Pages:
1
2 |
Loptr
International Hazard
   
Posts: 1348
Registered: 20-5-2014
Location: USA
Member Is Offline
Mood: Grateful
|
|
Sodium Borohydride Group Buy
Hey guys,
A few people have reached out to me about the potential for a Sodium Borohydride group buy. I am curious to see how many people would be interested in
participating, so if you are interested please say so in a comment below.
The price will be a lot lower than I was previously selling it for at the $0.50/gram price mark. However, I will only be selling it in kilogram
increments. I will also be requiring a %50 payment upfront to help with the costs of the material and shipping. I will also only be shipping to North
America. I am a respectable and trustworthy guy, otherwise you would have heard about it on these forums. I have been selling here, eBay, and
elsewhere for quite a while now, so I know how this works.
The more people that show interest, the lower the price goes, so be sure to leave a comment showing your interest. You aren't committing to anything
at this point as I just need a guesstimate of what to expect, so that I can submit a quote to my supplier that I have dealt with previously on several
occasions.
Also, if you want to work something out, I am willing to entertain. Send me a message.
I am going to keep this interest check open for 1 month, so the end date will be 10/15/2019.
Cheers! 
[Edited on 15-9-2019 by Loptr]
"Question everything generally thought to be obvious." - Dieter Rams
|
|
Loptr
International Hazard
   
Posts: 1348
Registered: 20-5-2014
Location: USA
Member Is Offline
Mood: Grateful
|
|
Bump.
"Question everything generally thought to be obvious." - Dieter Rams
|
|
j_sum1
|
Thread Topped 16-9-2019 at 18:56 |
j_sum1
Administrator
      
Posts: 6367
Registered: 4-10-2014
Location: At home
Member Is Offline
Mood: Most of the ducks are in a row
|
|
Sticky for a month.
Remind me when time's up.
|
|
Loptr
International Hazard
   
Posts: 1348
Registered: 20-5-2014
Location: USA
Member Is Offline
Mood: Grateful
|
|
Thanks, j_sum1!
"Question everything generally thought to be obvious." - Dieter Rams
|
|
Tsjerk
International Hazard
   
Posts: 3035
Registered: 20-4-2005
Location: Netherlands
Member Is Offline
Mood: Mood
|
|
Why the change to only North America?
|
|
Loptr
International Hazard
   
Posts: 1348
Registered: 20-5-2014
Location: USA
Member Is Offline
Mood: Grateful
|
|
The packages will be over a kilogram and air shipping requires additional shipping requirements that I would have to research. I could probably do
that, if I have enough non-North American members interested.
Who else would be interested that isnt in North America? Should I open this to the world?
[Edited on 17-9-2019 by Loptr]
"Question everything generally thought to be obvious." - Dieter Rams
|
|
j_sum1
Administrator
      
Posts: 6367
Registered: 4-10-2014
Location: At home
Member Is Offline
Mood: Most of the ducks are in a row
|
|
Maybe we could have another crack at getting an aussie package done. I am thinking one quantity sent over for division and redistribution.
I don't mind doing the organisation, but it would need to be a cash-up-front kind of a deal. And the shipping costs would obviously be higher.
Post desired quantities here if you want to be part of this. If there is enough interest we can discuss cash via u2u.
|
|
TD64209
Harmless
Posts: 13
Registered: 12-6-2019
Member Is Offline
|
|
Definitely interested, consider me in.
(North America)
[Edited on 21-9-2019 by TD64209]
|
|
myr
Harmless
Posts: 48
Registered: 18-7-2018
Member Is Offline
|
|
I would be interested
|
|
j_sum1
Administrator
      
Posts: 6367
Registered: 4-10-2014
Location: At home
Member Is Offline
Mood: Most of the ducks are in a row
|
|
Bumping this.
Any aussies interested in a group buy?
https://www.sciencemadness.org/whisper/viewthread.php?tid=15...
|
|
carrant
Harmless
Posts: 39
Registered: 19-3-2015
Location: Dallas, Tx
Member Is Offline
Mood: No Mood
|
|
I would be interested.
USA
|
|
OldNubbins
Hazard to Others
 
Posts: 136
Registered: 2-2-2017
Location: CA
Member Is Offline
Mood: Comfortably Numb
|
|
Interested
USA
|
|
Loptr
International Hazard
   
