Unfortunately, using calcium nitrate in composition was not tested. Is possible that acetic acid catalyse better properties of guar gum as binder.
But also not tested. Measurement in cavity showing density 1.6 g/cc. Not 1.7. Composition is castable at 80 C without guar gum. Repeatedly.
Composition, respectively his surface is partially hygroscopic. It was observed. Ferocene was not tested. Yes, was tested different acrylic
pigment colors. Yellow, red, green, orange. Interest: This dry (any color) acrylic pigment create
with NH4ClO4 pretty explosive mixture at ratio AP 75 / color 25. Without change of nice color of pigment.
https://www.google.com/search?q=pigment+to+wall+color+paint&...
Maybe colors works as catalyseur of shockwave. (no confirmed, no measured)
But confirmed is better binding effect with acrylic colors. (acryl is binder itself)
Yes, different colors is possible use as identificator.
Else composition can looks: NaClO4 75, DEG 25, liquid pigment (red from link) 11, dH2O 4, guar gum 1. In of part by weight. 20g sensitive on No.8,
confirmed.
![71mnW78e+tL.jpg - 368kB](http://www.sciencemadness.org/talk/files.php?pid=680280&aid=96628)
[Edited on 10-1-2023 by Laboratory of Liptakov]
Development of primarily - secondary substances CHP (2015) Lithex (2022) Brightelite (2023) Nitrocelite and KC primer (2024)
|
|
Bert
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2821
Registered: 12-3-2004
Member Is Offline
Mood: " I think we are all going to die. I think that love is an illusion. We are flawed, my darling".
|
|
I just spent a few minutes going over solubilities of various perchlorates in various liquid fuels.
One combination that struck me: Barium diperchlorate, 125g soluble in 100ml ethanol @ 25° C. And barium (di) perchlorate is DENSE at around 3.1 g/cc.
Not so cheap as technical Sodium perchlorate, toxic like all water soluble barium salts- but also NOT HYGROSCOPIC.
Rapopart’s Rules for critical commentary:
1. Attempt to re-express your target’s position so clearly, vividly and fairly that your target says: “Thanks, I wish I’d thought of putting it
that way.”
2. List any points of agreement (especially if they are not matters of general or widespread agreement).
3. Mention anything you have learned from your target.
4. Only then are you permitted to say so much as a word of rebuttal or criticism.
Anatol Rapoport was a Russian-born American mathematical psychologist (1911-2007).
|
|
Laboratory of Liptakov
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1366
Registered: 2-9-2014
Location: Technion Haifa
Member Is Offline
Mood: old jew
|
|
Is it slightly exotic composition, but should by works. Ba(ClO4)2 with OB + 38.06 is also soluble in acetone (OB - 220.3) ethanol OB - 208.7 on CO2.
In acetone is soluble (as binder) nitrocellulose, camphor, rosin. In ethanol is soluble camphor , rosin. Testing mixture can be:
1) Ba(ClO4)2 80 + 20 ethanol, final OB - 11.29 on CO2.
2) Ba(ClO4)2 80 + acetone 20 .........final OB - 13.61 on CO2.
3) Ba(ClO4)2 75 + ethanol 20 + rosin 5 ..........final OB - 26.39 on CO2
4) Ba(ClO4)2 75 + acetone 20 + nitrocellulose/12,4N/ .... 5 ........final OB - 17.3 on CO2
All mixtures looks no hygroscopic. Problem can be evaporation of solvents. Any way, interesting idea with Barium perchlorate. It seems , that adding
Alu powder is possible.
Development of primarily - secondary substances CHP (2015) Lithex (2022) Brightelite (2023) Nitrocelite and KC primer (2024)
|
|
Bert
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2821
Registered: 12-3-2004
Member Is Offline
Mood: " I think we are all going to die. I think that love is an illusion. We are flawed, my darling".
|
|
Quote: Originally posted by Laboratory of Liptakov ![](images/xpblue/lastpost.gif) | Is it slightly exotic composition, but should by works. Ba(ClO4)2 with OB + 38.06 is also soluble in acetone (OB - 220.3) ethanol OB - 208.7 on CO2.
In acetone is soluble (as binder) nitrocellulose, camphor, rosin. In ethanol is soluble camphor , rosin. Testing mixture can be:
1) Ba(ClO4)2 80 + 20 ethanol, final OB - 11.29 on CO2.
2) Ba(ClO4)2 80 + acetone 20 .........final OB - 13.61 on CO2.
3) Ba(ClO4)2 75 + ethanol 20 + rosin 5 ..........final OB - 26.39 on CO2
4) Ba(ClO4)2 75 + acetone 20 + nitrocellulose/12,4N/ .... 5 ........final OB - 17.3 on CO2
All mixtures looks no hygroscopic. Problem can be evaporation of solvents. Any way, interesting idea with Barium perchlorate. It seems , that adding
Alu powder is possible.
|
In pyotechnics, it has been traditional to include a small % of a weak acid such as boric acid in compositions containing powdered aluminum and
intended to be bound with water activated adhesives. Mixtures containing nitrates which are prone to evolving ammonia, undergoing self heating and
thermal runaway leading to ignition in particular.
At this point, my questions regarding your HE mixtures video have lead us far from the original topic of this thread- Although it began with sourcing
diethylene glycol to use as an energetic precursor chemical for propellants, we're now talking about fuel use "as is" and detonation rather than
deflagration?
Laboratory of Liptakov, I propose to split this thread, do you concur? If so, should our side trip into HE mixtures with soluble in fuels oxidizer
salts be rejoined with one of the related earlier threads or would you like to start a new thread with this?
[Edited on 1-11-2023 by Bert]
Rapopart’s Rules for critical commentary:
1. Attempt to re-express your target’s position so clearly, vividly and fairly that your target says: “Thanks, I wish I’d thought of putting it
that way.”
2. List any points of agreement (especially if they are not matters of general or widespread agreement).
3. Mention anything you have learned from your target.
4. Only then are you permitted to say so much as a word of rebuttal or criticism.
Anatol Rapoport was a Russian-born American mathematical psychologist (1911-2007).
|
|
Laboratory of Liptakov
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1366
Registered: 2-9-2014
Location: Technion Haifa
Member Is Offline
Mood: old jew
|
|
The trip can be plugged with some related thread. Thanks, Bert. Maybe after testing described mixture (on BaP base) can be serious reason create a new
thread....![:cool:](./images/smilies/cool.gif)
[Edited on 11-1-2023 by Laboratory of Liptakov]
Development of primarily - secondary substances CHP (2015) Lithex (2022) Brightelite (2023) Nitrocelite and KC primer (2024)
|
|
Pages:
1
..
8
9
10 |
|