Pok
potassium Prometheus
***




Posts: 176
Registered: 5-12-2010
Member Is Offline


[*] posted on 18-5-2020 at 18:29


It seems that the addition of NaOH is not needed, when the concentrations are not too high and when Na2SO3 is used as a reducing agent. The original source is a patent. Attachment: Patent DE000000055152A.pdf (194kB)
This file has been downloaded 414 times

It says "In order to avoid further exposure of the copper cyanide to the 6 molecules of sulphuric acid formed, either work in a highly diluted solution or neutralize most of the free sulphuric acid formed by adding alkali, unless you prefer to use a sulphite from the outset."

I used about a 10 % solution of copper sulphate, heated it nearly to the boiling point and added a solution of about 10 % sodium sulfite/ferrocyanide very slowly with stirring. According to the patent a slight excess of copper sulfate is required to avoid the formation of a iron-rich precipitate. Maybe that's the brown stuff? So I used a 10 % excess of copper and about 10-15 minutes after the whole mixture was added, the precipitate has turned almost pure white. (I made a few q&d tests before including NaOH, Cu(OH)2 and so on and the products turned brown very fast and contained noticable amouns of iron.)

I washed the precipitate with pure water and pressed it between filter paper. My sample is drying now and looks similar to your last picture, but rather with a gray tint than pink. Some small pieces are already dry and look off-white. I'm still afraid it could be contaminated with iron. I will check that later.

1.jpg - 449kB 2.jpg - 258kB 3.jpg - 338kB
View user's profile View All Posts By User
Boffis
International Hazard
*****




Posts: 1886
Registered: 1-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 19-5-2020 at 05:29


There you go, your question answered!

Is the presence of iron a big issue? I suspect that it is present either as a ferric oxide hydrate or as a copper cyanoferrate complex, niether of which should be a problem in organic chemistry.
View user's profile View All Posts By User
Bedlasky
International Hazard
*****




Posts: 1245
Registered: 15-4-2019
Location: Period 5, group 6
Member Is Offline

Mood: Volatile

[*] posted on 19-5-2020 at 13:30


Nice preparation!

May I asked what did you do with filtrate? I know that it probably containted only very small amount of free cyanide ions but still there were present in it. Did you add bleach in it to oxidised cyanide in to cyanate?

Btw CuCN can be also used for hydrocyanation of alkynes to make unsaturated nitriles. See: http://organicreactions.org/index.php?title=Hydrocyanation_o...




View user's profile View All Posts By User
Pok
potassium Prometheus
***




Posts: 176
Registered: 5-12-2010
Member Is Offline


[*] posted on 19-5-2020 at 13:35


I prefer pure compounds. ;) My goal is to make KCN from it and iron impurities could be a problem.

Unfortunately, my dry product is not as white as shown in the second picture. Better washing could have helped. Or maybe the colour only comes from tiny Fe impurities. I will test for iron soon. My yield is only about 90 %. Maybe it still was too acidic and some HCN escaped. But a single addition of some NaOH just after adding all the K4Fe(CN)6 should be enough I think. I will make further tests. :)

I didn't throw away the solution yet. It still contains some copper. I will probably add bleach and a precipitation agent for the copper.

[Edited on 19-5-2020 by Pok]
View user's profile View All Posts By User
Bedlasky
International Hazard
*****




Posts: 1245
Registered: 15-4-2019
Location: Period 5, group 6
Member Is Offline

Mood: Volatile

[*] posted on 19-5-2020 at 21:44


How did you convert CuCN in to KCN? I firstly think about double displacement between CuCN and KI because corresponding Ag salt is less soluble than AgCN. But I found solubility product of CuCN and CuI and CuCN is much less soluble than CuI.

Another way which comes to my mind is reaction between CuCN and Mg or Zn to make magnesium or zinc cyanide and copper. Than heating with potassium carbonate to form KCN and insoluble basic carbonate.

