Author: Subject: Help identifying these metal ions
Metallus
Hazard to Others
***




Posts: 116
Registered: 16-5-2013
Member Is Offline

Mood: No Mood

[*] posted on 1-5-2023 at 16:06
Help identifying these metal ions


Hello,
recently I stumbled upon a test for metal ions that puzzled me. The starting compound is the residue of coal waste, treated with KOH, which looks like a mix of iron oxides (pale green/brown), but it reacts in odd ways, which suggests there might be other things in there.

When dissolved in water, it has a pH > 13 due to a large excess of potassium hydroxide in the solution

• A first, concentrated batch was dissolved in water and was dark emerald green, but after a day at room temperature, it turned yellow and there was no precipitate formation.

• After a couple of days, a second less concentrated batch was dissolved in water, but this time it was a paler green and not fully clear. Acidifying with HCl led to violent foaming (likely due to the decomposition of carbonates) and turned the solution from pale green to bright yellow.

• Adding H2O2 to this solution led to the formation of a deep blue solution, which rapidly became colorless (within 2s).

The suspect metal ions are Fe and Cr mainly, but some things don't sound right:
1) In the starting green solution (pH >13), if it was Fe(II), it would make sense that it undergoes oxidation with air overtime and turns into Fe(III), but shouldn't the high pH make Fe(III) precipitate?

2) Dissolving a new batch yielded a paler green solution. If it was Fe(II), it could be that the 2nd batch underwent some oxidation on its own overtime; acidifying this solution with HCl instantly turned it into a bright yellow which could be due to the oxidation of Fe(II) to Fe(III).

3) Adding H2O2 turned the solution from yellow to a deep blue, before becoming completely colorless. The acid solution of Cr(VI) is known to temporarily make a deep blue complex with H2O2, that rapidly decomposes back to green Cr(III), but this one becomes completely colorless. Also, if it was Cr (VI), where would that come from? What can oxidise Cr III to VI in such conditions?

Do you have any idea what it might be and why it behaves like this?

starting solid waste.png - 1.1MB conc solid waste solution overnight.png - 568kB metal ion identificaiton.png - 1.6MB
View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6338
Registered: 4-10-2014
Location: At home
Member Is Offline

Mood: Most of the ducks are in a row

[*] posted on 1-5-2023 at 17:02


Looks like Cr plus something oxidising in the mix.
View user's profile View All Posts By User
Admagistr
Hazard to Others
***




Posts: 376
Registered: 4-11-2021
Location: Central Europe
Member Is Offline

Mood: The dreaming alchemist

[*] posted on 1-5-2023 at 17:39


Quote: Originally posted by j_sum1  
Looks like Cr plus something oxidising in the mix.


I also immediately thought of chromium, but why is the solution colourless afterwards?! So Cr3+ doesn't behave like that... Is any chromium compound colourless, I highly doubt it!

[Edited on 2-5-2023 by Admagistr]
View user's profile View All Posts By User
clearly_not_atara
International Hazard
*****




Posts: 2801
Registered: 3-11-2013
Member Is Offline

Mood: Big

[*] posted on 1-5-2023 at 20:25


Mo (V) is blue, and Mo (VI) can be colorless.



Quote: Originally posted by bnull  
you can always buy new equipment but can't buy new fingers.
View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6338
Registered: 4-10-2014
Location: At home
Member Is Offline

Mood: Most of the ducks are in a row

[*] posted on 1-5-2023 at 20:45


Quote: Originally posted by clearly_not_atara  
Mo (V) is blue, and Mo (VI) can be colorless.

I thought of that. But the blue is a bit different. And that does not explain the green, which is quite an intense forest green.
View user's profile View All Posts By User
DraconicAcid
International Hazard
*****




Posts: 4363
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline

Mood: Semi-victorious.

[*] posted on 1-5-2023 at 20:58


Dilute chromium(III) is pretty close to colourless, especially compared to the intensity of the peroxide complex.



Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
View user's profile View All Posts By User
kmno4
International Hazard
*****




Posts: 1504
Registered: 1-6-2005
Location: Silly, stupid country
Member Is Offline

Mood: No Mood

[*] posted on 1-5-2023 at 21:12


It looks like Cr, of course, but with some admixture.
This admixture(s) may catalyze air oxidation of Cr(III) to Cr(VI) - for example Mn does this trick.
About colourless solution - it reminds me Ni(II) and Co(II) mixture.
At some ratio Ni/Co, the solution is purely colourless. It may be similar case.




Слава Україні !
Героям слава !
View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6338
Registered: 4-10-2014
Location: At home
Member Is Offline

Mood: Most of the ducks are in a row

[*] posted on 2-5-2023 at 00:43


Quote: Originally posted by DraconicAcid  
Dilute chromium(III) is pretty close to colourless, especially compared to the intensity of the peroxide complex.

