So attempted the transformation above.

First step is to neutralise p-Tosyl acid into sodium p-Tosylate. Easily peasy, used ¼ mole (~ 50 g) of p-Tosyl acid. 100 mL seems to be enough to dissolve it. Just drop in the right amount of sodium hydroxide. Boil the solution. Get Na p-Tosylate.

Next step is caustic fusion with potassium hydroxide. That’s where it gets critical. There is information available, but it is not really detailed as to how run the reaction. I mixed KOH and Na p-Tosylate in a stainless steel pot and put it on a gas burner. My reference says ½ hour at 360 °C when the molar ratio of KOH to Na p-Tosylate is 2.5:1 should result in 70% yield.

Not really what I got. It seems KOH must be fused first and only then p-Tosylate added piecemeal. Why? Because p-Tosylate will darken and get tarry as the crucible heats. TBH, it was only when I got at the end of the half-hour that the mix began to liquify, and it was already very brown, almost black because of what I assume p-Tosylate decomposition. I stopped there lest I got only charred products. Apparently, nothing takes place before the mix is liquid, so this first try resulted in an infinitesimal yield.

There is a characteristic smell of phenol escaping from the pot, though.

The cake is cooled, transferred to a beaker of water, neutralised with HCl to revert any super-soluble p-cresolate to less but still soluble p-cresol, filtered. I got only tarry residues on the frit, so I attempted a liquid-liquid extraction with toluene, followed by boiling away the toluene with added chips of activated charcoal. It wasn't completely unsuccessful, as I was left with a small amount of a dark brown liquid which strongly smells like phenol, so it is definitely there, and in principle, this is working (needless to say, the result is so impure it didn't solidify as it should have).

I have one question, though. Reaction is supposed to be conducted at 360 °C but p-cresol b.p. is lower, 200 °C. Unless by using a distillation apparatus – which, by the way, the authors in the paper I quoted didn't seem to do – how can the yield be significant?
View user's profile View All Posts By User
Tsjerk
International Hazard
*****




Posts: 3028
Registered: 20-4-2005
Location: Netherlands
Member Is Offline

Mood: Mood

[*] posted on 11-10-2022 at 21:20


About the question: the phenol also forms a sodium/potassium salt which doesn't boil. Did you acidify the product?
View user's profile View All Posts By User
Keras
National Hazard
****




Posts: 864
Registered: 20-8-2018
Location: (48, 2)
Member Is Offline


[*] posted on 11-10-2022 at 22:21


Quote: Originally posted by Tsjerk  
About the question: the phenol also forms a sodium/potassium salt which doesn't boil. Did you acidify the product?


Yes I did. At least, I neutralised the excess of potash using HCl until the pH was neutral. I reasoned that going further would serve no purpose, since the pKa of cresol is around 10, like phenol's. Maybe I should’ve gone all the way to pH ~ 2.

Cresol is surprisingly soluble in water, like 2 g / 100 mL, which can seem really little (and is markedly less than phenol), but since I had 600 mL of water, that makes an appreciable 12 g.

I perused the paper I had and found out I overlooked the passage describing the experimental conditions. Indeed, Na p-Tosylate must be added to the already molten potash. Will do that next time.
View user's profile View All Posts By User
Keras
National Hazard
****




Posts: 864
Registered: 20-8-2018
Location: (48, 2)
Member Is Offline


[*] posted on 6-4-2023 at 08:58


So, I’m back with this thread.

I retried today this experiment on the back of an enveloppe. I also wanted to verify that NaOH can be used, since some sources claim that NaOH without extra KOH won’t react.

To be honest, the starting material is NOT TsOH but TsNa, so the first step is to dissolve TsOH in water, neutralise it with sodium hydroxide, and boil the water off to get solid TsNa. TsNa is well behaved, it will form a nice free flowing powder, very few clumping after evaporating the last traces of water.

So, I decided to use 50 mmol of TsNa (~ 9.7 g). Since the paper I have indicates that the best yields are obtained when NaOH is in a 2.5::1 excess ratio, I put 5 g (125 mmol) of NaOH in a crucible, and the crucible in a heating mantle which was set for 400 °C (taking into account that the crucible didn't touch the mantle, I had to make allowances for reduced thermal efficiency). When the sodium hydroxide was melted, I added the TsNa in four portions. The crucible was capped and the mix stirred every ten minutes, for a total duration of 35 mn. After the last addition of TsNa, the mixture is pasty, but not solid, it’s quite easy to stir. It was a bit frothy at 10 minutes, but whatever gaseous emission happened rapidly subsided. Some vapours of TsNa or cresol escaped each time the crucible was uncapped, but it was really manageable (it doesn’t fume like crazy). After 20 minutes, the mixture began to darken, and it was quite dark at 30 and 35 min when I turned the heating mantle off and let everything cool.

