how to chemically waterproof sodium silicate coating


I plan on making a machine out of cast aluminium, and some moving parts i want to coat with a solution of sodium silicate (Na2O:3SiO2). After drying without boiling, it should make a layer of true glass, and solve the abrasion problem of bare aluminium.

But since in theory the coating could be redissolved by moisture,
Is there a way to treat the surface so it becomes insoluble? For example, if i put it in molten calcium nitrate, would the surface become insoluble soda lime glass?
View user's profile View All Posts By User
Boffis
International Hazard
*****




Posts: 1843
Registered: 1-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 20-12-2020 at 10:15


Sodium silicate solution is very alkaline and attacks aluminium. You will not get a glassy layer at room temperature but you will get an amorphous layer sodium aluminium silicate. If subjected to steam or atleast moderately elevated temperatures in the presence of water you may get a clay or zeolite like coating but I doubt it will be particularly abrasion resistant.
View user's profile View All Posts By User
rockyit98
Hazard to Others
***




Posts: 283
Registered: 12-4-2019
Location: The Known Universe
Member Is Offline

Mood: no mood is a good mood

[*] posted on 20-12-2020 at 10:21


anodize Al first. maybe try one of that ceramic coating paint.



"A mind is a terrible thing to lose"-Meisner
View user's profile View All Posts By User
Fulmen
International Hazard
*****




Posts: 1698
Registered: 24-9-2005
Member Is Offline

Mood: Bored

[*] posted on 20-12-2020 at 12:10


I agree. Your focus should be on anodizing. It's really not hard: A "dumb" 12V charger and 10-15% sulfuric acid. Make sure to keep the bath cool. Cook for 30 minutes and Bob's your uncle.



We're not banging rocks together here. We know how to put a man back together.