Merryp
Harmless
Posts: 29
Registered: 27-4-2019
Member Is Offline
|
|
Making iron phosphide without elemental phosphorus?
I was wondering whether there's a convenient method.
Carbothermal reduction of iron phosphate? (what temperatures would that require?)
Maybe heating P2O5 with iron powder?
|
|
Tellurium
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 84
Registered: 12-7-2017
Location: Group 16, Chalcogen City
Member Is Offline
Mood: smelly
|
|
Well it is possibe to reduce Calcium phosphate(other phosphates should be usable too) with elemental carbon at high temperatures to elemental P. I
thing somewhere on youtube I also saw a video using Al as reducing agent. I think using a mixture of phosphate, C and Fe with the absence of oxygen
might work. But note that very high temperatures are needed(e.g. a muffle furnance or something similar).
|
|
Merryp
Harmless
Posts: 29
Registered: 27-4-2019
Member Is Offline
|
|
Quote: Originally posted by Tellurium ![](images/xpblue/lastpost.gif) | Well it is possibe to reduce Calcium phosphate(other phosphates should be usable too) with elemental carbon at high temperatures to elemental P. I
thing somewhere on youtube I also saw a video using Al as reducing agent. I think using a mixture of phosphate, C and Fe with the absence of oxygen
might work. But note that very high temperatures are needed(e.g. a muffle furnance or something similar). |
That's why I was wondering whether P2O5 would be a more convenient source, given the enthalpy of formation.
|
|
Fery
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1003
Registered: 27-8-2019
Location: Czechoslovakia
Member Is Offline
|
|
Quote: Originally posted by Merryp ![](images/xpblue/lastpost.gif) | That's why I was wondering whether P2O5 would be a more convenient source, given the enthalpy of formation. |
check P2O5 b.p.
|
|
Boffis
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1850
Registered: 1-5-2011
Member Is Offline
Mood: No Mood
|
|
Could you use an alumothermic thermite type reaction with anhydrous FePO4? The latter is easily prepared if you have a ferric salt and a phosphate
salt. Iron phosphide is given as Fe3P so you would need to add some iron filling to the mixture which might chill the reaction too much and prevent
the reaction being self sustaining. You could use a mixture of iron phosphate and say magnetite;
3FePO4 + 6Fe + 8Al = 3Fe3P + 4Al2O3
The aluminium oxide would be inert to most reaction and the melting point of the phosphide c 1100 C is possibly low enough to get away with it. With
magnetite it would be:
9FePO4 + 6Fe3O4 + 40Al = 9Fe3P + 20Al2O3
You could also use red iron oxide. I can see a few experiments might be required but hey, isn't that what we are here for? ![:)](./images/smilies/smile.gif)
|
|
BromicAcid
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3237
Registered: 13-7-2003
Location: Wisconsin
Member Is Offline
Mood: Rock n' Roll
|
|
Quote: | ...and R.A. Brooman heated a mixture of silica, iron, coal, and calcium phosphate so as to form a fusible slag and iron phosphide. The latter when
heated with sulphur, hydrogen sulphide, carbon disulphide, etc., furnished phosphorus.
Inorganic and Theoretical Chemistry: pg 740 |
|
|
bluamine
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 196
Registered: 17-8-2015
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Boffis ![](images/xpblue/lastpost.gif) |
9FePO4 + 6Fe3O4 + 40Al = 9Fe3P + 20Al2O3
You could also use red iron oxide. I can see a few experiments might be required but hey, isn't that what we are here for? ![:)](./images/smilies/smile.gif)
|
Wow that's superinteresting!
Did anyone try it yet?
|
|