This is not my experience. I have often been surprised by the intensity of Cr(iii) solutions.
View user's profile View All Posts By User
Metallus
Hazard to Others
***




Posts: 116
Registered: 16-5-2013
Member Is Offline

Mood: No Mood

[*] posted on 2-5-2023 at 08:59


Thanks for your replies

Another update on this test. One of the batch of the pale green solution was left overnight and the following day it was bright yellow. To this, H2O2 was added while the solution was still basic, but nothing happened. But after the addition of some acid, part of the solution became blue/purple and then turned colorless, but the most interesting thing is... it separated!

As you can see from the pictures, the colorless liquid is floating on top of the yellow one (which is still basic). Adding extra acid, makes the remaining yellow react and go to blue and colorless and mix with the rest.

What could this immiscible colorless liquid be? So far we hypothesized it was a reaction of Cr VI making the blue peroxocomplex and then going to Cr III, but then the solution should be green, but instead it's colorless and not miscible with water. Any idea?

One additional detail, the basic yellow solution reacts with organic matter like cellulose from wood and turns orange with some brown precipitate, but this could be gunk from the wood bits.

yellow solution with wood chips.png - 469kBimmiscible yellow white solution.jpg - 11kB
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8034
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 2-5-2023 at 09:42


The floating on top is most likely due to difference in density. If you have miscible liquids, but one of them is denser than the other, then they remain separated for quite a while, but slowly they will diffuse into each other.

I think that there is chromium in the mix, but that is not the complete story. The blue color with H2O2 at low pH and the fading of that color is quite specific for hexavalent chromium. Even very dilute hexavalent chromium can be detected this way. Iron could also be present. If you have potassium ferrocyanide (yellow prussiate of potash, K4Fe(CN)6), then you could try adding some of that. With trivalent iron it gives an intense blue color or low to medium pH, which persists. At high pH, the blue color disappears and the liquid turns pale yellow/brown and a little opalescent.




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
Metallus
Hazard to Others
***




Posts: 116
Registered: 16-5-2013
Member Is Offline

Mood: No Mood

[*] posted on 4-5-2023 at 02:44


Update

A dried green/white chunk of the raw material was dissolved in water, yielding a rusty precipitate, a dark green solution and some whitish suspension (this solid contains KOH and its pH is >13). This was centrifuged, forming 2 precipitates (a whitish and orange one) and leaving a very intense dark green solution. The dark green solution was isolated.

1) to 1 ml of this dark green solution, HCl was added, turning the solution yellow and producing a brown precipitate (acid pH). To the resulting solution, H2O2 was added, initially turning the solution blue (for 1s) and then pale green/colorless (a separation of the two liquids was observed, as shown in the previous post).
On the pale green/colorless solution, KOH was added again to bring the pH back to 13, turning the solution fully colorless and producing a dark brown precipitate.

2) to 1 ml of the starting dark green solution, H2O2 was added, turning the solution dark orange.

Hypothesis:
1) The starting solution has an intense dark green color, and the only thing I know that is so intensely colored is Cr III, likely in the form of Cr(OH)63- due to the very basic pH.
- Acidifying this solution turns it yellow, with a brown precipitate. The yellow could be attributed to the formation of CrO42-, but which species could be oxidising Cr III to VI, while leaving behind a brown precipitate?
- My hypothesis is that there is some MnO4- or MnO42- in there (the latter being green too!), and that acidifying the solution leads to the oxidation of Cr III to Cr VI, and the reduction of Mn VI/V to Mn IV, which precipitates as MnO2 (brown precipitate).
- Then, following the addition of H2O2 in acid environment, the CrO42- (and MnO2) are reduced to Cr3+ and Mn2+, which leave a pale green/colorless solution.
- Upon addition of KOH, a dark brown solid precipitates. Now, I'm not sure why this is happening. Could it be that the excess H2O2, coupled with the basic pH, is oxidising Mn2+ to MnO2? Usually H2O2 is a strong oxidiser in basic pH (or more precisely, these metal oxides are less oxidising in basic environments), so that would explain the brown precipitate.

2) Upon addition of H2O2 to the raw, basic, dark green solution, the solution turns dark orange. If the H2O2 was oxidising Cr III to Cr VI, this should be bright yellow instead of dark orange (which is typical of acid Cr VI solutions), and if there was Mn in there, not much should happen. The only metal that turns orange in basic H2O2 solutions that I know of, is lead IV/II oxide (Pb3O4).

Do you have any observations or thoughts about what else could be in there?

raw green chunk.png - 838kB raw green + HCl + H2O2.png - 667kB pale green + KOH.png - 462kB Raw green + H2O2.png - 332kB
View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6338
Registered: 4-10-2014
Location: At home
Member Is Offline

Mood: Most of the ducks are in a row

[*] posted on 4-5-2023 at 03:16


Ti forms an amber complex with peroxide.

