Phosphoric Acid dry distillation
Recently I carried out the below using a dry distillation.
100g of ammonium dihydrogen phosphate (MAP fertilizer) + 200g of sodium bisulphate and recovered around 35ml of phosphoric acid.
I actually mixed up my sums as that is quite and excess of bisulphate, however what surprised me is once the reaction flask had slowly cooled down and
left overnight I had a single solid mas in the flask but completely crystal clear like glass!
Could this be a double salt of ammonium sulphate and sodium sulphate or is it possible to get a really clear mix of the two salts?
Anyway I think my acid yield was poor (although quite concentrated I expect) so I will probably try a wet method next time I think.
[Edited on 1-2-2023 by Chemgineer]
|
|
Texium
|
Thread Moved 1-2-2023 at 11:41 |
BromicAcid
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3237
Registered: 13-7-2003
Location: Wisconsin
Member Is Offline
Mood: Rock n' Roll
|
|
There's a thread kicking around somewhere on the forum on pyro/poly phosphoric acids. In another life I was trying to make polyphosphoric acids by
heating ammonium dihydrogen phosphate dry and ended up with massively corrosive solids. Generally phosphoric acid doesn't boil, it just keeps losing
more and more water. But I suppose there has to be some point where something volatile comes over as it never gets to the oxide by heat alone.
|
|
chornedsnorkack
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 539
Registered: 16-2-2012
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by BromicAcid ![](images/xpblue/lastpost.gif) | Generally phosphoric acid doesn't boil, it just keeps losing more and more water. But I suppose there has to be some point where something volatile
comes over as it never gets to the oxide by heat alone. |
The azeotropic phosphoric acid boils at around 850 C, and has a composition slightly towards P2O5 from HPO3.
A link:
https://www.google.com/url?sa=t&rct=j&q=&esrc=s&...
quotes another source (an 1950 one) as giving the azeotrope around 870 C and 92,1% P2O5 (HPO3 would be 88,8%)
[Edited on 2-2-2023 by chornedsnorkack]
|
|
Chemgineer
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 193
Registered: 25-5-2021
Member Is Offline
|
|
I was getting a red indication for low PH to begin with, i've just checked my distillate bottle again and the final solution actually indicates a PH
of around 9 and smells of ammonia! I guess this is a failed attempt.
|
|
chornedsnorkack
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 539
Registered: 16-2-2012
Member Is Offline
Mood: No Mood
|
|
Phosphoric acids form no crystal forms between H4P2O7 and the various forms of P2O5. Just glasses. So the residue must have contained all of your
phosphorus, plus freeze into the glass some water, all Na and whatever else does not distil over. What is likely is that NH3 did go over in your
distillate. If your melt got hot enough, some SO3 too.
|
|
Chemgineer
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 193
Registered: 25-5-2021
Member Is Offline
|
|
If phosphoric acid does not boil why does literature online state it's boiling point at 158-200 deg C?
|
|
chornedsnorkack
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 539
Registered: 16-2-2012
Member Is Offline
Mood: No Mood
|
|
Because compositions that are not azeotropes do not boil at constant composition. Composition H3PO4 does reach total vapour pressure 1 bar and boil
with bubbling, at a reproducible temperature. The matter is that the vapour at that condition is pure water.
|
|
RustyShackleford
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 196
Registered: 10-12-2020
Location: Northern Europe
Member Is Offline
|
|
Phosphoric acid polymerizes on heating, this forms the actually pretty useful polyphosphoric acid, powerful dehydrating agent useful for many organic
reactions.
The reason it has a stated boiling point (or range) is because that is the temperature at which 100% phosphoric acid will start polymerizing with the
loss of water.
|
|
chornedsnorkack
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 539
Registered: 16-2-2012
Member Is Offline
Mood: No Mood
|
|
Some details
https://isolab.ess.washington.edu/resources/H3PO4.pdf
Page 12 (16 of pdf) Figure 2 has boiling point curve. Cuts off above 160 C short of 90%. Boiling point at 100% is elsewhere reported around 260 C
Page 19 (23 of pdf) Figure 11 has vapour pressure of acid at various temperatures and concentrations. Note the 100% acid. Even at 100 C, the pressure
3,65 mm Hg is just 15% of the 24 mm Hg vapour pressure of 0% acid (pure water) at 25 C. Since the pressure of water vapour tends to be the same in
furnace and lab, then unless your lab has humidity under 15%, the H3PO4 will still absorb water from air at 100 C.
Page 20 (24 of pdf) discusses vapour composition. Small amounts of acid vapour are shown from around 300 C, but the composition is already
H3PO4-H4P2O7 mix. Figure 12 reaches 800 C and 55% P2O5 in vapour, but this is short of azeotrope (870 C and 92% P2O5 in vapour)
|
|