Platinium/Titanium electrodes for sale (EU)
Im selling platinized expanded titanium mesh electrodes
specs: 40x95mm -1mm thickness
with attached handle in grade 2 1.5mm titanium 74 x 6mm
the electrodes are joined by spot welding
i dont know the exact thickness of the platinum coating, but just a single coating doesnt seem to fail under electrolysis and i give them 2 coatings
i also sell expanded titanium mesh electrodes as cathode as well as 316 stainless steel cathodes made in 3mm
Platinized titanium anode 40x95: 40 euro
https://gyazo.com/983ea5238e91f676970eb2b0bb4c6957
Expanded titanium mesh cathode: 10 euro
https://gyazo.com/f49ba712262dd56ce6f0664791313433
316 Stainless steel cathode: 2 euro
https://gyazo.com/0d5c3decc10b7ae94290716c89585301
in the industry straight up carbon steel is sometimes used as cathode so stainless should last an extra bit
shipping costs are 14 euro in europe
methylene blue positive test
https://gyazo.com/fe0c3276084f75e9dd3bccab2b5fed57
i can also make larger electrodes upon request, i have some solid titanium sheet laying around still, or smaller ones too.
|
|
B(a)P
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1132
Registered: 29-9-2019
Member Is Offline
Mood: Festive
|
|
Any reason you only ship to the EU?
|
|
Fantasma4500
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1681
Registered: 12-12-2012
Location: Dysrope (aka europe)
Member Is Offline
Mood: dangerously practical
|
|
i can ship to all countries at same price but im based in EU, it appears to be exact same shipping price to all countries.
u2u if interested.
|
|
Herr Haber
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1236
Registered: 29-1-2016
Member Is Offline
Mood: No Mood
|
|
Is this for real or am I still asleep ? I went to bed yesterday or the day before thinking about quality electrodes...
I thought it would be nice if someone from SM could point me to a trusted and reliable source for such electrodes.
Any details on the manufacture to give us an idea on how long they could last would probably be interesting.
PM tonight with my order
The spirit of adventure was upon me. Having nitric acid and copper, I had only to learn what the words 'act upon' meant. - Ira Remsen
|
|
Fantasma4500
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1681
Registered: 12-12-2012
Location: Dysrope (aka europe)
Member Is Offline
Mood: dangerously practical
|
|
well there are some strict parameters for running a platinum electrode but in optimum conditions electrolysis electrodes can last up to 20 years, so
its unlikely that anyone on sciencemadness would even end up stresstesting these things so much that it does end up falling apart- maybe excluded
bromide electrolysis- dont do that with titanium substrate.
i might also add i have some much cheaper grade of titanium stretch, china quality, maybe half a millimeter, but the surface area is greater so i can
sell those too as cheaper cathodes- even after one of those was used as anode for an amount of hours its still good to go as cathode
i suppose this thinner grade titanium with platinum deposited on would be especially great for stuff like catalytic oxidation of alcohols as you can
cut it to shape with a metal shear by hand, roll it up and put into a pipe and dump methanol fumes through maybe.
but about 1L concentrated solution of NaClO3 with some NaCl in it was turned into NaClO4 without visible deteoriation of the anode, while running it
at merciless amps.
|
|
Herr Haber
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1236
Registered: 29-1-2016
Member Is Offline
Mood: No Mood
|
|
My package arrived yesterday !
I ordered 2 of each, unsure if I wanted a spare or just a potential gift.
I have no experience with this kind of electrode and cant estimate their lifespan or performance with my eyes only.
Under a magnifying glass they look absolutely perfect. No defect in the coating, it might be a little bit thicker on one of the edges but this might
be an optical effect only.
The welds are definitely not going to break and make good contact. It's quality work, no doubt about that.
I'm happy with my purchase, glad it came from a forum member and totally recommend him.
Oh, and I got a shiny shiny piece of MgAl as a bonus ![:)](./images/smilies/smile.gif)
Unless life has more unpleasant surprises for me I should be testing them soon. I'll probably be traveling next week to a funeral.
The spirit of adventure was upon me. Having nitric acid and copper, I had only to learn what the words 'act upon' meant. - Ira Remsen
|
|
B(a)P
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1132
Registered: 29-9-2019
Member Is Offline
Mood: Festive
|
|
I have also placed an order. Unfortunately I don't currently have a fixed address so it won't be delivered until I do, though I have seen a picture of
the completed electrodes and can't wait to put them to use.
|
|
Fantasma4500
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1681
Registered: 12-12-2012
Location: Dysrope (aka europe)
Member Is Offline
Mood: dangerously practical
|
|
yes i ordered more titanium mesh so i can do at least 10 more platinum anodes
for some reason the titanium plates i can get cant be chemically pre-treated so i prefer to do mesh instead, if someone wants a bigger anode i can
just weld multiple anodes together
|
|