Stoichiometry of the reaction of ascorbic acid and copper sulfate
I am interested in doing the reaction of ascorbic acid and copper sulfate to produce copper powder. I like to do my reactions very close to the
stoichiometric amounts, but I can't find any information on the reaction except for that it exists. I probably just missed something, so could someone
help me?
Collected elements:
Al, Cu, Ga, C (coal), S, Zn, Na
Collected compounds:
Inorganic:
NaOH; NaHCO3; MnCl2; MnCO3; CuSO4; FeSO4; aq. 30-33% HCl; aq. NaClO; aq. 9,5% ammonia; aq. 94-96% H2SO4; aq. 3% H2O2
Organic:
citric acid, sodium acetate, sodium citrate, petroleum, mineral oil
|
|
Tsjerk
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 20-4-2005
Location: Netherlands
Member Is Offline
Mood: Mood
|
|
Should be 1:1.
Ascorbic acid loses two electrons while forming dehydroascorbic acid.
|
|
Draeger
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 185
Registered: 31-1-2020
Location: North-Rhine Westfalia, Germany
Member Is Offline
Mood: Slowly getting ready for new projects
|
|
Alright. Thank you.
Collected elements:
Al, Cu, Ga, C (coal), S, Zn, Na
Collected compounds:
Inorganic:
NaOH; NaHCO3; MnCl2; MnCO3; CuSO4; FeSO4; aq. 30-33% HCl; aq. NaClO; aq. 9,5% ammonia; aq. 94-96% H2SO4; aq. 3% H2O2
Organic:
citric acid, sodium acetate, sodium citrate, petroleum, mineral oil
|
|
UC235
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 565
Registered: 28-12-2014
Member Is Offline
Mood: No Mood
|
|
To avoid under-reduction and formation of Cu(I) species, I would advise a generous excess of ascorbic acid.
|
|