Burnt hotplate cord
As many amateur chemists have experienced, I had the unfortunate experience of allowing my hotplate cord to contact the hotplate for a few seconds.
After realising, I immedaitely removed the cord. Around 0.5 mm of the plastic covering to the cord was burnt off, but none of the contents were
visible. I removed the small plastic deposit on the hotplate and wrapped the exposed cord with electrical wire.
The hotplate should now be fully functional and hopefully safe. Are there any obvious unforseen dangers that I am missing?
|
|
markx
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 645
Registered: 7-8-2003
Location: Northern kingdom
Member Is Offline
Mood: Very Jolly
|
|
Change the cord out for a new one that is undamaged. The conduits might not be visible, but the internal insulation might have become damaged by the
heat and may cause a short after being bent or wrapped in the wrong way.
Exact science is a figment of imagination.......
|
|
Murexide
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 51
Registered: 1-12-2018
Member Is Offline
|
|
The cord is attached internally and leads directly into the hotplate. Is it still possible to replace such a cord?
|
|
Ubya
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1246
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline
Mood: I'm a maddo scientisto!!!
|
|
Quote: Originally posted by Murexide ![](images/xpblue/lastpost.gif) | The cord is attached internally and leads directly into the hotplate. Is it still possible to replace such a cord? |
by opening the case of your hotplate, yes
---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------
|
|
wg48temp9
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 769
Registered: 30-12-2018
Location: not so United Kingdom
Member Is Offline
|
|
and there is a good chance the power connections are push on spade connectors so you could replace the lead with one salvaged from some other
equipment but make certain the conductors are the same size/large or the salvaged equipment has the same or greater power rating.
Alternatively just cut the lead at the damage point and put a plug on it and if needed use an extension cord.
I am wg48 but not on my usual pc hence the temp handle.
Thank goodness for Fleming and the fungi.
Old codger' lives matters, wear a mask and help save them.
Be aware of demagoguery, keep your frontal lobes fully engaged.
I don't know who invented mRNA vaccines but they should get a fancy medal and I hope they made a shed load of money from it.
|
|
Tsjerk
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 20-4-2005
Location: Netherlands
Member Is Offline
Mood: Mood
|
|
You could cut out the damaged part and reconnect the wires with something like this. Then put some tape over the connector.
|
|
Praxichys
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1063
Registered: 31-7-2013
Location: Detroit, Michigan, USA
Member Is Offline
Mood: Coprecipitated
|
|
If you're worried about it, just cut out the damaged part and make the cord shorter. I've done this a couple of times having accidentally cut cords
with both a circular saw and an electric edger.
Cut out the damaged area, strip both ends, slide small heat shrink tube over each conductor and a large one over the whole cord, twist conductors
together, solder, shrink the tubes to cover the conductors, then shrink the larger one to contain the others. For my outdoor cords I usually put some
silicone caulk or dielectric grease under the heat shrink to waterproof the whole thing.
As mentioned, most strain reliefs are standardized and you can probably find a replacement cord if you're willing to open the case.
|
|
Deathunter88
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 511
Registered: 20-2-2015
Location: Beijing, China
Member Is Offline
Mood: No Mood
|
|
Honestly you're better off keeping it as is, you might just make it worse by trying to replace it. Based on your description of (a few seconds), I
have no idea why people think the internals could be damaged, unless your rubber suddenly changed into a superconductor of heat.
|
|
woelen
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7987
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
I agree with Deathunter88. As long as the cord is not damaged too much, keep it as is. Wrap some tape around it, just to be sure. I myself have
similarly damaged cords on some equipment, with dents in the isolation of half a mm or so. No problem at all.
If you take apart the heater, then you may introduce a bigger risk of electrical shock, if things do not fit nicely together after replacing the cord.
|
|
phlogiston
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1376
Registered: 26-4-2008
Location: Neon Thorium Erbium Lanthanum Neodymium Sulphur
Member Is Offline
Mood: pyrophoric
|
|
Hardware stores sell special heat-resistant cords for equipment that gets hot, like a clothes iron. The outer coating looks like it is some kind of
fibrous ceramic material. They are inexpensive.
Seems like a better replacement than the usual rubber or PVC cords.
-----
"If a rocket goes up, who cares where it comes down, that's not my concern said Wernher von Braun" - Tom Lehrer
|
|
SWIM
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 970
Registered: 3-9-2017
Member Is Offline
|
|
So I'm not quite clear on what you mean by hotplate.
If You're talking about a Corning or other lab type hotplate, especially a nice brand like Corning, I might be tempted to try some of the recommended
fixes above.
But if it's like the hotplate I used for many years which was just a single burner kitchen hotplate I bought for $15 (USD) Then I'd just leave it the
way it is.
The damage is shallow and you taped it up. That ought to do.
My old hotplate was the kind where the stuff to be heated sat on a flat metal coil that would get red hot when turned up.
I think back on all the reactions I did that way (Even making some pretty nasty stuff) and I'm amazed that I never cracked a flask. I even used to
heat RBFs on that thing, with the coil contacting maybe 2% of the flask.
Either I was very lucky, or Ace Makes some great glassware.
(Probably a bit of both)
|
|
Murexide
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 51
Registered: 1-12-2018
Member Is Offline
|
|
So the hotplate is a cheap ebay hotplate magnetic stirrer sold widely. Doesn't have temperature control functionality, used to be sold for about $50.
You can't find them anywhere now, they're replaced with the tempearture control variant (it says up to 100 degrees C, but I think it actually can go a
lot higher -anyone have any experience with these - https://www.ebay.com.au/itm/Value-1000ml-Magnetic-Stirrer-Mi... ).
I have very little experience with electronics and as a result any modification I make will probably make the situation worse.
Here's some photos of the hotplate / damage for reference (last photo shows damage)
Attachment: 1 (1.5MB) This file has been downloaded 388 times
Attachment: 2 (982kB) This file has been downloaded 368 times
Attachment: 3 (926kB) This file has been downloaded 355 times
Attachment: Damage wrapped with tape (1.5MB) This file has been downloaded 380 times
Attachment: Damage uncovered (317kB) This file has been downloaded 383 times
|
|
Deathunter88
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 511
Registered: 20-2-2015
Location: Beijing, China
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Murexide ![](images/xpblue/lastpost.gif) | So the hotplate is a cheap ebay hotplate magnetic stirrer sold widely. Doesn't have temperature control functionality, used to be sold for about $50.
You can't find them anywhere now, they're replaced with the tempearture control variant (it says up to 100 degrees C, but I think it actually can go a
lot higher -anyone have any experience with these - https://www.ebay.com.au/itm/Value-1000ml-Magnetic-Stirrer-Mi... ).
I have very little experience with electronics and as a result any modification I make will probably make the situation worse.
Here's some photos of the hotplate / damage for reference (last photo shows damage)
|
You are fine.
|
|
Sulaiman
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3621
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline
|
|
Based on the photograph, I would just wrap some pvc tape over the melted area and not worry about it.
As the damage was casued by a brief exposure to high temperature it is likely that the internal insulation is OK.
CAUTION : Hobby Chemist, not Professional or even Amateur
|
|