Optical furnace for growing crystals
I am looking into the idea of creating a smaller and simplified optical furnace for some crystals and gemstone production. The basis of this furnace
is a quartz tube, halogen bulbs, ellipsoidal mirrors. The amount of energy required to prepare ruby is about 4000 W, depending on the technical
arrangement. The starting powder material is pressed and sintered and then gradually remelted in this furnace, resulting in an optically flawless
crystal if everything goes right. Would anyone tech-savvy know how to make ellipsiod mirrors so that they concentrate all the light energy received
from halogen lamps into one spot, and what particular IR halogen lamps to choose? Of course it depends on the diameter of the quartz tube, I have
several of even large diameters, the largest one I have is about 13.5 cm diameter from my memory. I also have smaller quartz tubes, perfect optical
quality, I guess 5 cm diameter. I'd have to check... I'm thinking of using four halogen IR bulbs, each with a power of 1000 W, and concentrating their
energy in one focal point, where a ruby crystal would be formed.
|
|
JohnnyBuckminster
Harmless
Posts: 40
Registered: 6-6-2018
Member Is Offline
|
|
You have some interesting thoughts & projects! I'm by no means an expert, but just out of curiosity, why do you abandon the Nernst lamp for the
halogen bulbs? It's all about the getting the IR focused on the sample?
...I'm sourcing material for a small mini-furnace along the lines in the previous post " A high-temperature mini-furnace for temperatures above 2000
C." and thought the Nernst lamp should fit the bill, can even work without protective atmosphere...
|
|
Chemetix
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 375
Registered: 23-9-2016
Location: Oztrayleeyah
Member Is Offline
Mood: Wavering between lucidity and madness
|
|
I floated this idea a while ago. ( can't remember when and can't find it on here anymore) But the idea is sound. I spoke to a furnace designer
refractory specialist since my first post and they confirmed the idea would work.
|
|
Twospoons
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1306
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline
Mood: A trace of hope...
|
|
Quote: Originally posted by Chemetix ![](images/xpblue/lastpost.gif) | I spoke to a furnace designer refractory specialist since my first post and they confirmed the idea would work.
|
Which suggests they don't much about optics. You've drawn parallel rays coming off your element, and while a few will be parallel, by far most will
not be and will not be focused.
You might look to Nd:YAG laser cavity reflectors for inspiration - the sort used to transfer light from a linear flashlamp to the laser rod.
Bear in mind that the focii of an ellipse are points, so with any source you put there the radiating surface cannot be at the focus, only
close to it.
Helicopter: "helico" -> spiral, "pter" -> with wings
|
|
Chemetix
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 375
Registered: 23-9-2016
Location: Oztrayleeyah
Member Is Offline
Mood: Wavering between lucidity and madness
|
|
"You've drawn parallel rays coming off your element, and while a few will be parallel, by far most will not be and will not be focused. "
It's not about optical purity, this isn't a telescope. The rays are there to represent the majority of the EM flux, which emanating from the floor of
the kiln will be more or less a constant temperature. Yes it's focused too close to the parabola for the rays to be close to parallel but that doesn't
matter. The focal point only has to be a concentration of energy not a perfect intersection of rays for image resolution. What we worked out was that
there will be a spot that will concentrate most of the energy from the floor heating on a small area. Ending up with a large magnitude of energy
concentration. Taking 1000W.m^-2 and concentrating this to 10x makes a small area with an energy density far higher than a conventional kiln.
Fixating on the optical purity of the system misses the point. It's still powerful enough to make a small area very very very hot.
|
|
Sulaiman
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3625
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline
|
|
Although you will be focussing a lot of heat onto the target,
I believe that you can not heat an area o a temperature higher than the heater element temperature.
CAUTION : Hobby Chemist, not Professional or even Amateur
|
|
JohnnyBuckminster
Harmless
Posts: 40
Registered: 6-6-2018
Member Is Offline
|
|
Quote: Originally posted by Sulaiman ![](images/xpblue/lastpost.gif) | Although you will be focussing a lot of heat onto the target,
I believe that you can not heat an area o a temperature higher than the heater element temperature. |
Not general true, look at solar power towers, can even melt steel, Melting steel with solar power...
|
|
Fulmen
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1700
Registered: 24-9-2005
Member Is Offline
Mood: Bored
|
|
And what's the temperature of that heater element?
