Synthesis of Acetophenone


Synthesis of Acetophenone

Introduction

Acetophenone is an aromatic ketone with a pleasant odor. It is a chemical that has many uses as a precursor and as a flavoring for various foods. In this experiment Acetophenone is prepared from benzene and acetic anhydride with anhydrous aluminum chloride.
WARNING! This reaction deals with corrosive acids, toxic fumes and poisonous liquids. It is advised not to perform this unless you are a trained chemist with proper laboratory equipment. This is to be performed in a fumehood.

This is a classic example of a Friedel Crafts acylation. A mechanism for the reaction can be found at this link:
http://www.chm.wright.edu/feld/chm216/CHM%20216%20Ex%205%20F...

Table of Reagents
120g anhydrous aluminum chloride
185mL anhydrous benzene
36mL acetic anhydride
450mL concentrated hydrochloric acid
450g crushed ice
50mL diethyl ether
50mL 10% sodium hydroxide solution
Reaction

A 1L 3-neck RBF was set up on a cold water bath that could be raised or lowered. To the top neck a mechanical stirrer was added. To another neck a 60mL addition funnel containing the acetic anhydride was added and to the third neck a reflux condenser was added with a gas trap connected to the top. The gas trap consisted of an inverted funnel into a beaker of water with a drying tube in between in case moist air were to be sucked into the system. Stirring was started and the ice bath was raised. The acetic anhydride was slowly dripped into the flask over the course of 30mins. There was some sort of white solid residue that build up where the acetic anhydride was being dripped in, it eventually fell in and bubbled vigorously. Once all the acetic anhydride had been added the mixture was refluxed for an hour. The reaction mixture turned a deep orange/brown colour part way through the acetic anhydride addition. At the start of the reflux period the mixture fizzed smoothly. A lot of hydrogen chloride gas could be seen dissolving into water in the gas trap. Once reflux was done the heat was removed and the reaction was allowed to cool back down to room temperature on its own. Near the end of reflux there was no more hydrogen chloride being emitted.
Work-Up

The cooled reaction mixture was poured into a mixture of 450mL concentrated hydrochloric acid and 450g of ice. WARNING! THIS STEP IS VERY VIOLENT. The quenching of the reaction mixture liberated enormous amounts of heat and hydrogen chloride and probably lots of benzene fumes. Once the reaction had all been poured into the ice/HCl mixture it was stirred for 15 mins to fully quench the organic layer. The mixture was then transferred to a separatory funnel with 25mL of ether. The funnel was well shaken and the aqueous layer and organic layer were separated into different Erlenmeyer flasks. The aqueous layer was then extracted with another 25mL portion of ether. Remove the aqueous layer and discard it. Add the organic layer back into the separatory funnel and wash it with two 25mL portions of a 10% sodium hydroxide solution. Drain the organic layer into a clean Erlenmeyer flask and dry it with anhydrous magnesium sulfate.
Purification

Take the organic layer and remove the ether/benzene mixture by distilling off on a water bath, or use a rotovap if available. Once all of the solvent has been removed, transfer the crude Acetophenone to a clean distillation apparatus and distill using an air condenser. Collect the fraction boiling between 195-202 C. Pure Acetophenone should be clear and I obtained a product that was slightly tan in colour. The Acetophenone was then redistilled to collect a perfectly clear sweet cherry scented liquid. The total weight of Acetophenone obtained was 32.94g which was a 71.8% yield based off acetic anhydride. The melting point of the obtained Acetophenone was 17.2-19.5 C. The Acetophenone was collected boiling between 200-201C in the second distillation. The lit. value for the boiling point of acetophenone is 202C. The lit. value for the melting point of acetophenone is 19-20C.

Important Notes about the reaction:
-The glassware must be absolutely anhydrous as water decreases the yield. For this procedure all of the glassware was flame dried
-The benzene must be dried and it is advantageous to remove any sulfur impurities as it may interfere with the reaction, the benzene used in this procedure was purified as per Vogel 3rd Ed to remove thiophene. The benzene was then dried using anhydrous magnesium sulfate and 3A molecular sieves, filtered then distilled
-The chemicals used in this experiment are TOXIC!, especially the benzene and anhydrous aluminum chloride. This procedure is to be preformed in an efficient fumehood, especially during the quenching stage.
-The Acetophenone can be distilled under a vacuum but it works just as well to distill it under atmospheric pressure. The distillation may only need to be performed once if one is very careful to take many fractions to avoid the tan contamination which seems to come over before the Acetophenone.
References
(1) Vogel, A.: Aromatic Ketones. A text-book of Practical Organic Chemistry Including qualitative organic analysis; 3rd Ed.; No Editors, Eds; Lowe and Brydone, 1956, pp 729-730.

