Silica gel for food packaging->silica gel for chromatography?
Can I process silica gel for food packaging to a form that can be used for chromatography? (Column chromatography or making my own TLC plates)
I was thinking about dissolving SG in NaOH then reprecipitate as SG using acid. Can this form be used for chromatography?
|
|
Dr.Bob
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2692
Registered: 26-1-2011
Location: USA - NC
Member Is Offline
Mood: No Mood
|
|
Not readily. The stuff in food packets is not even close to what you need for chromatography. The particle and pore sizes are all different. You
could try to ppt it from sodium silicate, but the washing and drying process is tough, and you need to be able to at least crudely separate the
particle sizes. There are some chemicals you can make at home just fine, but that is a tough one, as if it is not consisent, you will not be able
to reproduce anything well.
If you need small amounts, and you are in the US I can help you. I have lots of various glass columns, and a few plastic prepacked ones. And I
have some old bits of silia gel that are still fine for most work. I also have some large 200 x200 mm TLC plates that can be cut into smaller ones
for use. All are pretty cheap, at least compared to buying them from Fisher/
|
|
S.C. Wack
bibliomaster
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2419
Registered: 7-5-2004
Location: Cornworld, Central USA
Member Is Offline
Mood: Enhanced
|
|
IDK, can you? Chemist, chem thyself...then start a thread IMHO. Ground prill could be closer to the real thing than something that the aspiring
chromatographer/supplier precipitated theirself. I suspect that the cheap silica gel sold on ebay (coming from the UK) is made that way. (at the very
least it must be technical grade) The experimenter may find that there is an unexpected learning curve in making good silica, alumina, and
florisil.
PS TLC silica is like 600-1200 mesh. 400-600 is already a chore with mortar and pestle.
[Edited on 1-11-2019 by S.C. Wack]
|
|
Ubya
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1247
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline
Mood: I'm a maddo scientisto!!!
|
|
and i have been fantasizing of using kitty litter silica gel as stationary phase in column chromatography for 2 years. meh i'll still try
---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------
|
|
DavidJR
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 908
Registered: 1-1-2018
Location: Scotland
Member Is Offline
Mood: Tired
|
|
If grinding up silica gel, be sure to use appropriate respiratory protection.
|
|