I'm doing an extraction with pentane, which I understand can be used to remove joint grease when cleaning glass. So if I use grease in assembling the glassware, can I assume that the chances are good of contaminating my extract?

If that's the case, is my only option using sleeves? What if I don't use anything? Achieving vacuum is not necessary.
View user's profile View All Posts By User
dawt
Hazard to Self
**




Posts: 74
Registered: 9-5-2016
Location: EU
Member Is Offline

Mood: fluorescent

[*] posted on 7-4-2021 at 21:30


Glycerine works well in those cases, as does a paste made from glycerine and starch. You can also get away with not using a sealant, but on the off-chance your glassware does get stuck you'll curse yourself for not investing those 10 seconds. :)



View user's profile View All Posts By User
itsallgoodjames
Hazard to Others
***




Posts: 276
Registered: 31-8-2020
Location: America Lite
Member Is Offline


[*] posted on 8-4-2021 at 05:41


Quote: Originally posted by dawt  
but on the off-chance your glassware does get stuck you'll curse yourself for not investing those 10 seconds. :)

This is why you keep around a piece of wood dedicated to lightly tapping stuck ground glass joints to dislodge them




Nuclear physics is neat. It's a shame it's so regulated...

Now that I think about it, that's probably a good thing. Still annoying though.
View user's profile View All Posts By User
electrokinetic
Hazard to Self
**




Posts: 52
Registered: 6-6-2012
Location: Rhuidean
Member Is Offline

Mood: No Mood

[*] posted on 8-4-2021 at 09:54


I'll try the glycerin and starch route. I have the wood, but would rather not have to use it.

Thanks both!
View user's profile View All Posts By User
Panache
International Hazard
*****




Posts: 1290
Registered: 18-10-2007
Member Is Offline

Mood: Instead of being my deliverance, she had a resemblance to a Kat named Frankenstein

[*] posted on 10-4-2021 at 05:32


depends on how good your joints are. this cuts both ways as in if they are married well you can lose little without using grease but they are more likely to seize. If they are crappy you are compromised with or without grease...
Red wax is an old school high vacuum thread sealant that works well on gg joints. if i recall its one part iron oxide one part beeswax one part paraffin something...pentane wont take off every joint grease. the fluorinated high mw corning stuff is essentially insoluble in everything except itself.
i cant stand the sleeves, dont know why, they just seem so unnecessary, rather like this reply really, god what an inane 6 lines....lmao.
View user's profile View All Posts By User
monolithic
Hazard to Others
***




Posts: 436
Registered: 5-3-2018
Member Is Offline

Mood: No Mood

[*] posted on 10-4-2021 at 05:51


PTFE plumber's tape is much, much cheaper than purpose made sleeves.
View user's profile View All Posts By User
Junk_Enginerd
Hazard to Others
***




Posts: 251
Registered: 26-5-2019
Location: Sweden
Member Is Offline


[*] posted on 10-4-2021 at 07:59


I use Krytox. PTFE grease. Though I only use it for things I don't mind having PTFE grease on them until the end of time lol, that does not come off with any solvent.