Batteries are Friggin Complicated Yo (also voltage determination)
Preface: I actually have very little knowledge in regards to electrochemistry. I'd like to do some more analytical experiments with batteries, but I
decided to start small here. The point of today's experiment was to measure voltage between two different setups and observe any differences.
Setup
4 beakers, 2 of which were 50 mL and 2 of which were 100 mL, were both filled with their respective volumes of water. Call the 100 mL set A and the 50
mL set B.
Magnesium Sulfate was then added to both sets of beakers in 10 gram portions for set A and 5 gram portions for set B to ensure equal concentration of
the electrolyte solution in both sets.
Unfortunately, this is where I failed to be scientific and accurate in my little experiment. Originally, I wanted to use known metals for the
terminals, but all I had were some copper and zinc coins lying around. Despite all my best efforts, I could not securely attach the coins to the sides
of the beakers while immersing them in the electrolyte solution. I was forced to use a nail and screw of different but unknown metal to act as the
terminals. The screw was bronze, and the nail was probably iron. Here is what the setup looked like:
![](https://i.ibb.co/SttHsRv/20200929-110433.jpg)
First the 100 mL beakers were measured using a multimeter across both the nail and screw, and the voltage measured ranged between .3 volts to .4
volts. This was consistent across both beakers in set A.
Next the 50mL beakers were measured using the same nail and screw. Both beakers in set B showed a consistent voltage reading peaking at around .395
volts.
Before I come to my conclusion, there are a couple observations I'd like to make regarding the measurements.
O1) Each beaker was measured multiple times to account for variations in readings, but all readings were fairly consistent.
O2) The voltage in each beaker was noticed to peak at around .4 volts, and then suddenly drop back down again to a lower voltage, and slowly climb
back up to the .4 volt mark after 2-3 seconds.
Conclusion
If the concentration of electrolyte is constant, then changing the volume of liquid will not affect voltage.
This might sound like an extremely obvious "no s*** you f****** d******" moment, however I think it will be useful in terms of deciding what volume
quantities to work with in the future. Hopefully this means I can work on fairly small scales.
Questions
Q1) Did I make a battery? Can that be considered a battery? Or was I merely getting readings on my multimeter from some EM concept I don't fully grasp
yet
Q2) Why did I notice the change in voltage over time as described in O2?
Thoughts/comments appreciated all ^^
-Cap'n Rum the Science Bum
|
|
Tsjerk
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 20-4-2005
Location: Netherlands
Member Is Offline
Mood: Mood
|
|
The volume of the electrolyte shouldn't make a difference in voltage, this will only correlate to the capacity of the battery.
Yes, you did make a battery.
I think the change in voltage comes from the bubbles made at the anode and cathode. They will make the surface of the electrodes smaller. That
shouldn't matter in a perfect environment but probably does in this.
|
|
arkoma
Redneck Overlord
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1761
Registered: 3-2-2014
Location: On a Big Blue Marble hurtling through space
Member Is Offline
Mood: украї́нська
|
|
Any two dissimilar metals in a electrolyte will produce a "potential difference" (voltage). An interesting experiment would be to use electrodes of
as many different types of metals you can get your hands on, and different electrolytes. One can also take dissimilar coins and stack them alternately
with a piece of electrolyte soaked blotter paper in between each layer. Each set of two coins is a "cell", and the stack is a battery.
"We believe the knowledge and cultural heritage of mankind should be accessible to all people around the world, regardless of their wealth, social
status, nationality, citizenship, etc" z-lib
|
|
markgollum
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 53
Registered: 21-2-2004
Member Is Offline
Mood: No Mood
|
|
I would say that because open circuit voltage is a thermodynamic property of the system, that the varying voltage seems to be more likely due to
contact resistances of the components.
In general, a higher resistance multimeter can sometimes help when measuring voltages with high resistances in series with the voltage source.
|
|