Rutherford
Harmless
Posts: 8
Registered: 7-10-2019
Member Is Offline
|
|
Should 99.99% mercury contain slag? [Update from seller]
I recently purchased mercury for demonstration purposes. The mercury was purchased from Onyxmet and it states it is 99.99% pure. What would be this
slag floating around? Is this normal?
I'm just wondering if I should contact them... because it certainly isn't as clean as I thought it would be.
My first theory was that it would be iron oxide, considering the mercury probably came from an iron flask but it isn't magnetic.
![DS7_9196-2.jpg - 5.3MB](http://www.sciencemadness.org/talk/files.php?pid=624599&aid=77648)
![DS7_9194-2.jpg - 7.2MB](http://www.sciencemadness.org/talk/files.php?pid=624599&aid=77650)
[Edited on 19-10-2019 by Rutherford]
|
|
Ubya
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1247
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline
Mood: I'm a maddo scientisto!!!
|
|
If I remember correctly not all iron oxides are magnetic, so probably it is just rust
---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------
|
|
Rutherford
Harmless
Posts: 8
Registered: 7-10-2019
Member Is Offline
|
|
Do you think this would merit a chat with the vendor?
|
|
morganbw
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 561
Registered: 23-11-2014
Member Is Offline
Mood: No Mood
|
|
I think a chat would be in order.
|
|
DavidJR
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 908
Registered: 1-1-2018
Location: Scotland
Member Is Offline
Mood: Tired
|
|
If it's just that small amount of insoluble crud then that could quite easily still meet the 99.99% spec considering how dense mercury is... Of
course, there could be dissolved metals too, but i'm not sure i'd worry about that just because of some insoluble crap floating on top.
|
|
Boffis
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1850
Registered: 1-5-2011
Member Is Offline
Mood: No Mood
|
|
Even the purest mercury oxidizes slowly and more importantly absorbs sulphur from the atmosphere. Sulphur generally cretes a black scum the browner
colours are generally the oxide. Traditionally mercury has to be cleaned periodically by dripping into dilute 10% nitric acid. The aqueosu phase is
easily separated from the clean mercury which is then washed with water remove the remaining nitric acid. Don't through the washings down the drain!
Kept them for next time.
This procedure should give you nice shiny mercury.
|
|
Rutherford
Harmless
Posts: 8
Registered: 7-10-2019
Member Is Offline
|
|
Quote: Originally posted by Boffis ![](images/xpblue/lastpost.gif) | Even the purest mercury oxidizes slowly and more importantly absorbs sulphur from the atmosphere. Sulphur generally cretes a black scum the browner
colours are generally the oxide. Traditionally mercury has to be cleaned periodically by dripping into dilute 10% nitric acid. The aqueosu phase is
easily separated from the clean mercury which is then washed with water remove the remaining nitric acid. Don't through the washings down the drain!
Kept them for next time.
This procedure should give you nice shiny mercury. |
I think I will try that, would you recommend I first past it through a plunger? Or will the nitric acid take care of this brown oxide?
|
|
G-Coupled
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 287
Registered: 9-3-2017
Member Is Offline
Mood: Slightly triturated
|
|
If you feel brave, and wish to try distilling your Mercury to purify it, both NileRed and Cody's Lab have pretty good videos on YouTube on how they
did it.
NileRed
Cody's Lab
[Edited on 19-10-2019 by G-Coupled]
|
|
Rutherford
Harmless
Posts: 8
Registered: 7-10-2019
Member Is Offline
|
|
Quote: Originally posted by G-Coupled ![](images/xpblue/lastpost.gif) | If you feel brave, and wish to try distilling your Mercury to purify it, both NileRed and Cody's Lab have pretty good videos on YouTube on how they
did it.
NileRed
Cody's Lab
[Edited on 19-10-2019 by G-Coupled] |
I don't have the necessary safety equipment to perform a mercury distillation. Awesome videos though, I love both of those channels.
|
|
draculic acid69
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1371
Registered: 2-8-2018
Member Is Offline
|
|
Looks more like copper than rust.
|
|
UC235
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 565
Registered: 28-12-2014
Member Is Offline
Mood: No Mood
|
|
You can just let it drip through a pinhole in a folded filter paper. The oxides stick to the paper and the mercury comes out shiny. I have some
mercury and it has all eventually gotten cruddy looking despite good storage.
|
|
Ubya
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1247
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline
Mood: I'm a maddo scientisto!!!
|
|
copper forms an amalgam with mercury, so i doubt that it would flow on it and do nothing
---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------
|
|
fusso
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1922
Registered: 23-6-2017
Location: 4 ∥ universes ahead of you
Member Is Offline
|
|
Those red stuff looks like rust more than Cu or HgO to me.
|
|
Rutherford
Harmless
Posts: 8
Registered: 7-10-2019
Member Is Offline
|
|
He sent me this. On the one hand I feel bad for him, but then again it costed like 150€. What do you guys think would be a fair amount? Or just
clean it with a syringe and move on?