Once cold, the mixture is a dark solid, but doesn’t really stick to the walls of crucible too much, so it’s easy to scrape off. It is very soluble in water, so the best way to remove it is probably to simply add water in the crucible and stir until everything has dissolved.

The dark solution thus obtained was acidified with HCl. There is, at start, a huge bubbling of what appears to be SO₂, so there has definitely be formation of sodium sulphite. Judging by the quantity of HCl I had to add to neutralise the solution, there was quite a bit of it, which is a good sign. At the end, I was left with a dark brown solution full of small particles (precipitate of cresol)? Unfortunately, I had no equipment to either filter or distill, so after having smelt a strong (but not unpleasant to me) smell of phenol (which p-cresol is supposed to smell), I simply discarded the solution :/

To wrap up, caustic fusion of TsNa with NaOH to form cresol seems to work. I’m going to repeat the experiment Saturday in my lab, and will try to get a decent product out of it.
View user's profile View All Posts By User
Texium
Administrator
********




Posts: 4554
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline

Mood: PhD candidate!

[*] posted on 6-4-2023 at 09:44


Nice. Minor critique though: you should write TsONa or NaOTs, not TsNa, cause Ts means tosyl, not tosylate. And why did you throw out the crude solution? Seems like a waste when that could have instead been combined with the crude from your next run.



Come check out the Official Sciencemadness Wiki
They're not really active right now, but here's my YouTube channel and my blog.
View user's profile Visit user's homepage View All Posts By User
Keras
National Hazard
****




Posts: 864
Registered: 20-8-2018
Location: (48, 2)
Member Is Offline


[*] posted on 6-4-2023 at 10:24


Quote: Originally posted by Texium  
Nice. Minor critique though: you should write TsONa or NaOTs, not TsNa, cause Ts means tosyl, not tosylate. And why did you throw out the crude solution? Seems like a waste when that could have instead been combined with the crude from your next run.


Err… Your definitely right, somehow I had imagined that with neutralisation the whole -OH group was taken off :p :p Talk about being dense.

You’re right (again!). I should’ve kept it. As a matter of fact, I botched the end. I waited a while for the particles to settle down and then I intended to get rid of the supernatant water, but I tilted the beaker too much and a lot went down the drain before I even realised it did. After that, I was left with a thin layer mostly black tar (with a strong odour of phenol) that I tried to recrystallise. I heated the beaker up to 50 °C and then let it cool, and indeed I got a few crystals of a whitish substance floating on the tar. But there was only milligrams of it, so I poured everything to the bin. It was just a proof of concept, so to speak.

This weekend, I’ll steam distill the result, since apparently cresol can be steam distilled out of solution.




[Edited on 6-4-2023 by Keras]
View user's profile View All Posts By User
Keras
National Hazard
****




Posts: 864
Registered: 20-8-2018
Location: (48, 2)
Member Is Offline


[*] posted on 24-4-2023 at 12:50


So, third time is a charm, so they say.

Starting materials : ~ 19 g of TsONa ( ← This time I got it right :p) = 100 mmol
~ 14 g of KOH representing 250 mmol, that is a 2.5::1 excess over TsONa, which is apparently the ratio that maximises the yield.

KOH is loaded in a small earthenware crucible (50 mL), but a larger one in metal would probably be better suited (I’m actually waiting for a 75 mL one in stainless steel). The crucible is capped and put into a heating mantle which is set for 400 °C (given that the crucible doesn’t fit exactly the walls of the heating mantle). To maximise the heat efficiency, the heating mantle is covered with aluminium foil.

When KOH has all melted, the temperature is sampled using an infrared thermometer and found around 320 °C. At this point, TsONa is added in small portion with ⅔ min between each addition to allow for the mixture to regain its fluidity. After the final addition, a timer is set to 30 min.

After a few minutes, a characteristic sizzle is heard and the mixture begins to froth. I’m not sure what gas is released. Possibly this is the water contained in the KOH crystals, though no water wisps escape. At this point, the crucible must be open every two to three minutes and the mixture stirred (which result in instant collapse of the frothing matter). The colour, initially yellow/orange, progressively darkens as the reaction progresses.