We're not banging rocks together here. We know how to put a man back together.
|
|
JohnnyBuckminster
Harmless
Posts: 40
Registered: 6-6-2018
Member Is Offline
|
|
Well that's a gotcha question ![;)](./images/smilies/wink.gif)
.. but seriously, are there any thermodynamics here, or any other physics, that impose such a a limit?
[Edited on 2022-1-30 by JohnnyBuckminster]
|
|
Admagistr
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 350
Registered: 4-11-2021
Location: Central Europe
Member Is Offline
Mood: The dreaming alchemist
|
|
Quote: Originally posted by JohnnyBuckminster ![](images/xpblue/lastpost.gif) | You have some interesting thoughts & projects! I'm by no means an expert, but just out of curiosity, why do you abandon the Nernst lamp for the
halogen bulbs? It's all about the getting the IR focused on the sample?
...I'm sourcing material for a small mini-furnace along the lines in the previous post " A high-temperature mini-furnace for temperatures above 2000
C." and thought the Nernst lamp should fit the bill, can even work without protective atmosphere... |
Thanks! The Nernst rod is not out of the picture, I'm still looking for it, I listed the halogen IR lamp because it is available, but I only found it
in tube form, even at power 2000 watts! The idea is to concentrate the heat into one spot-focus and place the emerging crystal as close to the focal
point as possible. I'd coat the elliptical mirror with thin gold leaf, the kind sold to artists who want to gold leaf something. Gold reflects IR
radiation best of all metals, and even firefighters use gold-plated shields as heat protection when they put out fires. By being very thin, the gold
leaf is light in weight and therefore affordable....
|
|
Sulaiman
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3625
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline
|
|
Yes, black body radiation, Stefan–Boltzmann law, solid angles and other stuff.
CAUTION : Hobby Chemist, not Professional or even Amateur
|
|
Twospoons
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1306
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline
Mood: A trace of hope...
|
|
Thats exactly my point - those rays do not represent the majority of the EM flux, but only a small fraction. Every point on that floor is radiating in
all directions, distributing energy in all directions. Which means the energy following your ray diagram is only a small fraction of the
total energy.
But you are more than welcome to build it and test it - thats what experimenting is all about.
Helicopter: "helico" -> spiral, "pter" -> with wings
|
|
JohnnyBuckminster
Harmless
Posts: 40
Registered: 6-6-2018
Member Is Offline
|
|
Postulate:
It is not possible to heat an object to a temperature higher than the heater element temperature.
I hear this argument every now and then, and I always get bogged down, so let’s investigate.
Assume the element radiates according to Stefan-Boltzmann law, and by applying Wien's displacement law we can find the temperature of the element.
Now, to make things a bit cleaner, replace the heater elements by six identical pulsed CO2 lasers arranged like in the figure below. Each laser is
directed at a 1 g target consisting of Al2O3 powder. A CO2 laser will emit at around 10 um, and we assume that the pulse energy is 1 J.
![](https://i.postimg.cc/Y0kL58Tb/image.png)
The heat capacity for solid Al2O3 at room temperature is 90 J/(mol K), if all losses are ignored, the temperature of the target will rise about 1 K
for each pulse.
If all six lasers are fired simultaneously, the temperature of the target will rise 6 K. Repeat this 100 times and the target will be at around 600 K.
This is nothing spectacular, CO2 lasers are commonly used in industry for welding a range of different metals.
But, and here it comes, if our heater elements, the lasers, emit at a peak wavelength of 10 um, according to Wien's displacement law that corresponds
to a temperature of 290 K. How can an emitter at 290 K melt metals at around 1 500 K?
What is the difference if I replace the lasers with heated elements, like Nernst lamps, and mirrors to direct the energy at a focal spot? Obviously,
for all practical reasons, the energy required to increase the temperature 1 K of a sample at 1 000 K will be far greater compared to increasing the
temperature 1 K for a sample at room temperature. This is more of a fundamental question. Can you generally claim the stipulated postulate?
[Edited on 2022-1-31 by JohnnyBuckminster]
|
|
wg48temp9
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 770
Registered: 30-12-2018
Location: not so United Kingdom
Member Is Offline
|
|
JohnnyBuckminster:
Its the second law of thermodynamics that forbids heat flowing from a lower temperature to a high temperature under equilibrium conditions.
