[*] posted on 25-11-2020 at 18:21
Help, I think I accidentally made copper nanoparticles.


I was trying to use electrolysis to remove copper from some graphite electrodes and I put these electrodes as anodes in a sodium chloride solution and as cathode I used a stabdard graphite rod(no cooper here) and connected to a 20v 3.6A power supply, the current drawn was about 2A, at the beginning it as all as I expected, the blue oxide started to preciptate, but then a black stuff started forming, and it turned all black(like the paint it black from the Rolling Stones) and brownish black stuff and it got hot, but at the bottom cold as usual... I turned it off, and I was left with a fine dark suspension that slowly (took days) to precipitate and eveb then, when I shine a laser beam it shows floating particles, I got a couple of photos, sorry, not so good quality though, but it will help you get the Idea of what I'm talking about.

I'm not sure of what it is nor what to do with it, I googled applications of copper nanoparticles and it seems that there isn't much I could do with it.

IMG_20201125_165142244~2.jpg - 667kBIMG_20201125_165139947~2.jpg - 275kB




"NOOOOOO!!! The mixture is all WROOOOOOONG!"
View user's profile View All Posts By User This user has MSN Messenger
Bedlasky
International Hazard
*****




Posts: 1225
Registered: 15-4-2019
Location: Period 5, group 6
Member Is Offline

Mood: Volatile

[*] posted on 25-11-2020 at 18:45


It is mix of graphite and CuO. Cu(OH)2 decompose at 80°C to CuO and water.

20V is too high voltage. You don't need that high voltage for this electrolysis.