maqce
Harmless
Posts: 11
Registered: 12-11-2019
Location: Bordeaux, France
Member Is Offline
|
|
Chemical attack inside the flask
Hello,
I recieved new flasks and I had a problem : I can't boil liquids in it because the surface inside the flask is too smooth. I haven't any magnetic
stir, and even with boiling chips (broken glass) it still bumps violently. I scratched the botton of the flask but it's not efficient.
So I thought I could chemicaly attack the glass to create porosity. I have NaOH, I can reflux concentrated NaOH solution in the bottom of the flask.
Do you think it could work ?
|
|
BromicAcid
International Hazard
   
Posts: 3266
Registered: 13-7-2003
Location: Wisconsin
Member Is Offline
Mood: Rock n' Roll
|
|
In my experience accidentally injuring a flask with NaOH I did not end up with a frosted inside but instead a very smooth bumpy inside. Are all your
issues bumping related to the same liquid/solution? Are you heating it too fast, applying vacuum too fast, or maybe not examining all the variables?
|
|
maqce
Harmless
Posts: 11
Registered: 12-11-2019
Location: Bordeaux, France
Member Is Offline
|
|
Quote: Originally posted by BromicAcid  | Are all your issues bumping related to the same liquid/solution? Are you heating it too fast, applying vacuum too fast, or maybe not examining all
the variables? |
I already had this problem before, but today it happened when I was distilling ethanol, heating it very gently with boiling chips and scratched
bottom, and no vacuum. I don't know what it could be..
[Edited on 18-4-2020 by maqce]
|
|
maqce
Harmless
Posts: 11
Registered: 12-11-2019
Location: Bordeaux, France
Member Is Offline
|
|
The scratches helped a bit, but it still bumps
|
|
DraconicAcid
International Hazard
   
Posts: 4412
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline
Mood: Semi-victorious.
|
|
Broken glass for boiling chips? You want broken ceramic.
Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
|
|
unionised
International Hazard
   
Posts: 5135
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
The silica gell beads you get in little bags that say "do not eat" do a much better job as boiling chips than broken glass does.
|
|
maqce
Harmless
Posts: 11
Registered: 12-11-2019
Location: Bordeaux, France
Member Is Offline
|
|
Quote: Originally posted by unionised  | The silica gell beads you get in little bags that say "do not eat" do a much better job as boiling chips than broken glass does.
|
Oh that's smart ! Thx I'll try it
|
|
mackolol
Hazard to Others
 
Posts: 459
Registered: 26-10-2017
Member Is Offline
Mood: Funky
|
|
And is it round bottom flask or the Erlenmeyer?, because Erlenmeyers always bump without vigorous stirring during distillation.
If it's Round bottom, you can add some acid washed sand, I used it in ether synthesis and worked just fine.
[Edited on 19-4-2020 by mackolol]
|
|