[Edited on 20-5-2020 by Bedlasky]




View user's profile View All Posts By User
Boffis
International Hazard
*****




Posts: 1886
Registered: 1-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 20-5-2020 at 06:56


Does anyone have a reference to an example of the use of cuprous cyanide to prepare a nitrile by halogen displacement either aliphatic or aromatic? I have found a few using alkali cyanides but I was wondering if Cu-1 cyanide can be used as a substitute? anomalous in his orginal post indicates that it work in the case of some aromatic cyanations of haloaromatic compounds, presumably reactive ones like nitrobromobenzenes etc.

I have a few details for Sandmeyer type diazo reactions to give aromatic nitriles but its not the same.

[Edited on 20-5-2020 by Boffis]
View user's profile View All Posts By User
DavidJR
National Hazard
****




Posts: 908
Registered: 1-1-2018
Location: Scotland
Member Is Offline

Mood: Tired

[*] posted on 20-5-2020 at 08:47


That looks great.
View user's profile View All Posts By User
Pok
potassium Prometheus
***




Posts: 176
Registered: 5-12-2010
Member Is Offline


[*] posted on 23-5-2020 at 14:30


Quote: Originally posted by Bedlasky  
How did you convert CuCN in to KCN? I firstly think about double displacement between CuCN and KI because corresponding Ag salt is less soluble than AgCN. But I found solubility product of CuCN and CuI and CuCN is much less soluble than CuI.

Another way which comes to my mind is reaction between CuCN and Mg or Zn to make magnesium or zinc cyanide and copper.

I planned to convert the CuCN (which was a bit brown after drying)
0.jpg - 181kB

to Copper(I) oxide with KOH. Unfortunately, it turned out that a complex copper potassium cyanide is formed, which doesn't get further attacked by KOH. After mixing a small amount of CuCN with a solution of KOH in excess, everything seemed to work. Yellow hydrated Cu2O formed with a colourless solution above (not visible in the following picture because the whole mixture was stirred)
1.jpg - 67kB

After heating the precipitate became brown (water-free Cu2O) and crystals appeared during cooling, which seem to be not very soluble in water.
2.2.jpg - 215kB

There are many different complexes of CuCN and KCN and this one doesn't seem to be very usefull. After letting it sit for 1-2 days under the colourless liquit it became a mixture of a black compound (probably CuO) and a green compound (some basic copper salt).
3.jpg - 269kB

The liquid above didn't decolorize a copper tetrammine solution.

The CuCN seems to be quite pure. Only very small amounts of iron seem to be present. I also tried to convert it to Mg(CN)2. 250 mg of CuCN were suspended in about 2-3 ml water and 150 mg (or so) Mg powder was added. The mixture became quite warm and some gas was produced. After a few hours a brown solid (Cu + remaining Mg) and a clear solution was visible. Again, this solution didn't decolorize a copper tetrammine solution.

I don't see an easy way to convert CuCN to KCN. Silver cyanide should offer a much better way.

[Edited on 23-5-2020 by Pok]
View user's profile View All Posts By User
S.C. Wack
bibliomaster
*****




Posts: 2419
Registered: 7-5-2004
Location: Cornworld, Central USA
Member Is Offline

Mood: Enhanced

[*] posted on 23-5-2020 at 16:04


Has anyone considered that the precipitate is cuprous ferrocyanide when white (and the basis for Williams' "bullshit" method for quantifying ferrocyanide) and cupric ferrocyanide when red-brown?



"You're going to be all right, kid...Everything's under control." Yossarian, to Snowden
View user's profile Visit user's homepage View All Posts By User
Bedlasky
International Hazard
*****




Posts: 1245
Registered: 15-4-2019
Location: Period 5, group 6
Member Is Offline

Mood: Volatile

[*] posted on 23-5-2020 at 20:49


Quote: Originally posted by Pok  

The CuCN seems to be quite pure. Only very small amounts of iron seem to be present. I also tried to convert it to Mg(CN)2. 250 mg of CuCN were suspended in about 2-3 ml water and 150 mg (or so) Mg powder was added. The mixture became quite warm and some gas was produced. After a few hours a brown solid (Cu + remaining Mg) and a clear solution was visible. Again, this solution didn't decolorize a copper tetrammine solution.


