[*] posted on 14-3-2020 at 06:19
What to do with unknown copper waste?


So, from the experiment I did a while ago, I still have some copper waste left. I had thought that it was all copper hydroxide and basic copper carbonate. So, I added acetic acid to covert it all to copper acetate so that I finally had generally the same product.

Well, that didn't end up working. A lot of it converted to copper acetate, but a lot of it stayed as an insoluble solid, even after adding distilled water. Thus, I am now stuck with some copper acetate and unknown blue waste.

What do I do with this?

And, for the future, what do I do with unknown waste in general?




Collected elements:
Al, Cu, Ga, C (coal), S, Zn, Na

Collected compounds:

Inorganic:
NaOH; NaHCO3; MnCl2; MnCO3; CuSO4; FeSO4; aq. 30-33% HCl; aq. NaClO; aq. 9,5% ammonia; aq. 94-96% H2SO4; aq. 3% H2O2

Organic:
citric acid, sodium acetate, sodium citrate, petroleum, mineral oil
View user's profile View All Posts By User
stephill92
Harmless
*




Posts: 24
Registered: 19-3-2019
Member Is Offline


[*] posted on 14-3-2020 at 07:20


You could probably just put it in a container and save it or just take it to a chemical waste disposal since you know that it contains copper. As for other waste, I just try to save all the stuff I can't pour down the drain if it's inorganic, and for organics I just try to evaporate or burn them off.
View user's profile View All Posts By User
Draeger
Hazard to Others
***




Posts: 185
Registered: 31-1-2020
Location: North-Rhine Westfalia, Germany
Member Is Offline

Mood: Slowly getting ready for new projects

[*] posted on 14-3-2020 at 09:17


Quote: Originally posted by stephill92  
You could probably just put it in a container and save it or just take it to a chemical waste disposal since you know that it contains copper. As for other waste, I just try to save all the stuff I can't pour down the drain if it's inorganic, and for organics I just try to evaporate or burn them off.

Okay. Thanks.




Collected elements:
Al, Cu, Ga, C (coal), S, Zn, Na

Collected compounds:

Inorganic:
NaOH; NaHCO3; MnCl2; MnCO3; CuSO4; FeSO4; aq. 30-33% HCl; aq. NaClO; aq. 9,5% ammonia; aq. 94-96% H2SO4; aq. 3% H2O2

Organic:
citric acid, sodium acetate, sodium citrate, petroleum, mineral oil
View user's profile View All Posts By User
anti
Harmless
*




Posts: 32
Registered: 17-2-2020
Member Is Offline

Mood: Mood: Mood:

[*] posted on 14-3-2020 at 10:39


Do electrolysis with lead dioxide anode to plate out the copper out of your acetate.
The blue stuff could be any of the following :
Copper Oxychloride
Copper Carbonate
Copper(I) Chloride
ALL ARE INSOLUBLE
Tho the carbonate should have reacted with the acetic acid. Try adding more.


View user's profile View All Posts By User
garphield
Hazard to Self
**




Posts: 58
Registered: 9-12-2019
Member Is Offline


[*] posted on 14-3-2020 at 11:18


Couldn't you just add sodium hydroxide or carbonate to precipitate out the copper as the hydroxide/oxide/carbonate?

[Edited on 14-3-2020 by garphield]