[*] posted on 8-4-2020 at 18:43
The mingling of Palladium and Arsenic


Dichlorobis(triphenylphosphine)palladium is a very common precatalyst in cross coupling reactions. Being a Pd(II) species, it's a relatively air stable and inexpensive form of Palladium. I recently set out to make the triphenylarsine version. While the Pd-As bond is not nearly as strong, causing faster catalyst initiation, it also means that the AsPh3 cannot stabilize Pd0 intermediates as well, ultimately causing faster decomposition. That coupled with Arsenic's toxicity means this complex is really just a nice collector's item.

I made triphenylarsine from arsenic trichloride, which I've made recently here. Some people expressed concern about AsCl3 not being easy to access at home. There is limited literature precedent that AsI3 can be used as a substitute for AsCl3 in this reaction, although the exact reaction is not reported. I've also included a quick prep for AsI3 in case someone wants to attempt this route.

Triphenylarsine
To a 100 mL schlenk flask under Ar was added arsenic trichloride (2.5 g, 1 equiv) and a stir bar. Dry THF (20 mL) was added via syringe. The chloride quickly dissolved giving a homogenous solution. Phenylmagnesium chloride (3.3 equiv, 2M in THF) was added dropwise over 20 minutes. There is a notable exotherm in this reaction which I saw as a good sign. After the addition was complete, I was left with a clear brown solution. I heated this to 50 oC overnight resulting in a thick precipitate (likely MgCl2).

20200405_155755-min.jpg - 975kB

This was left to cool to RT and water (30 mL) was added. This was extracted twice with ether (15 mL) and the combined organics dried over MgSO4. The solution was concentrated under reduced pressure to yield an off white oil. A small amount of ether (1-2 mL) was added and the solution left overnight. I was kind of disappointed not to see any crystals. Luckily, the oldest trick in the book, scratching with a glass stir rod and waiting a few hours afforded these beautiful clear crystals. These were rinsed with a few mL of hexanes several times, and left to dry on a piece of filter paper yielding 2.2 g of crystals (52%).

20200408_141454-min.jpg - 969kB 20200408_142241-min.jpg - 1MB

Arsenic triiodide
In a test tube was placed 1 g KI (6 equiv) which was dissolved in 1 mL water. In another test tube with stir bar was added arsenic trioxide (0.2g, 1 equiv). Concentrated aq HCl (2.9 mL) was added and the tube was gently heated with stirring to dissolve everything resulting in a yellowish solution. This took about 5 minutes at 40 oC. The KI solution was quickly poured into the arsenic solution with stirring resulting in a thick orange precipitate. The precipitate was left for 5 minutes and filtered. Rising with water causes immediate hydrolysis. So the solid was left on the frit for a few minutes and then dried under vacuum.

20200408_173104-min.jpg - 457kB20200408_191445.jpg - 177kB

Potassium tetrachloropalladate
Palladium (II) chloride (1 equiv) and potassium chloride (4 equiv) are dissolved in the minimum amount of boiling water resulting in a homogenous brown solution. Upon cooling the title compound crystallized out as beautiful green-red crystals which are filtered and dried under vacuum. Yields are almost quantitative.

20200408_160549-min.jpg - 128kB

Dichlorobis(triphenylarsine) palladium (II)
Potassium tetrachloropalladate (100 mg, 1 equiv) was placed in a test tube and dissolved in 1.5 mL water. In another test tube, triphenylarsine (187 mg, 2 equiv) was dissolved in 1.5 mL EtOH. Gentle heating was necessary to dissolve both compounds. The solutions are mixed and stirred for 5 minutes resulting in a dense yellow precipitate. The color is identical to what you would expect for the analogous triphenylphosphine complex. The compound is filtered, rinsed with water, EtOH, ether, and dried under reduced pressure. The yield is 220 mg (90%)

20200408_162458-min.jpg - 566kB20200408_1914451.jpg - 207kB

I think this concludes my adventures with Arsenic. Some really pretty chemistry but that's about the extent I'm willing to go. Keep in mind that toxic arsine gas could be produced at any of these steps and many arsenic compounds are absorbed through skin. Gloves and good ventilation are key to these reactions. In any case, I hope the pictures are at least nice to look at!

