I'm browsing the Better Equipped site (https://www.betterequipped.co.uk) and in addition to regular glassware with ground glass connections they also offer glassware with ground glass connections called "PLUS" jointed. Does anyone know what the PLUS stands for and how its different from the other stuff?

Here's an example of PLUS jointed glassware: https://www.betterequipped.co.uk/a-plus-jointed-chemistry-ki...

Thanks
View user's profile View All Posts By User
elapid
Harmless
*




Posts: 2
Registered: 17-8-2020
Location: UK
Member Is Offline


[*] posted on 17-11-2020 at 07:40


I think it is their own brand of Quickfit - I cant see any difference
View user's profile View All Posts By User
danton
Harmless
*




Posts: 6
Registered: 13-11-2019
Member Is Offline


[*] posted on 17-11-2020 at 10:19


Quote: Originally posted by elapid  
I think it is their own brand of Quickfit - I cant see any difference


Yes, maybe. I'll email them and ask.
View user's profile View All Posts By User
danton
Harmless
*




Posts: 6
Registered: 13-11-2019
Member Is Offline


[*] posted on 20-11-2020 at 02:56


So here's their reply to my enquiry:

"Thanks for the mail.
We have three brands of jointed glassware :

Glassco is basic economy range
Labglass mid range
And A PLUS premium range

All compatible with the brand ‘Quickfit’ which we don’t currently supply.

The A PLUS range is precision engineered which is why the price is much higher.
All brands should be fit for purpose."

View user's profile View All Posts By User
Fery
International Hazard
*****




Posts: 1000
Registered: 27-8-2019
Location: Czechoslovakia
Member Is Offline


[*] posted on 20-11-2020 at 07:23


I experienced something according the fitting of joints. Here I can buy a glass from local manufacturer (Simax), ground glass joints fit always perfectly, very little of silicone grass and every connection perfectly tight and completely transparent for hours/days. I've also bought a glass from china and the joints seem to fit well for the first sight, but when the temperature increases (e.g. distillation) I see the grass concentrating in one half of the joint (where force applies) and second half of the joint on the opposite side contains mostly strait gap filled with air - joints seem to be still tight enough and no signs of any leak, perhaps 1-2 mm ring where the grass is completely circularly is enough...
Anyway I switched from grass to ptfe sleeves for the Simax glass (would be better for no such good fitting Chinese joints).




View user's profile Visit user's homepage View All Posts By User
Fyndium
International Hazard
*****




Posts: 1192
Registered: 12-7-2020
Location: Not in USA
Member Is Offline


[*] posted on 20-11-2020 at 13:25


The only PLUS that comes in mind could be when cashing out their bonuses.

I do agree that some very cheap chinese joints have had some play with them, but the difference to DURAN glassware has so far been minor to nonexistent. Nothing that a little paraffin grease wouldn't fix. I have had to apply some during vacuum distillations, but the very minor bubbling stopped quickly when the glass settled. It's fun to think that stream of effervescence through ebulliator that is draw more fine than a strand of hair expands into huge, multiple-cm sized bubbles.
View user's profile View All Posts By User
macckone
International Hazard
*****




Posts: 2160
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline

Mood: Electrical

[*] posted on 20-11-2020 at 15:30


It is a UK based brand: https://aplusinterchange.com/
View user's profile View All Posts By User
Chemetix
Hazard to Others
***




Posts: 375
Registered: 23-9-2016
Location: Oztrayleeyah
Member Is Offline

Mood: Wavering between lucidity and madness

[*] posted on 20-11-2020 at 18:53


Indian glass, I can tell from the blue decal and it's font on the joint indicating the joint size.
View user's profile View All Posts By User
Clear_horizons_glass
Harmless
*




Posts: 42
Registered: 30-9-2019
Location: Pullman, WA
Member Is Offline

Mood: Glass

[*] posted on 23-11-2020 at 01:03


Glassco is an India brand.
https://www.glasscolabs.com/

So I would assume labglass is from China?

This thread has been quite informative.

From my experience, there's not a lot of difference in terms of workability, but the main differences are in terms of regulations and labor laws of the countries they are from, and the quality of the shipping and packaging. A box of Chinese joints will come packed in a box and wrapped in paper, some may b broken, and the joints are rough cut. German joints come in a nicely packaged box with flame polished ends.
Also, in a way, some of all the glass is from China. As I don't think there are many other sources for the Boron necessary to make Borosilicate glass.





Clear Horizons Laboratory Glassblowing Services
-------------------------------------------------------------
www.clearhorizonsglass.com
Phone and Fax:
(855) LAB-GLAS
(855) 522-4527
Have a glass project you want made? email me at
info@clearhorizonsglass.com
or message us here |
with a U2U |
message |
\/
View user's profile Visit user's homepage View All Posts By User

  Go To Top