After about 20 minutes, the frothing dies down and quickly after the mixture turns blackish. At that point, when the lid is open, white vapours of what I assume is boiling cresol escape. The quantity of released vapours increases with time.

At 30 min, the mixture has definitely assumed a pitch black colour and is more fluid than it is before. The heating is stopped, the crucible is removed and the mixture is transferred while hot to a stainless steel cup (ashtray like) and left to cool. Meanwhile 120 mL of water is heated to boiling. When the mixture has cooled enough, the hot water is added to the stainless steel cup in two portions and the solution is transferred to a beaker. Normally, all the mixture dissolves. Even the tar seems water soluble, which eases up later cleaning of the crucible (no organic solvant needed, soap works well with a light abrasive sponge).

The pH is tested and found (of course) to be very alkaline (≥ 14). 23% hydrochloric acid is added until the pH turns neutral. At this time, nothing much happens. HCl continues to be added piecemeal, resulting in bubbling and release of sulphur dioxide (from decomposition of the sulphurous acid created along with KCl and NaCl). Addition of HCl is stopped when this bubbling dies down.

The resulting solution, which is now strongly acidic, is transferred to a 250 mL round bottom flask and set for steam distillation (don’t forget the boiling chips, it bumps a lot).

The first drops of water collected are undoubtedly milky and soon seen to be yellowish. When enough has passed, the liquid collected separates into a yellow lower organic layer covered in milky water. All along, sulphur dioxide escapes, so it is important to work outside or in a well ventilated area.

The steam distillation is stopped when the drops of water collected are clear, containing no more cresol.

Owning to the slight difference in density between cresol (d = 1.03) and water (d = 1), the cloudy water does not readily separate. I had to put the solution to rest overnight to get a clear separation of both phases. The upper aqueous layer, still a bit cloudy, is saturated with table salt and transferred to a sep funnel and the lower layer, with as few as possible of remaining water, is put aside.

The aqueous layer is extracted three times with 10 mL of toluene. The third extraction results in a perfectly clear aqueous layer. The toluene fractions are collected and combined with the yellow organic layer from the steam distillation. The aqueous layer is discarded, and the organic layer returned to the round bottom flask for another distillation.

This second distillation conducted around 150 °C results first in the azeotrope water/toluene passing through at around 78/80 °C, followed by the rest of the toluene at around 110 °C. Using excess toluene over water allows for the compound to be dried off during the distillation (no CaCl step is needed). Once the 30 mL of toluene have been recovered, the distillation is stopped, and the liquid still present in the flask is transferred to a small beaker (unfortunately, I had an insulation problem with my heating mantle at this point that made the RCD go off).

The toluene/water mix collected clears up with a few minutes, resulting in two very nice phases. I saved the toluene fraction for further use as entrainer. Salt crystals stick to the RBF walls, part from the initial HCl addition and most from the saturation step.

The (what I assume to be) liquid p-cresol collected from the RBF weighs 7.6 g, which, given that M ~ 108 g/mol, translates to around 70 mmol or 70% yield, which is not bad given the published figures. However, although it has a smell strongly redolent of phenol, the product is (slightly?) impure: it is not yellow but somewhat creamy in colour, and doesn’t crystallise at 35 °C as expected. In fact, I had to put it in the freezer to have it solidify, and when taken back to room temperature, it quickly remelted. So a further distillation, possibly under reduced pressure, should be attempted, if I can fix my heating mantle.

I will post some pictures tomorrow.
View user's profile View All Posts By User
Keras
National Hazard
****




Posts: 864
Registered: 20-8-2018
Location: (48, 2)
Member Is Offline


[*] posted on 7-5-2023 at 22:42


Further follow-up.

I redistilled the result yesterday. Except for a tiny forerun corresponding to a very small amount of water, most of the product passed as a clear liquid at 192 °C. I was left with a minute amount of tar in the flask.

Few problems though:

1. 192 °C is not the expected temperature for p-cresol but o-cresol.
2. The product won’t cristallise at r.t. as expected.

So either p-cresol shows significant supercooling, or it is not what it is expected to be (maybe a mix between o- and p-cresols?)