References:
AsPh3: adapted from Org. Synth. 1950, 30, 95
AsI3: Reproduced from Inorg. Synth. V1, 103
K2PdCl4: adapted from Inorg. Chem. 1985, 24, 1503
Pd(AsPh3)2Cl2: Reproduced from Inorg. Chem. 1965, 3, 1587 (Also a very important paper)
View user's profile View All Posts By User
numos
Hazard to Others
***




Posts: 269
Registered: 22-2-2014
Location: Pasadena
Member Is Offline

Mood: No Mood

[*] posted on 8-4-2020 at 18:47


Also, I know a few of you have asked to see my schlenk setup. I'm working on putting that together in the near future :)
View user's profile View All Posts By User
reactofurnace
Hazard to Self
**




Posts: 76
Registered: 17-7-2015
Member Is Offline

Mood: Volatile

shocked.gif posted on 8-4-2020 at 19:17


Nice! Beautiful colored compounds and large crystals are the best
View user's profile Visit user's homepage View All Posts By User
woelen
Super Administrator
*********




Posts: 7987
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 8-4-2020 at 23:15


Very interesting stuff. The preparation and use of AsCl3 is well beyond my confidence level, but the use of As2O3 to make some AsI3 is something, which I could try.



The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
Tsjerk
International Hazard
*****




Posts: 3026
Registered: 20-4-2005
Location: Netherlands
Member Is Offline

Mood: Mood

[*] posted on 8-4-2020 at 23:30


Nice write up! I'm not going to try any of this but it is always nice to see posts like this.
View user's profile View All Posts By User
Metacelsus
International Hazard
*****




Posts: 2537
Registered: 26-12-2012
Location: Boston, MA
Member Is Offline

Mood: Double, double, toil and trouble

[*] posted on 9-4-2020 at 09:45


Another excellent experiment and writeup!

Quote: Originally posted by numos  
Also, I know a few of you have asked to see my schlenk setup. I'm working on putting that together in the near future :)


Yay! I'm excited to see it




As below, so above.

My blog: https://denovo.substack.com
View user's profile View All Posts By User
DraconicAcid
International Hazard
*****




Posts: 4298
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline

Mood: Semi-victorious.

[*] posted on 9-4-2020 at 09:52


Very nice!

Some days I miss working with such metal complexes (I worked with phosphine complexes of rhodium and iridium). Then I remember what grad studies was like and I go back to puttering with simple coordination complexes.




Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
View user's profile View All Posts By User
Heptylene
Hazard to Others
***




Posts: 319
Registered: 22-10-2016
Member Is Offline

Mood: No Mood

[*] posted on 10-4-2020 at 00:33


Nice chemistry! And very pretty colors, especially that arsenic triiodide! I'll have to try to make some one day.

Btw is that tin shot in your heating bath? Does it work well to heat flasks?
View user's profile View All Posts By User
numos
Hazard to Others
***




Posts: 269
Registered: 22-2-2014
Location: Pasadena
Member Is Offline

Mood: No Mood

[*] posted on 10-4-2020 at 11:41


Quote: Originally posted by woelen  
AsI3 is something, which I could try.


Glad to hear it, I had you in mind when I was making this one ;)

Quote: Originally posted by Heptylene  

Btw is that tin shot in your heating bath? Does it work well to heat flasks?


I believe it's aluminum shot. It functions kind of like a sand bath but has pros and cons. The biggest pro is it's very clean and doesn't foul over time. Unlike sand it doesn't cover everything with sand and pose risk to scratching ground glass joints. It also heats up much faster, I would say even faster than an oil bath which is nice.

Downside is that you can't push a flask into it and expect it to move out of the way. You always have to put your flask in first and then pour this over it - which is hard to do when it's hot. Frankly not a huge deal but sometime I want to take my flask out to check and then stare dishearteningly as my little flask tunnel collapses.
View user's profile View All Posts By User
Justin Blaise
Hazard to Self
**




Posts: 82
Registered: 5-10-2011
Location: Parts Unknown
Member Is Offline

Mood: No Mood

[*] posted on 17-4-2020 at 14:43


Really nice work! Do you plan on making other transition metal complexes with your AsPh3? Maybe some Co or Ni complexes?
View user's profile View All Posts By User
numos
Hazard to Others
***




Posts: 269
Registered: 22-2-2014
Location: Pasadena
Member Is Offline

Mood: No Mood

[*] posted on 17-4-2020 at 18:49


Probably not anytime soon. I wanted to make the Pd complex because I've used the PPh3 analog for coupling reactions, so it has nostalgic value. Lots of other things planned though, don't worry!