Looking for CaC2 in ton quantities (EU)


Hi all,

Yes, another topic about Calcium Carbide.
The same people who supplied me with the carbide I'm offering to SM members are also looking for carbide by the ton / pallet / several drums.

What seems now a long time ago several associations I've been involved with used to order carbide from China or Romania by pallet or even container.

Customs have made this too complicated and expensive over time to get containers from China. Romania has stopped producing Calcium carbide.
We're looking for suppliers within Europe.
The carbide is to be used in carbide lamps / acetylene generators so any size and grade are acceptable.

If you can supply or have a suggestion on where to look I will tranmit them.




The spirit of adventure was upon me. Having nitric acid and copper, I had only to learn what the words 'act upon' meant. - Ira Remsen
View user's profile View All Posts By User
Σldritch
Hazard to Others
***




Posts: 309
Registered: 22-3-2016
Member Is Offline

Mood: No Mood

[*] posted on 8-3-2023 at 12:04


Look for manufacturer in Russia, Norway or Iceland? They have cheap/excess energy. Europe hardly manufactures anything anymore, though. You could look at countries with aluminium production, too, similar requirements I think and should be easier to find data on.
View user's profile View All Posts By User
Elemental Phosphorus
Hazard to Others
***




Posts: 184
Registered: 11-11-2016
Location: Is everything
Member Is Offline

Mood: No Mood

[*] posted on 12-3-2023 at 12:06


Quote: Originally posted by Herr Haber  
Hi all,

Yes, another topic about Calcium Carbide.
The same people who supplied me with the carbide I'm offering to SM members are also looking for carbide by the ton / pallet / several drums.

What seems now a long time ago several associations I've been involved with used to order carbide from China or Romania by pallet or even container.

Customs have made this too complicated and expensive over time to get containers from China. Romania has stopped producing Calcium carbide.
We're looking for suppliers within Europe.
The carbide is to be used in carbide lamps / acetylene generators so any size and grade are acceptable.

If you can supply or have a suggestion on where to look I will tranmit them.



Donau Chemie in Germany claims to sell calcium carbide packed in containers in 100kg or 250kg drums, and their website claims it is manufacture in Landeck, Austria. However, whether or not they are actively producing calcium carbide or have available stock is unclear. The minimum order is also 20 tons, but they have another arm that deals with smaller acquisitions that you might be able to contact.

https://www.donau-chemie.com/Products-Solutions/BU-Chemie/Ka...

https://www.donauchem.com/LandingPageEN.aspx

They are headquartered in Austria but have facilities throughout Europe, including in Romania, so I'm not sure if this is the same supplier from which the carbide became unavailable.

https://www.bloomberg.com/profile/company/DONA:AV#xj4y7vzkg

https://greco.services/more-procurement-logistics-resilience...

I don't know if it would work or if it's what you're looking for, but maybe worth giving them a call.

AlzChem, based in Bavaria also apparently has calcium carbide for sale in 120kg drums or 1 or 1.5 ton containers. I couldn't find much information on that, not sure where it's manufactured or where it would ship from, and AlzChem also mostly manufactures organic chemicals, but could be worth contacting them too.


[Edited on 12-3-2023 by Elemental Phosphorus]
View user's profile View All Posts By User
SuperOxide
Hazard to Others
***




Posts: 486
Registered: 24-7-2019
Location: Devils Anus
Member Is Offline


[*] posted on 13-3-2023 at 14:53


Just curious, what do they/you need so much CaC2 for?
View user's profile View All Posts By User
Herr Haber
International Hazard
*****




Posts: 1236
Registered: 29-1-2016
Member Is Offline

Mood: No Mood

[*] posted on 16-3-2023 at 09:09


Quote: Originally posted by SuperOxide  
Just curious, what do they/you need so much CaC2 for?


To feed carbide lamps / generators.
Besides chemistry my main other hobby is "everything underground".
Despite the advent of electricity last century and the LED revolution at the begining of this century many people still use acetylene for light.

With it's high carbon content just one lamp with a 14L/h burner will give more light than a dozen candles. For many people it's not just "more light" but also a better, warmer light.