IMG_1344.jpeg - 364kBIMG_1346.jpeg - 1.3MBIMG_1348.jpeg - 988kBIMG_1347.jpeg - 832kB
View user's profile View All Posts By User
ErgoloidMesylate
Banned
**




Posts: 89
Registered: 8-8-2022
Location: Norad
Member Is Offline

Mood: Freedom of thought is priceless - You can't afford it

[*] posted on 8-5-2023 at 09:05


Quote: Originally posted by Keras  
So, third time is a charm, so they say.

When KOH has all melted, the temperature is sampled using an infrared thermometer and found around 320 °C. At this point, TsONa is added in small portion with ⅔ min between each addition to allow for the mixture to regain its fluidity. After the final addition, a timer is set to 30 min.

After a few minutes, a characteristic sizzle is heard and the mixture begins to froth. I’m not sure what gas is released. Possibly this is the water contained in the KOH crystals, though no water wisps escape. At this point, the crucible must be open every two to three minutes and the mixture stirred (which result in instant collapse of the frothing matter). The colour, initially yellow/orange, progressively darkens as the reaction progresses.

After about 20 minutes, the frothing dies down and quickly after the mixture turns blackish. At that point, when the lid is open, white vapours of what I assume is boiling cresol escape. The quantity of released vapours increases with time.



I will post some pictures tomorrow.


Some old 1800s style chemistry.
This source says your gas is hydrogen:

http://www.orgsyn.org/demo.aspx?prep=CV1P0175

They presume they started with the correct isomers.




Cannula transfer and cannula filtering is used for lysergic synth Compressed air and remove co2
View user's profile View All Posts By User
ErgoloidMesylate
Banned
**




Posts: 89
Registered: 8-8-2022
Location: Norad
Member Is Offline

Mood: Freedom of thought is priceless - You can't afford it

[*] posted on 8-5-2023 at 09:19


Quote: Originally posted by Texium  
Nice. Minor critique though: you should write TsONa or NaOTs, not TsNa, cause Ts means tosyl, not tosylate. And why did you throw out the crude solution? Seems like a waste when that could have instead been combined with the crude from your next run.


Looks like this guy did some experiments on this topic:

http://www.sciencemadness.org/talk/viewthread.php?tid=15522#...

He got some of his equipment from "Dr" Bob (the guy who makes a ton of typos) but he doesn't seem to post here or make videos anymore.





Cannula transfer and cannula filtering is used for lysergic synth Compressed air and remove co2
View user's profile View All Posts By User
clearly_not_atara
International Hazard
*****




Posts: 2752
Registered: 3-11-2013
Member Is Offline

Mood: Big

[*] posted on 8-5-2023 at 16:41


The balanced reaction does evolve hydrogen:

PhSO3Na + 2 KOH >> KSO3Na + PhOK + H2

EDIT: no lol, idkwtf

[Edited on 9-5-2023 by clearly_not_atara]




Quote: Originally posted by bnull  
you can always buy new equipment but can't buy new fingers.
View user's profile View All Posts By User
Keras
National Hazard
****




Posts: 864
Registered: 20-8-2018
Location: (48, 2)
Member Is Offline


[*] posted on 9-5-2023 at 00:24


Quote: Originally posted by clearly_not_atara  
The balanced reaction does evolve hydrogen:

PhSO3Na + 2 KOH >> KSO3Na + PhOK + H2


You’re missing an oxygen atom on the right, if I’m not mistaken.
View user's profile View All Posts By User
Keras
National Hazard
****




Posts: 864
Registered: 20-8-2018
Location: (48, 2)
Member Is Offline


[*] posted on 9-5-2023 at 01:26


Quote: Originally posted by ErgoloidMesylate  


Looks like this guy did some experiments on this topic:

http://www.sciencemadness.org/talk/viewthread.php?tid=15522#...



You mean synthesising p-toluene sulphonic acid? Nurdrage has a video on this, it is fairly easy to do given you have a Dean-Stark apparatus available. Separating o- from p- isomers is probably a bit more tricky, though. He didn't attempted it.

But that’s irrelevant to me since I started from commercial p-TsOH (cheap, because TsOH is used for saccharin synthesis). It was slightly rosy, which I attribute to Fe³⁺ contamination. Matter of fact, when neutralising the acid with lye, past the neutral point I got a small amount of red flakes with I think is ferric hydroxide that was filtered out, living a clear solution (see picture below, the colour difference between the funnel and the erlenmeyer is quite dramatic. The purple colour is caused by micrograms of phenolphtalein I added to aid in the neutralisation).

