Author: Subject: Calcium electrolysis with alternative salts
John paul III
Hazard to Others
***




Posts: 110
Registered: 28-4-2018
Member Is Offline

Mood: No Mood

[*] posted on 2-11-2019 at 03:42
Calcium electrolysis with alternative salts


Shouldn't it be easy (in theory) to find a Calcium salt with a low melting point (CaH2PO4 melts at 109°C) and perform an ordinary electrolysis to obtain Calcium? Calcium is said to be hard to make by an amateur
View user's profile View All Posts By User
wg48temp9
National Hazard
****




Posts: 787
Registered: 30-12-2018
Location: not so United Kingdom
Member Is Offline


[*] posted on 2-11-2019 at 04:23


Quote: Originally posted by John paul III  
Shouldn't it be easy (in theory) to find a Calcium salt with a low melting point (CaH2PO4 melts at 109°C) and perform an ordinary electrolysis to obtain Calcium? Calcium is said to be hard to make by an amateur


I would think using an acid phosphate the hydrogen would be released first.

Using a eutectic with salts that can not be reduced easily, from memory the eutectic can contain sodium or potassium. I think there is a thread about it.

Sorry I could not find the thread.

[Edited on 11/2/2019 by wg48temp9]




I am wg48 but not on my usual pc hence the temp handle.
Thank goodness for Fleming and the fungi.
Old codger' lives matters, wear a mask and help save them.
Be aware of demagoguery, keep your frontal lobes fully engaged.
I don't know who invented mRNA vaccines but they should get a fancy medal and I hope they made a shed load of money from it.
View user's profile View All Posts By User
John paul III
Hazard to Others
***




Posts: 110
Registered: 28-4-2018
Member Is Offline

Mood: No Mood

[*] posted on 2-11-2019 at 04:46


Damn I wish I could find this thread. Do you remember any details, like what the anions could have been?
View user's profile View All Posts By User
WGTR
National Hazard
****




Posts: 972
Registered: 29-9-2013
Location: Online
Member Is Offline

Mood: Outline

[*] posted on 2-11-2019 at 04:51


Have fun:

http://www.crct.polymtl.ca/fact/documentation/FTsalt/FTsalt_...




View user's profile View All Posts By User
John paul III
Hazard to Others
***




Posts: 110
Registered: 28-4-2018
Member Is Offline

Mood: No Mood

[*] posted on 2-11-2019 at 06:19


Thank you!
View user's profile View All Posts By User
wg48temp9
National Hazard
****




Posts: 787
Registered: 30-12-2018
Location: not so United Kingdom
Member Is Offline


[*] posted on 2-11-2019 at 07:19


Quote: Originally posted by John paul III  
Damn I wish I could find this thread. Do you remember any details, like what the anions could have been?


I had an other search and found the following but I don't think its the one I was thinking about.

We successfully made a small amount of calcium metal by electrolysis of a barium chloride, calcium chloride, strontium chloride and potassium chloride (http://www.google.com/patents/US3226311). Addition of the other chlorides lowers the melting point of the mixture to around 600 C (and calcium is pretty much the product). We were wondering if barium could be made in a similar way.

Does anyone know anything about this?

[Edited on 11/2/2019 by wg48temp9]




I am wg48 but not on my usual pc hence the temp handle.
Thank goodness for Fleming and the fungi.
Old codger' lives matters, wear a mask and help save them.
Be aware of demagoguery, keep your frontal lobes fully engaged.
I don't know who invented mRNA vaccines but they should get a fancy medal and I hope they made a shed load of money from it.
View user's profile View All Posts By User
wg48temp9
National Hazard
****




Posts: 787
Registered: 30-12-2018
Location: not so United Kingdom
Member Is Offline


[*] posted on 2-11-2019 at 07:34


Quote: Originally posted by John paul III  
Thank you!


Search for "Calcium electrolysis" there are a few more




I am wg48 but not on my usual pc hence the temp handle.
Thank goodness for Fleming and the fungi.
Old codger' lives matters, wear a mask and help save them.
Be aware of demagoguery, keep your frontal lobes fully engaged.
I don't know who invented mRNA vaccines but they should get a fancy medal and I hope they made a shed load of money from it.
View user's profile View All Posts By User

  Go To Top