
Quote: Originally posted by Rainwater  | thats why i used a drill, you would have to be
insane to use a grinder. But all jokes aside, it was perty stupid and resulted in scars and infection. Next time ill use more alcohol
|
I might be wrong, but it sounds like too much alcohol may have contributed to the problem in the first place.
|
|
Chemgineer
Hazard to Others
 
Posts: 223
Registered: 25-5-2021
Member Is Offline
|
|
The real issue here is the danger of getting married!
|
|
Rainwater
National Hazard
  
Posts: 988
Registered: 22-12-2021
Member Is Offline
Mood: Break'n glass & kick'n a's
|
|
From experience, if you happen to grind off some surface layers of concrete by accident or to remove discoloration, you can easily and cheaply
resurface that section by making a "patch". mix an equal volume of portland cement and sand to 1/3 but not more than 1/2 that volume of water. Stir
violently until the mix is spreadable. Work time, 10 minutes, set time 90 minutes, walk time 12 hours. For non driveable areas, 1/2 the portland
cement is needed
"You can't do that" - challenge accepted
|
|