New Picture.png - 150kB
The acetophenone after the first distillation. It's hard to see but it has a light tan colour
New Picture (2).png - 168kB
The residue left in the flask after the first distillation
New Picture (3).png - 130kB
The distillation set up
New Picture (4).png - 106kB
The acetophenone after it's second distillation, it crystallized into a beautiful mass of crystals. The liquid before it solidified was a perfectly clear colourless liquid with a sweet cherry smell.

[Edited on 31-10-2012 by Mercedesbenzene]
View user's profile View All Posts By User
Mildronate
Hazard to Others
***




Posts: 428
Registered: 12-9-2009
Member Is Offline

Mood: Ruido sintetico

[*] posted on 31-10-2012 at 13:08


if ou whant make bromketone from it i can sell you bromketone :)
View user's profile View All Posts By User
Magpie
lab constructor
*****




Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline

Mood: Chemistry: the subtle science.

[*] posted on 31-10-2012 at 14:13


Nice work. I like the fact that you took the time and effort to purify your reagents. It paid off with a good yield of high purity product. Here are some suggested additions to improve pedagogic value and readability:

1. This is a Friedel & Crafts synthesis is it not? If so this should be so stated.
2. Show the chemical reaction.
3. State the literature values for the mp and bp.




The single most important condition for a successful synthesis is good mixing - Nicodem
View user's profile View All Posts By User
Mercedesbenzene
Hazard to Self
**




Posts: 64
Registered: 4-9-2011
Location: BC
Member Is Offline

Mood: Sub Zero

[*] posted on 31-10-2012 at 15:24


Good ideas, thanks Magpie, and I am not using it to make a bromoketone, thanks for the offer though
View user's profile View All Posts By User
bbartlog
International Hazard
*****




Posts: 1139
Registered: 27-8-2009
Location: Unmoored in time
Member Is Offline

Mood: No Mood

[*] posted on 2-11-2012 at 14:47


Nice work! Some pedantic quibbles with the writeup:
- the contents of the three-necked RBF should be described. I realize that those familiar with this synthesis will after a moment of bogglement realize that the flask has been charged with benzene and AlCl3 prior to the addition of the acetic anhydride, but as long as you're describing the steps take a moment and say so...
- since your table of reagents includes some stuff needed in the workup (like ether) you might as well list the anhydrous magnesium sulfate you use for drying the organic phase (in the work-up section) as well
- towards the end of the work-up section you switch from the standard passive tense ('The aqueous layer was then extracted...') to the imperative ('Add the organic layer back...'). Jarring, and anyway since it's a writeup of a synthesis you performed you might as well describe it all in the passive tense.




The less you bet, the more you lose when you win.
View user's profile View All Posts By User
gdflp
Super Moderator
*******




Posts: 1320
Registered: 14-2-2014
Location: NY, USA
Member Is Offline

Mood: Staring at code

[*] posted on 28-5-2015 at 17:15


I realize that the OP hasn't been active for a while, I just wanted to note what I believe may be a mistake. The amount of hydrochloric acid and ice used for workup are double that which Vogel recommends, while the amounts of ether and sodium hydroxide used are 2/3 that recommended by Vogel. Not sure if there was a specific reason for this, just thought I would mention it.



View user's profile View All Posts By User
aab18011
Hazard to Self
**




Posts: 75
Registered: 11-7-2019
Location: Connecticut, USA
Member Is Offline

Mood: Moving out and setting up shop in my new chemistry hobbit hole

[*] posted on 26-3-2021 at 00:59


I understand that this thread is dead, but I was attempting to make myself some acetophenone and was wondering if I can use Acetyl Chloride instead. I am set to made Acetyl Chloride from PCl5 and Anhydrous Acetic Acid, which I do have the equipment for. But I also have the ability to buy acetic anhydride as well. I would like to avoid buying it due to its regulation here in my state, as well as I don't need it at the moment.



I am the one who boils to dryness, fear me...
H He Li B C(12,14) Na S Cl Mn Fe Cu Zn Ba Ag Sn I U(238)
"I'd rather die on my feet than live on my knees" -Emiliano Zapata
View user's profile Visit user's homepage View All Posts By User
outer_limits
Hazard to Others
***




Posts: 139
Registered: 3-3-2020
Member Is Offline

Mood: hybridized

[*] posted on 26-3-2021 at 03:37


Of course - you can use acetyl chloride.
And then you need just a ~1.1 molar equivalent of AlCl3 instead of ~2.2 when using anhydride.
View user's profile View All Posts By User
Yorty2040
Harmless
*




Posts: 41
Registered: 1-2-2024
Member Is Offline


[*] posted on 26-5-2024 at 18:15


Would replacing the 36mL of acetic anhydride with 53mL of trifluoroacetic anhydride be the only change to the procedure required to produce the alpha-trifluoro derivative of acetophenone, or would further modifications be necessary?

Other than to the purification steps, obviously, since the boiling point is different.

[Edited on 27-5-2024 by Yorty2040]