[Edited on 19-10-2019 by Rutherford]
|
|
Ubya
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1247
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline
Mood: I'm a maddo scientisto!!!
|
|
if it is just that stuff on the surface you can filter it through a syringe with a cotton plug at the bottom, you won't loose much Hg
---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------
|
|
fusso
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1922
Registered: 23-6-2017
Location: 4 ∥ universes ahead of you
Member Is Offline
|
|
HNO3 will also
dissolve Hg. Why isn't HCl better?
[Edited on 191019 by fusso]
|
|
S.C. Wack
bibliomaster
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2419
Registered: 7-5-2004
Location: Cornworld, Central USA
Member Is Offline
Mood: Enhanced
|
|
Because HCl isn't an oxidizer or a better solvent. In the sphygmomanometer thread I gave a method that works well. Shake violently for 2 min. w/ conc.
KMnO4, wash, shake again for 2 min. w/ cold dil. HNO3, wash, dry w/ something lint-free. No mercury is dissolved even though it's in a very finely
divided state.
|
|
G-Coupled
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 287
Registered: 9-3-2017
Member Is Offline
Mood: Slightly triturated
|
|
Quote: Originally posted by Rutherford ![](images/xpblue/lastpost.gif) | He sent me this. On the one hand I feel bad for him, but then again it costed like 150€. What do you guys think would be a fair amount? Or just
clean it with a syringe and move on? |
Ehh, if it's a really small percentage of the total amount you were sold, and you think you might be dealing with them in the future, it might be best
to just let him know and to eat the (hopefully small) cost. Might buy some goodwill for the future, maybe?
|
|
karlos³
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1520
Registered: 10-1-2011
Location: yes!
Member Is Offline
Mood: oxazolidinic 8)
|
|
Try to clean it up first, a small amount of course, and only then complain.
Tom is a very good guy and most helpful, he will surely replace it if your cleanup fails.
|
|
draculic acid69
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1371
Registered: 2-8-2018
Member Is Offline
|
|
Quote: Originally posted by Ubya ![](images/xpblue/lastpost.gif) | if it is just that stuff on the surface you can filter it through a syringe with a cotton plug at the bottom, you won't loose much Hg
|
Sounds like the best thing to do.then try the paper with a pinhole method.if that doesn't work I'd be asking for a replacement.
|
|
Rutherford
Harmless
Posts: 8
Registered: 7-10-2019
Member Is Offline
|
|
Quote: Originally posted by karlos³ ![](images/xpblue/lastpost.gif) | Try to clean it up first, a small amount of course, and only then complain.
Tom is a very good guy and most helpful, he will surely replace it if your cleanup fails. |
Yeah he is great. He ended up offering me some more mercury at a reduced rate, which I think I'm going to take.
|
|
j_sum1
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 6256
Registered: 4-10-2014
Location: Unmoved
Member Is Offline
Mood: Organised
|
|
Sounds like a good option all round.
You get experience with handling and cleaning Hg, which is a good thing.
You get a reasonable quantity of Hg at a good price.
Tom gets an additional sale and a happy customer.
|
|
Boffis
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1850
Registered: 1-5-2011
Member Is Offline
Mood: No Mood
|
|
10% nitric acid attacks mercury rather slowly, the oxide dissolves almost instantly. By the time the mercury drops have coalesced its time to pour off
the acid and wash with a small amount of water several times. I collect the water washings separately let them evaporate down to a small volume
spontaneously and then store them until I have enough to be worth reprocessing.
|
|
diddi
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 723
Registered: 23-9-2014
Location: Victoria, Australia
Member Is Offline
Mood: Fluorescent
|
|
all my purchases from tom have been good. just saying.
Hg is easy to clean. i shake in HCl, then KMnO4, then water rinse and a dilute HNO3. then us a sep funnel to run it off. HCl is good for removing
stuff like Zn that can be amalgamated.
sometimes I receive old portions of Hg from people so anything is possible in terms of contaminants. if i get any from possible Au prospectors i have
to distill, but i usually do a batch rather than messing around setting up for small amounts.
Beginning construction of periodic table display
|
|
Bezaleel
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 444
Registered: 28-2-2009
Member Is Offline
Mood: transitional
|
|
Quote: Originally posted by Boffis ![](images/xpblue/lastpost.gif) | (...)
I collect the water washings separately let them evaporate down to a small volume spontaneously and then store them until I have enough to be worth
reprocessing. |
So the mercury stays in solution? Or does it just evaporate slower?
|
|