Dissolve in your cyanide solution huge excess of sodium thiosulfate. Than add some ferric salt. Upon acidification with dilute acid you should obtain red solution (with some sulfur from thiosulfate decomposition). Cyanides reacts with thiosulfate or sulfur to form thiocyanate which form with ferric ions red complex. Be sure that acid which you use doesn't contain iron (test it with thiocyanate, salicylic acid or other iron sensitive reagent). From my expirience vinegar is good choice - commercial HCl or battery acid contain lots of iron (especially battery acid).

Another good test is mixing your solution with Fe(II)+Fe(III) solution. If cyanide is present, there is a formation of prussian blue.

Quote: Originally posted by S.C. Wack  
Has anyone considered that the precipitate is cuprous ferrocyanide when white (and the basis for Williams' "bullshit" method for quantifying ferrocyanide) and cupric ferrocyanide when red-brown?


I didn't find any mention about Cu(I) ferrocyanide. But I was thinking about this few days ago. I made few calculations for silver cyanide formation and in theory it shouldn't work, because silver ferrocyanide is more insoluble than silver cyanide. But reaction takes place in hot acidic solution. At these conditions HCN should form which can react with Cu(I) or Ag(I) to form CuCN or AgCN.

[Edited on 24-5-2020 by Bedlasky]

1.png - 16kB




View user's profile View All Posts By User
Pok
potassium Prometheus
***




Posts: 176
Registered: 5-12-2010
Member Is Offline


[*] posted on 24-5-2020 at 11:13


Regarding the solubility: AgCN is less soluble than AgCl. But you can make HCN from AgCN by letting it react with HCl!

Probably some complexes are formed which make this reaction possible.

@S.C. Wack: it's not cuprous ferrocyanide. The compound doesn't contain considerable amounts of iron!

I also tried to make HCN from CuCN by letting it react with HCl (formation of sparingly soluble CuCl). But this didn't work. The CuCN dissolved in the concentrated HCl. This is typical for CuCN.

[Edited on 24-5-2020 by Pok]
View user's profile View All Posts By User
S.C. Wack
bibliomaster
*****




Posts: 2419
Registered: 7-5-2004
Location: Cornworld, Central USA
Member Is Offline

Mood: Enhanced

[*] posted on 24-5-2020 at 12:15


Was there any distillation of that?

Has anyone compared their cyanide from ferrocyanide to cyanide from cyanide?

[Edited on 24-5-2020 by S.C. Wack]




"You're going to be all right, kid...Everything's under control." Yossarian, to Snowden
View user's profile Visit user's homepage View All Posts By User
kmno4
International Hazard
*****




Posts: 1504
Registered: 1-6-2005
Location: Silly, stupid country
Member Is Offline

Mood: No Mood

[*] posted on 30-5-2020 at 13:34


Quote:

Has anyone compared their cyanide from ferrocyanide to cyanide from cyanide?

I did. CuCN from ferrocyanide is slightly darker than CuCN from KCN, but all tests I made gave the same results (but Fe contamination).
Besides, white Cu4Fe[(CN)6] is described in legendary "Chemistry of cyanogen compounds" by Williams.
I still dare to claim, that the simplest and cheapest method utilizes CuCl solution prepared in situ from CuSO4, NaCl and Cu.
Anyway, obtained CuCN is pretty useless, however its preparation from FeCy6 is interesting and surprising.
At least one question is explained: influence of Cu(I) on acidolysis of K4Fe[(CN)6].




Слава Україні !
Героям слава !
View user's profile View All Posts By User
Fery
International Hazard
*****




Posts: 1029
Registered: 27-8-2019
Location: Czechoslovakia
Member Is Offline


[*] posted on 17-11-2024 at 09:17


Quote: Originally posted by Boffis  
Does anyone have a reference to an example of the use of cuprous cyanide to prepare a nitrile by halogen displacement either aliphatic or aromatic? I have found a few using alkali cyanides but I was wondering if Cu-1 cyanide can be used as a substitute? anomalous in his orginal post indicates that it work in the case of some aromatic cyanations of haloaromatic compounds, presumably reactive ones like nitrobromobenzenes etc.