I'm in contact with two associations that have to storage capacity for many many tons. All of course veted by the fire department and located in non floodable areas ;)
The idea, by getting such huge amount it to "postpone the problem" of not finding CaC2 anymore. It's been getting harder to find over the years and the prices have climbed a lot. These associations used to pool their resources together and get container space for carbide from China.
The thing is that for them INCOTERMS are a pain in the ass and they're only looking for sources within Europe now. FOB seems nice until the bills start to add up.
Right now I can go by carbide from a store for 18 Euros / 800 grams.
Years ago, through these associations used to sell it a 3.50/kg. It went up to 5.50 Euros.
The carbide I'm sending to SM members I traded for so price was irrelevant to me. I'm just happy if it helps members.

I will definitely look into the suggestions everyone gave me. Many thanks for these :)
We're used to 50kg, 70kg and 120kg drums and to be honest, demand is so high that even a ton would get repackaged and distributed in less than a week.
Asking SM community an opinion on this is really a "hail Mary". There are a lot of smart people between these two associations and I'd be surprised if I managed to find a supplier they didnt contact already and ruled out for some reason.

Suggestions are still welcome :)




The spirit of adventure was upon me. Having nitric acid and copper, I had only to learn what the words 'act upon' meant. - Ira Remsen
View user's profile View All Posts By User
clearly_not_atara
International Hazard
*****




Posts: 2722
Registered: 3-11-2013
Member Is Offline

Mood: Big

[*] posted on 16-3-2023 at 18:17


Probably absurd, but could you make CaC2 "backwards" from acetylene? Modern chemical industry makes acetylene from methane these days, bypassing CaC2. But if you had some Ca(OEt)2 or something in solution, maybe you can gas acetylene and get the desired carbide?

A bit difficult for ton quantities, I guess.

Alternatively, maybe calcium acetylenedicarboxylate decomposes to CaC2? Or calcium mellitate? Mellitic acid is relatively stable.




Quote: Originally posted by bnull  
you can always buy new equipment but can't buy new fingers.
View user's profile View All Posts By User
Fantasma4500
International Hazard
*****




Posts: 1681
Registered: 12-12-2012
Location: Dysrope (aka europe)
Member Is Offline

Mood: dangerously practical

[*] posted on 27-3-2023 at 05:30


i was hinted at by a young carbide enthusiast that he got his 100kg from farmer supplies in holland
carbide cannons are kinda grey zone in holland, but if its really big amount i imagine they would care less, it seems more professional then




~25 drops = 1mL @dH2O viscocity - STP
Truth is ever growing - but without context theres barely any such.

https://en.wikipedia.org/wiki/Solubility_table
http://www.trimen.pl/witek/calculators/stezenia.html
View user's profile View All Posts By User
Herr Haber
International Hazard
*****




Posts: 1236
Registered: 29-1-2016
Member Is Offline

Mood: No Mood

[*] posted on 27-3-2023 at 17:42


@clearly_not_atara Well, I learnt a lot researching those compounds and it certainly would be poetic to use a chemical that has such ties to stone !
But it would be very impractical. Anything more than splitting drums between buyers, weighting and putting into HDPE buckets is beyond what they can do.
Ah... if only I had an arc furnace and a nuclear plant...

@Fantasma4500
The people in these associations imported containers so the paperwork / professional aspect isnt a problem :) Maybe someone in Holland still has a few drums. It would be interesting to see the cost.
I've seen a couple of those crow cannons over the years. They are a thing of the past, as are carbide lamps, but they are pretty ingenious. The one I liked the most just worked by building up pressure which would activate a piezo spark thingie at the moment the gas was released.




The spirit of adventure was upon me. Having nitric acid and copper, I had only to learn what the words 'act upon' meant. - Ira Remsen
View user's profile View All Posts By User
Fantasma4500
International Hazard
*****




Posts: 1681
Registered: 12-12-2012
Location: Dysrope (aka europe)
Member Is Offline

Mood: dangerously practical

[*] posted on 4-9-2023 at 06:18


i just saw lately some CaC2 bags labeled as being used to make fruits ripen- theres a chance to get a backdoor deal with a fruit company, unsure if this is used in europe as technique, there was some asian font on the bags ..





~25 drops = 1mL @dH2O viscocity - STP
Truth is ever growing - but without context theres barely any such.

https://en.wikipedia.org/wiki/Solubility_table
http://www.trimen.pl/witek/calculators/stezenia.html