Yes you can melt steel with sunlight, because the sun's surface is at about 6,000 C , while steel melts at about 1500C
Wien's displacement law is applicable to blackbody radiation. The radiation from a laser does not have the spectrum of a black body so Wien's law can
not be used to convert the laser frequency to a meaningful blackbody temperature. For example blue LEDs are not at thousands of degrees.
I should add that it is possible to assign a temperature to electrons (and other particles) based on their velocity or energy. There are even
materials which are described as having a negative temperature based unusual definitions of temperature.
Perhaps an odd property of diffuse (Lambertian) matt and extended surfaces is they appear to have the same brightness when viewed through an optical
system near or far away. This effect prevents the intensity of heating effect form a heating element being increased by focusing the radiation from
the heating element using mirrors or lens.
Because lasers are not Lambertion (they can have diffraction limited parallel beams) they can be focused to increase their intensity. Heating elements
are Lambertion and can not be focused to increase their intensity.
I will try to find a better description of this effect. I will post a link to it if I do find a better description.
I am wg48 but not on my usual pc hence the temp handle.
Thank goodness for Fleming and the fungi.
Old codger' lives matters, wear a mask and help save them.
Be aware of demagoguery, keep your frontal lobes fully engaged.
I don't know who invented mRNA vaccines but they should get a fancy medal and I hope they made a shed load of money from it.
|
|
JohnnyBuckminster
Harmless
Posts: 40
Registered: 6-6-2018
Member Is Offline
|
|
Thanks for your comments wg48temp9, I enjoy these kind of discussions, so I dive straight in
1. Its the second law of thermodynamics that forbids heat flowing from a lower temperature to a high temperature under equilibrium
conditions.
The 2nd law of Thermodynamics does not prevent heat to flow from a colder to a hotter end as long as the net entropy generated in the Universe
increases. A laser has a typical efficiency of 50 %, so in the case of the furnace with six lasers focusing on a target, a lot of entropy will be
created in the surroundings. With heating elements it will get even worse, say only 5 % reach the target and 95 % of the energy is wasted to the
surroundings.
2. Yes you can melt steel with sunlight, because the sun's surface is at about 6,000 C , while steel melts at about 1500C
Let’s build a Dyson Sphere and collect every single photon emitted from the sun and direct the radiation at a block of Kryptonite 1 metre in
diameter placed in a thermos, i.e. a closed system. This will be an engineering challenge! If the temperature can’t exceed 6,000 C, and we are bound
by the 1st law of Thermodynamics, what happens with the “excess” energy hitting the Kryptonite block? We have the same energy, but it is localised
to a smaller space.
2. Wien's displacement law is applicable to blackbody radiation. The radiation from a laser does not have the spectrum of a black body so
Wien's law can not be used to convert the laser frequency to a meaningful blackbody temperature. For example blue LEDs are not at thousands of
degrees.
Imaging an observer located inside the furnace. All he ever will know is what he can see, and thus, he is clueless about what's behind the furnace
brick wall. One day he notices that the target material in the centre of his world gets warmer, and he traces this effect to an inflow of radiation
through “ports” in the furnace wall. Using a spectrograph he concludes that there is an inflow of radiation of wavelength 10 um that causes the
heating effect.
Let’s throw in a few more lasers at wavelengths to mimic blackbody radiation and direct them at the target, the observer inside the furnace will now
record an energy distribution similar to a black body radiation peaking at 10 um. He will probably use Wien’s displacement law and speculate about
the nature of this 290 K background radiation.
For the observer it doesn’t matter if it is a laser or a heating element that injects energy into his world, the effect is the same, it gets warmer.
3. Perhaps an odd property of diffuse (Lambertian) matt and extended surfaces is they appear to have the same brightness when viewed through
an optical system near or far away. This effect prevents the intensity of heating effect form a heating element being increased by focusing the
radiation from the heating element using mirrors or lens.
This might be the actual reason, it is not forbidden because it would violate any of the laws of thermodynamics, it is just not possible to collect
the energy and localise it to a smaller volume, in some analogy with a diffraction limited spot…. need to think a bit more about this...
Thanks for your your comments, food for thoughts...
|
|
Metallophile
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 82
Registered: 23-3-2018
Member Is Offline
Mood: No Mood
|
|
I remember a similar discussion years ago on an astronomy newgroup: Could you build a lens or mirror large enough to set something on fire, using the
light of the moon? If I remember correctly, the answer was no and the reason was the angular size of the moon.
|
|