1-bromonaphthalene + CuCN + pyridine -> 1-naphthonitrile = 1-cyanonaphthalene
you can also use 1-chloronaphthalene just the reaction time is slightly longer and temperature higher (15 hours 220 C for bromo, 24 hours 245-250 for chloro)
https://pubs.acs.org/doi/pdf/10.1021/ja01290a507
https://sci-hub.se/https://pubs.acs.org/doi/pdf/10.1021/ja01...
Attachment: newman1937.pdf (124kB)
This file has been downloaded 37 times

I rather posted something more "exothic" to synthesize as you can obtain benzonitrile from cheap benzoic acid + sulfamic acid
https://www.sciencemadness.org/whisper/viewthread.php?tid=16...
View user's profile Visit user's homepage View All Posts By User
clearly_not_atara
International Hazard
*****




Posts: 2801
Registered: 3-11-2013
Member Is Offline

Mood: Big

[*] posted on 17-11-2024 at 10:30


For the reaction of aliphatic halides with transition metal cyanides:
Quote:
The ratio of isocyanide to nitrile depends largely on the nature of the metal cyanide employed. Guillemard
(231), in an extensive study of different metal cyanides, showed that the heavier metal cyanides such as those of
silver gave isocyanides exclusively, while with other metals the following percentages of isocyanide were in the
mixture resulting from the reaction with ethyl iodide: cuprous copper, 56 per cent; cadmium, 11 per cent;
nickel, 8 per cent; zinc, 2.6 per cent. Sodium and potassium cyanides gave only minor amounts of isocyanides. The
temperature of reaction was also found to play an important role in the amount of isocyanide produced. All of the
metallic cyanides gave normal nitriles if the reaction were conducted above 150°C. Lower temperatures favored
isocyanide formation.

So for the rxn of CuCN with aliphatic halides, temperatures above 150 C are advisable, since the isocyanide is famously noxious. DMF refluxes at 153 C and seems like it could be an ideal medium for the preparation of heavy aliphatic nitriles. For lighter nitriles, the dehydration of amides over alumina or vanadium-hydrotalcite seems preferable. But benzyl bromide (bp 198 C) is already a reasonable candidate for this method.

Mowry, D.T. The Preparation of Nitriles, 1948, attached.

Attachment: mowry1948.pdf (5.2MB)
This file has been downloaded 36 times





Quote: Originally posted by bnull  
you can always buy new equipment but can't buy new fingers.
View user's profile View All Posts By User
Fery
International Hazard
*****




Posts: 1029
Registered: 27-8-2019
Location: Czechoslovakia
Member Is Offline


[*] posted on 17-11-2024 at 10:58


Nitrobenzene, DMF, pyridine are suitable solvents.
https://sci-hub.se/https://doi.org/10.1016/S0040-4039(01)02168-2
Quote:
The Rosenmund-von Braun reaction has been known for almost the same length of time, which gives rise to aryl nitriles from the coupling of copper cyanide (CuCN) with aryl halides. This reaction is usually carried out in polar solvents such as nitrobenzene, DMF and pyridine using excess of CuCN at 150-250°C. The product isolation is a tedious process, involving washings with water followed by extensive silica gel column chromatography.
...
We initially set out to investigate the feasibility of using ionic liquids, especially 1-n-butyl-3-methylimidazolium halides (bmiX, X=I, Br, Cl) as reaction media to replace DMF and pyridine in the Rosenmund-von Braun reaction. We reasoned that because of the nonvolatility of ionic liquids, the products could be distilled directly from the reaction mixture. On the other hand, owing to the limited solubility of these ionic liquids in certain organic solvents such as hexanes, ethyl acetate and toluene, isolation of products could be achieved directly via simple extraction using common organic solvents.


DMF (cca 10 EUR per 1 liter) is cheapest from all the 3 above solvents, but it is hard to dry, best method is sequential drying with 3A molecular sieves
https://www.tesble.com/10.1021/jo00414a038
View user's profile Visit user's homepage View All Posts By User
 Pages:  1  2

  Go To Top