Author: Subject: Ion exchange resin -> membrane
Parakeet
Hazard to Self
**




Posts: 73
Registered: 22-12-2022
Location: Japan
Member Is Offline

Mood: V (V)

[*] posted on 16-1-2023 at 02:54
Ion exchange resin -> membrane


Is it possible to use ion exchange resin as ion exchange membrane? I want to use it in electrolysis cell but they aren't cheap. However the resin is more easily available. They have different applications but the material are the same, aren't they?
View user's profile View All Posts By User
Rainwater
National Hazard
****




Posts: 850
Registered: 22-12-2021
Member Is Offline

Mood: indisposition to activity

[*] posted on 16-1-2023 at 03:23


https://www.sciencemadness.org/whisper/search.php?token=&...



"You can't do that" - challenge accepted
View user's profile View All Posts By User
Mateo_swe
National Hazard
****




Posts: 526
Registered: 24-8-2019
Location: Within EU
Member Is Offline


[*] posted on 17-1-2023 at 03:39


Ion exchange membranes dont have to be so expensive, there are many different ones and some are not that expensive.
Check out
https://www.fuelcellstore.com/fuel-cell-components/membranes
View user's profile View All Posts By User
Parakeet
Hazard to Self
**




Posts: 73
Registered: 22-12-2022
Location: Japan
Member Is Offline

Mood: V (V)

[*] posted on 17-1-2023 at 14:37


Thanks!
I wasn’t able to find that thread.
But I will look for cheap sources first.
View user's profile View All Posts By User