IMG_1249.jpeg - 119kB
View user's profile View All Posts By User
clearly_not_atara
International Hazard
*****




Posts: 2752
Registered: 3-11-2013
Member Is Offline

Mood: Big

[*] posted on 9-5-2023 at 08:29


Quote: Originally posted by Keras  
Quote: Originally posted by clearly_not_atara  
The balanced reaction does evolve hydrogen:

PhSO3Na + 2 KOH >> KSO3Na + PhOK + H2


You’re missing an oxygen atom on the right, if I’m not mistaken.

You're not.

By the Pourbaix diagram, sulfite is unstable. Maybe that's where the hydrogen comes from? What a strange phenomenon.




Quote: Originally posted by bnull  
you can always buy new equipment but can't buy new fingers.
View user's profile View All Posts By User
Keras
National Hazard
****




Posts: 864
Registered: 20-8-2018
Location: (48, 2)
Member Is Offline


[*] posted on 9-5-2023 at 10:52


Quote: Originally posted by clearly_not_atara  

By the Pourbaix diagram, sulfite is unstable. Maybe that's where the hydrogen comes from? What a strange phenomenon.


There’s definitely sulphite in the final product, since SO₂ escapes during neutralisation and steam distillation.

Your equation clearly shows that water is produced, so that would explain the frothing, IMHO.

Now, why is there hydrogen emitted at the end? Probably some sort of further attack of molten KOH (in excess) on the final product?
View user's profile View All Posts By User
ErgoloidMesylate
Banned
**




Posts: 89
Registered: 8-8-2022
Location: Norad
Member Is Offline

Mood: Freedom of thought is priceless - You can't afford it

[*] posted on 9-5-2023 at 15:32


Quote: Originally posted by Keras  
Quote: Originally posted by ErgoloidMesylate  


Looks like this guy did some experiments on this topic:




I started from commercial p-TsOH (cheap, because TsOH is used for saccharin synthesis).



If you are going to use stuff from industry sources, have you looked at the p-toluidine synthesis? I think it could be useful if you want to take a look.
I think it uses sodium nitrite and urea.




Cannula transfer and cannula filtering is used for lysergic synth Compressed air and remove co2
View user's profile View All Posts By User
ErgoloidMesylate
Banned
**




Posts: 89
Registered: 8-8-2022
Location: Norad
Member Is Offline

Mood: Freedom of thought is priceless - You can't afford it

[*] posted on 9-5-2023 at 16:28


Quote: Originally posted by ErgoloidMesylate  
Quote: Originally posted by Keras  
Quote: Originally posted by ErgoloidMesylate  


Looks like this guy did some experiments on this topic:




I started from commercial p-TsOH (cheap, because TsOH is used for saccharin synthesis).



If you are going to use stuff from industry sources, have you looked at the p-toluidine synthesis? I think it could be useful if you want to take a look.
I think it uses sodium nitrite and urea.


Just ignore the brominated portion for example:

http://orgsyn.org/demo.aspx?prep=CV3P0130




Cannula transfer and cannula filtering is used for lysergic synth Compressed air and remove co2
View user's profile View All Posts By User
Keras
National Hazard
****




Posts: 864
Registered: 20-8-2018
Location: (48, 2)
Member Is Offline


[*] posted on 9-5-2023 at 22:42


Quote: Originally posted by ErgoloidMesylate  

If you are going to use stuff from industry sources, have you looked at the p-toluidine synthesis? I think it could be useful if you want to take a look.
I think it uses sodium nitrite and urea.


Will definitely have a look, but my final goal is not p-toluidine, but anisaldehyde (p-cresol → p-methoxytoluene → p-methoxybenzaldehyde).
View user's profile View All Posts By User
ErgoloidMesylate
Banned
**




Posts: 89
Registered: 8-8-2022
Location: Norad
Member Is Offline

Mood: Freedom of thought is priceless - You can't afford it

[*] posted on 10-5-2023 at 05:53


Quote: Originally posted by Keras  
Quote: Originally posted by ErgoloidMesylate  

If you are going to use stuff from industry sources, have you looked at the p-toluidine synthesis? I think it could be useful if you want to take a look.
I think it uses sodium nitrite and urea.


Will definitely have a look, but my final goal is not p-toluidine


No shit, that would be the starting precursor, are you less than bright?

Most would try for 3,4,5 methoxy aldehyde, but i digress.

Note to you personally: being brainless won't benefit yourself.




