Planetary Ball mill gear sizes?
Ball mills are bloody expensive, so I'm working on making one I can 3D print.
however, I noticed many papers just give an rpm figure without further context, which means I have to get the gearing the same as professional
machines, the paper I'm currently interested in uses a Retsch PM100 (which seems to be a pretty common unit) anyone know the gearing
ratio's/measurements? the only size I can find is that of the sun gear (141mm) anyone know the other dimensions?
![](https://i.ibb.co/x6Kr48d/Ball-mill-gears.png)
any other input would be greatly appreciated. (or if you have questions on how I plan to do certain things, feel free to ask)
Cheers.
|
|
charley1957
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 155
Registered: 18-2-2012
Location: Texas
Member Is Offline
Mood: Extracted
|
|
Don’t know how big your mill is going to be but it’s really simple to drive the canister with a belt or rubber strap or band with just the shaft
of a motor, giving you lots of speed reduction and not having to create a gearbox. It won’t be as durable as a gearbox but there’s a lot of
utility in simplicity.
You can’t claim you drank all day if you didn’t start early in the morning.
|
|
NickBlackDIN
Harmless
Posts: 10
Registered: 10-5-2023
Member Is Offline
|
|
I think you may have been mistaken Charley, this isn't a rock polisher, the gearbox is to increase the simulated G-forces applied to the milling
media. (in my build there will be 3 canisters, each attached to one of the planet gears)
this picture I think does a decent job explaining it:
![](https://i.ibb.co/Bj1ZkGt/a-High-energy-milling-machine-b-planetary-ball-milling-and-c-pulverized-kaolin.png)
[Edited on 14-5-2023 by NickBlackDIN]
Edit #2:
Looking at some videos, and getting some more information, there isn't actually a sun gear in the traditional sense, looks like a plate with bearings
that roll the planet gears against the outer gear (at a ratio of 1:-2)
That basically gives me all the info I need.
[Edited on 15-5-2023 by NickBlackDIN]
|
|
Rainwater
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 870
Registered: 22-12-2021
Member Is Offline
Mood: indisposition to activity
|
|
Brilliant design. I never thought of anything like that. I always used a horizontal canister and relied on gravity/rotational speed to produce the
waterfall of sample/media. This makes gravity the limiting factor, as once your sample is exposed to a rotational force of 1G, it will no longer fall.
Note sure what a perfect value would be for any given grinding operation(i set mine by ear).
With the planetary gear configuration, your have removed gravity from the equation and replaced it with the gforce generated by the orbital of the
planet gears.
What will be of great importance( as its the only parameter you can control) is the ratio between planetary orbit rpm vs planetary rpm. PO and P for
short
If the radius of the planet(container) is properly matched to the radius of the planetary gear orbit radius, you will be able to maintain a linear G
Force ratio across a wide range of rpm's
Gforce within a circle can be calculated with this equation
1.118x10-4x R x (RPM)² = Gforce
R is in millimeters.
Just guessing but a PO/P ratio between .5~.75 should produce a waterfall effect inside the container.
"You can't do that" - challenge accepted
|
|
Sulaiman
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3634
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline
|
|
Nice idea but is it practical?
The rotating assembly will need to spin quite quickly to allow tumbling within the grinding cylinders so the balance of the two cylinders will be
important to minimise wear.
I can see the benefit
but is the complexity worth the time saved compared to a typical horizontal arrangement?
For commercial/professional use, time is money, so probably yes,
but for amateur use I guess not.
CAUTION : Hobby Chemist, not Professional or even Amateur
|
|
NickBlackDIN
Harmless
Posts: 10
Registered: 10-5-2023
Member Is Offline
|
|
Rainwater: spot on explanation!
I sure hope your guess is correct with the PO/P ratio range, since that is exactly what I'm aiming for myself :p (unless I can get more precise
numbers)
Sulaiman:
Not sure if it's practical or not, it's needed.
I'm using 3 cylinders to make balancing easier. Using very small canisters to decrease wear (less weight being slinged around)
Yes, the complexity is necessary. Not nearly enough force in the rock tumbler arrangement. (The chemicals won't bond properly otherwise, the other
option is very high pressure & temperature, which I hate doing, this is safer)
Edit: I should probably mention I'm making Na2S-P2S5 (solid electrolyte for an sodium ion battery)
[Edited on 15-5-2023 by NickBlackDIN]
|
|
Rainwater
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 870
Registered: 22-12-2021
Member Is Offline
Mood: indisposition to activity
|
|
excel calculator
Code: | R1 in mm 152.4
R1 RPM 30
R2 in mm 50.8
R2 RPM 45
cylinder orbit force = 15.334488 Gs
cylinder rotation force = 11.500866 Gs
total g force = 26.835354
ratio 0.75 |
Attachment: gforce.xlsx (9kB) This file has been downloaded 177 times
So lets say the containers are 1ft apart and 4in wide.
The orbit at 0.5Hz or 30rpm
And the containers are spinning at 1.33Hz or 45rpm
Now lets sat that the weight of 1 container is 1000 grams total (2.2lbs)
The container will, at its extreme, be experiencing and exerting about 26.8 kilos of force(59lbs).
The media/sample will be experiencing a force thats a function of D2 and rpm.
It will be less that the 15.3 g's listed above.
The equivalent would be about the same as using a griending media that weights 15x what your using now without increasing its volume..
Gonna need some heavy steal and a ballast system, or that thing will shake your building apart
Edit:
https://github.com/chrisspen/gears
Here is a link i used when i was making different gears, which will require a lot of fine tuning and experimentation
When 3d printing a planetary gears, I find it useful to mark the top of the gears with arrows so you can install them correctly.
Also, post processing in hot salt is a must to maximize plastic strength.
I recommend the Herringbone gears for high torque applications
Edit #2
Quote: | unless I can get more precise numbers |
The term "critical speed" or CS is what you need to google. Its basicly the speed at which the gravitational forced approaches the centrifugal force
and the media stops falling. Lots of math, there is a sweet spot at 68% of CS that most manufacturers recommend the mill operates at. Not sure how to
calculate it, but it is a function of the equation I quoted above.
[Edited on 16-5-2023 by Rainwater]
[Edited on 16-5-2023 by Rainwater]
"You can't do that" - challenge accepted
|
|
NickBlackDIN
Harmless
Posts: 10
Registered: 10-5-2023
Member Is Offline
|
|
Thank you very much Rain!
with your help I found this link, which includes the formula I need (all I need to do is change the g constant to whatever G force I'll be running at)
That gear generator is the same one I was planning to use, thank you!
and I appreciate the sample math as well =D
unfortunately I cant do much till Friday. but having this to think about will make work more enjoyable ^.^
Thank you.
|
|
charley1957
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 155
Registered: 18-2-2012
Location: Texas
Member Is Offline
Mood: Extracted
|
|
Okay I get it now. That's a whole different animal. It increases the G force for quicker and/or more efficient milling. Well I hope you can get it
worked out. I’m a huge fan of DIY to make something work well without having to spend a lot of money on it. Best of luck, and I’ll follow your
posts on it.
You can’t claim you drank all day if you didn’t start early in the morning.
|
|
Fulmen
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1702
Registered: 24-9-2005
Member Is Offline
Mood: Bored
|
|
Very interesting idea. It's comparable to a "ring and puck mill"
We're not banging rocks together here. We know how to put a man back together.
|
|
Texium
|
Thread Moved 30-11-2023 at 10:57 |
alexwoo10
Harmless
Posts: 4
Registered: 20-11-2023
Member Is Offline
|
|
Please send the stl files for this project
|
|