nikotyna1919
Harmless
*




Posts: 10
Registered: 10-9-2019
Location: reverse poland flag or nusantara
Member Is Offline


[*] posted on 9-3-2020 at 22:01
corrosion resistant stainless steel grades for distillation


I want to know which kind of austenitic stainless steel grade is the best for distilling and refluxing corrosive chemical such as sulfuric acid ,phosphoric acid, calcium hypochlorite
I need distilling sulfuric acid for making diethyl ether
phosphoric for elemental phosphorous
calcium hypochlorite for chloroform
(also please i don't want to use glass or ceramics because is fragile
i only want to use metals)

[Edited on 10-3-2020 by nikotyna1919]
View user's profile View All Posts By User
draculic acid69
International Hazard
*****




Posts: 1371
Registered: 2-8-2018
Member Is Offline


[*] posted on 10-3-2020 at 04:00


No chance of using SS for distilling sulfuric acid or refluxing hypochlorites.
Glass is your only option for this stuff.but if u want to make either u could use teflon coated steel bcoz it's less than 250'c at which point teflon softens but distilling sulfuric acid requires 300'c+ so teflon coated steel is out.im guessing phosphoric acid is no good for steels but I'm not sure.naocl and caocl will probably fuck steel too.
Glass is what u need.its that simple unless you have the money to get platinum metal
flasks made or glass coated steel like industry uses but this cost will be astronomical
compared to glass.just buy the glass.

[Edited on 10-3-2020 by draculic acid69]

[Edited on 10-3-2020 by draculic acid69]
View user's profile View All Posts By User
Fulmen
International Hazard
*****




Posts: 1702
Registered: 24-9-2005
Member Is Offline

Mood: Bored

[*] posted on 10-3-2020 at 04:09


You can start with this:
https://www.rolledalloys.com/shared/library/technical-papers...




We're not banging rocks together here. We know how to put a man back together.
View user's profile View All Posts By User
Herr Haber
International Hazard
*****




Posts: 1236
Registered: 29-1-2016
Member Is Offline

Mood: No Mood

[*] posted on 10-3-2020 at 04:28


Have any of the questions you keep asking actually gotten you to do any actual experimentation ?
Are your questions an elaborate way of trolling ?
If so, could you elaborate on how it gets you off to start empty debates among users ?

As for your questions, one of my suppliers carries Platinum labware. They also have steel alloyed with Palladium or Rhodium or both.
Nothing fancy, usually around 15% PGM. Not expensive at all !

That's the way to go if you want only ONE set of equipment.




The spirit of adventure was upon me. Having nitric acid and copper, I had only to learn what the words 'act upon' meant. - Ira Remsen
View user's profile View All Posts By User
clearly_not_atara
International Hazard
*****




Posts: 2725
Registered: 3-11-2013
Member Is Offline

Mood: Big

[*] posted on 10-3-2020 at 06:19


You don't reflux hypochlorites for chloroform!



Quote: Originally posted by bnull  
you can always buy new equipment but can't buy new fingers.
View user's profile View All Posts By User
nikotyna1919
Harmless
*




Posts: 10
Registered: 10-9-2019
Location: reverse poland flag or nusantara
Member Is Offline


[*] posted on 11-3-2020 at 03:15
not trolling


I'm not trolling I'm just planning to experimenting

also i wanted to save money by using less equipment
and metal container is leak proof

[Edited on 11-3-2020 by nikotyna1919]
View user's profile View All Posts By User
Herr Haber
International Hazard
*****




Posts: 1236
Registered: 29-1-2016
Member Is Offline

Mood: No Mood

[*] posted on 11-3-2020 at 04:29


If you want to save money then go to eBay and get cheap labware from Deschem.

Even if you break it 20 times it wont cost you as much as a custom piece of equipment made from special steel.




The spirit of adventure was upon me. Having nitric acid and copper, I had only to learn what the words 'act upon' meant. - Ira Remsen
View user's profile View All Posts By User
draculic acid69
International Hazard
*****




Posts: 1371
Registered: 2-8-2018
Member Is Offline


[*] posted on 11-3-2020 at 06:02


I imagine that this advice will fall on deaf ears until the next silly question
View user's profile View All Posts By User

  Go To Top