Cannula transfer and cannula filtering is used for lysergic synth Compressed air and remove co2
View user's profile View All Posts By User
Keras
National Hazard
****




Posts: 864
Registered: 20-8-2018
Location: (48, 2)
Member Is Offline


[*] posted on 10-5-2023 at 06:32


Quote: Originally posted by ErgoloidMesylate  

No shit, that would be the starting precursor, are you less than bright?


Lol, right. But p-toluidine to anisaldehyde???

Quote:

Note to you personally: being brainless won't benefit yourself.

I try to cope with the few neurones I’m left with :p

[Edited on 10-5-2023 by Keras]
View user's profile View All Posts By User
ErgoloidMesylate
Banned
**




Posts: 89
Registered: 8-8-2022
Location: Norad
Member Is Offline

Mood: Freedom of thought is priceless - You can't afford it

[*] posted on 10-5-2023 at 08:42


Quote: Originally posted by Keras  


Lol, right. But p-toluidine to anisaldehyde???



http://orgsyn.org/demo.aspx?prep=CV3P0130

Are you going to use the cobalt method at that point?

https://drive.google.com/file/d/1xGiV4FJO_pWh3gYv8fQwa4AED-j...

[Edited on 10-5-2023 by ErgoloidMesylate]




Cannula transfer and cannula filtering is used for lysergic synth Compressed air and remove co2
View user's profile View All Posts By User
Keras
National Hazard
****




Posts: 864
Registered: 20-8-2018
Location: (48, 2)
Member Is Offline


[*] posted on 11-5-2023 at 00:11


Quote: Originally posted by ErgoloidMesylate  

http://orgsyn.org/demo.aspx?prep=CV3P0130

Are you going to use the cobalt method at that point?

https://drive.google.com/file/d/1xGiV4FJO_pWh3gYv8fQwa4AED-j...
[Edited on 10-5-2023 by ErgoloidMesylate]


I mean, yes, I could start from p-toluidine, diazotise it and hydrolise it to p-cresol, but I don’t see the point. Either I start from p-toluenesulphonic acid which is cheap and of which I have a couple hundred grams, or I buy p-cresol directly. :p

I had forgotten about that cobalt method, although I've recently bought some cobalt chloride. I was planning to use the Étard reaction with chromyl chloride to oxide the methyl group to aldehyde. Also, the methylation of the hydroxy group I intended to carry out with dimethylcarbonate and cesium carbonate as a base (this, apparently, yields a quantitative amount of 4-methoxytoluene after four hours of refluxing, and doesn’t need any dubious methylating agent such as methyl iodide). Thanks for reminding me about the cobalt way. I need to buy an oxygen bottle, but that’s cheap, too.

[Edited on 11-5-2023 by Keras]
View user's profile View All Posts By User
ErgoloidMesylate
Banned
**




Posts: 89
Registered: 8-8-2022
Location: Norad
Member Is Offline

Mood: Freedom of thought is priceless - You can't afford it

[*] posted on 11-5-2023 at 11:44


Quote: Originally posted by Keras  
Quote: Originally posted by ErgoloidMesylate  

http://orgsyn.org/demo.aspx?prep=CV3P0130

Are you going to use the cobalt method at that point?

https://drive.google.com/file/d/1xGiV4FJO_pWh3gYv8fQwa4AED-j...
[Edited on 10-5-2023 by ErgoloidMesylate]


I mean, yes, I could start from p-toluidine, diazotise it and hydrolise it to p-cresol, but I don’t see the point.


It avoids the excessively caustic route is the point, plus seems like a somewhat better procedure in my opinion.




Cannula transfer and cannula filtering is used for lysergic synth Compressed air and remove co2
View user's profile View All Posts By User
Keras
National Hazard
****




Posts: 864
Registered: 20-8-2018
Location: (48, 2)
Member Is Offline


[*] posted on 12-5-2023 at 00:23


Quote: Originally posted by ErgoloidMesylate  

It avoids the excessively caustic route is the point, plus seems like a somewhat better procedure in my opinion.


It is certainly less caustic. The procedure with KOH is fairly straightforward, though, and spares sodium nitrite which is hard to come by these days.

Apparently p-toluidine is restricted in the EU for w/e reason, so impossible to source.

Thanks a bunch again for shaking my memory about that cobalt thing, though. I was wondering these days why I had bought it in the first place! :p
View user's profile View All Posts By User

  Go To Top