Ion exchange resin -> membrane
Is it possible to use ion exchange resin as ion exchange membrane? I want to use it in electrolysis cell but they aren't cheap. However the resin is
more easily available. They have different applications but the material are the same, aren't they?
|
|
Rainwater
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 881
Registered: 22-12-2021
Member Is Offline
Mood: indisposition to activity
|
|
https://www.sciencemadness.org/whisper/search.php?token=&...
"You can't do that" - challenge accepted
|
|
Mateo_swe
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 528
Registered: 24-8-2019
Location: Within EU
Member Is Offline
|
|
Ion exchange membranes dont have to be so expensive, there are many different ones and some are not that expensive.
Check out
https://www.fuelcellstore.com/fuel-cell-components/membranes
|
|
Parakeet
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 74
Registered: 22-12-2022
Location: Japan
Member Is Offline
Mood: V (V)
|
|
Thanks!
I wasn’t able to find that thread.
But I will look for cheap sources first.
|
|