Posts: 1348
Registered: 20-5-2014
Location: USA
Member Is Offline
Mood: Grateful
|
|
If you state interest, could you also be sure to let us know the country in which you reside?
@myr, where are you from?
"Question everything generally thought to be obvious." - Dieter Rams
|
|
Tdep
National Hazard
  
Posts: 519
Registered: 31-1-2013
Location: Laser broken since Feb 2020 lol
Member Is Offline
Mood: PhD is done! It isn't good but it's over lol
|
|
Shipping 1kg US to Aus is pretty dang expensive, is there scope to do 500g (where I believe the price is reduced quite a bit?) or is it all 1 kg bags?
Probably asking a bit much I know sorry
|
|
draculic acid69
International Hazard
   
Posts: 1371
Registered: 2-8-2018
Member Is Offline
|
|
It couldn't cost that much to send a kilo from usa could it?
I might be in for a hundred or so grams.
|
|
Uvxtal76
Harmless
Posts: 3
Registered: 24-10-2019
Member Is Offline
|
|
I am interested.
|
|
Loptr
International Hazard
   
Posts: 1348
Registered: 20-5-2014
Location: USA
Member Is Offline
Mood: Grateful
|
|
Quote: Originally posted by Tdep  |
Shipping 1kg US to Aus is pretty dang expensive, is there scope to do 500g (where I believe the price is reduced quite a bit?) or is it all 1 kg bags?
Probably asking a bit much I know sorry |
When I start getting quotes I can ask about 500g pouches.
"Question everything generally thought to be obvious." - Dieter Rams
|
|
tetraiodide
Harmless
Posts: 16
Registered: 8-6-2018
Member Is Offline
|
|
I'm deffinatly interested if this hasn't already gone by
|
|
Doc B
Hazard to Others
 
Posts: 107
Registered: 5-4-2012
Member Is Offline
Mood: No Mood
|
|
There is plenty in Oz. PM if interested.
|
|
smdftbh
Harmless
Posts: 1
Registered: 12-11-2019
Member Is Offline
|
|
I'm interested, North America
|
|
Phosgenetimemachine
Harmless
Posts: 6
Registered: 25-1-2018
Member Is Offline
Mood: No Mood
|
|
I don;t suppose this oporotunity is still available by chance?If so then I am interested???
|
|
nzlostpass
Hazard to Self

Posts: 66
Registered: 3-9-2019
Member Is Offline
|
|
Can anyone sell me some please? Even 50g would help.......I'm in NZ but happy to pay for shipping. Bought some from Poland but theres no postage from
there to here since February.
|
|
mackolol
Hazard to Others
 
Posts: 459
Registered: 26-10-2017
Member Is Offline
Mood: Funky
|
|
Quote: Originally posted by nzlostpass  | Can anyone sell me some please? Even 50g would help.......I'm in NZ but happy to pay for shipping. Bought some from Poland but theres no postage from
there to here since February. |
Which company did you buy it from?
|
|
nzlostpass
Hazard to Self

Posts: 66
Registered: 3-9-2019
Member Is Offline
|
|
It was on Ebay.....ChemPL or something similar
I'm also waiting on something from Mario since February due to the postal service.
|
|
zed
International Hazard
   
Posts: 2285
Registered: 6-9-2008
Location: Great State of Jefferson, City of Portland
Member Is Offline
Mood: Semi-repentant Sith Lord
|
|
Postal Service? I'm on the West Coast of the U.S.; adequate postal service depends on where it is coming from.
Our postal service has been politicized. I no long order from China. The last item I ordered, took not three weeks to arrive, but rather it took
three months. Where the hang up is, I do not know. But, it is too much to bear.
Last week, I got shipments from both Poland and Canada. My parcel from the East Coast of Canada (about 3000 miles away) arrived about a week after
it was shipped. Even though it made at least half a dozen stops along its route. Customs etc, etc, etc...
My Parcel from Poland was in transit for about a month. I think. Tracking international parcels is a murky business. I get a notice when it is
posted. Then I hear nothing, at all. Weeks or months pass, and then, the parcel is abruptly delivered.
At the moment, I am awaiting PPE from Israel. It will arrive or it won't. Only time will tell.
Parcels posted within the U.S. are eminently traceable. Mail, UPS, FedEx... You always know where your package is. It's a big country, but most
things get to me within in a week or so.
Service was even better, early in the pandemic. The U.S. postal service has been temporarily slowed down by political intervention.
|
|
Pages:
1
2 |