I think your detective work is good here. But it seems there is quite a mixture in there.
View user's profile View All Posts By User
Metallus
Hazard to Others
***




Posts: 116
Registered: 16-5-2013
Member Is Offline

Mood: No Mood

[*] posted on 5-5-2023 at 01:02


Some more weird things

The starting green, basic solution, becomes yellow overtime on its own. Adding HCl to this solution leads to the formation of a brown precipitate AND negative pressure. It's like it's consuming something from the atmosphere. As you can see in the pictures below, the glove is being sucked in. What could be causing that? I thought oxygen consumption from the air might be the reason, but shouldn't oxygen diffusion be a slow process anyways for this to be noticeable?

Some other tests on the pale green solution, obtained after HCl + H2O2 treatment, which in theory should have left a Cr3+ solution behind (the excess H2O2 was previously decomposed by heating):
- in one test tube of the pale green solution, adding ammonia till basic pH leads to the formation of a light blue/azure precipitate. After centrifugation, it still doesn't fully settle and remains suspended as a light blue gel. Upon addition of KOH, a dense gas is released (probably ammonia) and a brown precipitate forms. After centrifugation, this settles as a brown solid, leaving a pale brown solution.
- in another test tube of the pale green solution, adding ascorbic acid turns the solution light green, and adding KOH afterwards turns it very dark/black with an olive/red weird tint. Adding HCl, makes the solution lighter colored, revealing a dark red hue.

1) If the HCl + H2O2 left a Cr3+ solution, adding a weak base should make green Cr(OH)3 precipitate, but instead an azure precipitate is obtained. Could this be an amino-compound with Cr? I remember seeing something similar in Woelen's wegpage about Cr III. Adding KOH should in theory reverse the entire reaction and take us back to the starting dark green solution, hypothesized to be Cr(OH)63-, instead a dark brown precipitate forms.

2) Due to the acid pH, ascorbic acid should be in its protonated form and shouldn't be acting as a chelating agent, but could still be acting as a reductant. Are you aware of a reaction that turns pale green to light green? Adding KOH makes a very dark solution, that lightens up only upon addition of HCl.

I still think there's some Cr in there (because of the temporary blue complex) but what else could be giving these reactions? And why are we unable to revert back to the dark green solution?

Is anyone familiar with ascorbic acid and what metal complexes it might make? Or perhaps if in these conditions it is acting as a reductant. Are any of these colors familiar?



pale green + NH3 + KOH.png - 557kB vacuum.png - 340kB pale green + ascorbic + KOH + HCl.png - 458kB



[Edited on 5-5-2023 by Metallus]
View user's profile View All Posts By User
Boffis
International Hazard
*****




Posts: 1886
Registered: 1-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 5-5-2023 at 03:36


First of all what do you mean by "coal waste"? Some younger low rank coals have accumulated much vanadium and uranium. I worked on such deposits in Central Asia, some of them were mined in soviet times for uranium. The coal was burnt in a power plant then the ash processed to recovery the uranium and vanadium.

Deposits of this type exist in the USA too and probably else where. The grade is usually too low to be mined for the metals alone but they are greatly enriched in the ash.

So, as you can see there is a lot of scope, Zn, Se, Ge and various other base metals are not uncommon in some coals. If the coal "waste" hasn't been burnt but weathered at the surface organic phases are possible too. I worked on a project once where cores from the weathered zone of oil shale near Edinburgh in Scotland would "bleed" a beautiful purple colour is treated with alkali. The fresh shale didn't seem to do this.

So what exactly is your coal waste?

[Edited on 5-5-2023 by Boffis]
View user's profile View All Posts By User
kmno4
International Hazard
*****




Posts: 1504
Registered: 1-6-2005
Location: Silly, stupid country
Member Is Offline

Mood: No Mood

[*] posted on 5-5-2023 at 04:28



..... that is why I would use XRF spectrometer to analyse the raw material. Playing with probes gives more questions than answers.
At best, one or two main metals can be identified in this way.
One should use more specific tests, in better controlled conditions.
The colour of sediment on the first picture strongly reminds me sediments obtained during my experiments with Cr(III) performed long time ago, but it is only my personal impression.




Слава Україні !
Героям слава !
View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6338
Registered: 4-10-2014
Location: At home
Member Is Offline

Mood: Most of the ducks are in a row

[*] posted on 7-5-2023 at 15:56


This recently-posted yt clip seems relevant. It looks like a lot of what you have observed is happening here.
https://youtu.be/UeypljpiB-U



One of the things that confused me is the colourless solution containing Cr(iii). My experience of Cr3+ is that the colour is quite intense and I am never expecting colourless. Perhaps the presence of sulfate makes a difference: Cr2(SO4)3 has a very rich colour.