Bought a cheap ptfe rod, intend to cut it to small pieces to use as boiling chips. Wondering if they would be effective. Can they be washed and recycled for repeated use?

One thing I dun understand, ain't boiling chips supposed to be rough and porous? Ptfe is anything but, even those expensive ptfe boiling chips seem fairly smooth





View user's profile View All Posts By User
Deathunter88
National Hazard
****




Posts: 527
Registered: 20-2-2015
Location: Beijing, China
Member Is Offline

Mood: No Mood

[*] posted on 8-9-2019 at 22:43


Quote: Originally posted by artemov  
Bought a cheap ptfe rod, intend to cut it to small pieces to use as boiling chips. Wondering if they would be effective. Can they be washed and recycled for repeated use?

One thing I dun understand, ain't boiling chips supposed to be rough and porous? Ptfe is anything but, even those expensive ptfe boiling chips seem fairly smooth





Yeah all PTFE seems to have an almost magical effect in being able to facilitate smooth boiling. Most stir bars are smooth yet they are a good substitute for boiling chips.
View user's profile View All Posts By User
markx
National Hazard
****




Posts: 649
Registered: 7-8-2003
Location: Northern kingdom
Member Is Offline

Mood: Very Jolly

[*] posted on 8-9-2019 at 23:21


As far as I know solid PTFE parts are produced by pressing and sintering the virgin powder, so I guess at the microscopic level it is kind of uneven and perhaps also somewhat porous on the surface. It is a very slippery substance so this gives the illusion of it being very uniform and smooth.
Also it is for practical purposes pretty much indestructible by chemical means (apart from interactions with molten alkalies or media that require extremely high temperatures in excess of +300C), so yes, the chips can be washed and used indefinitely.


[Edited on 9-9-2019 by markx]




Exact science is a figment of imagination.......
View user's profile View All Posts By User
fusso
International Hazard
*****




Posts: 1922
Registered: 23-6-2017
Location: 4 ∥ universes ahead of you
Member Is Offline


[*] posted on 8-9-2019 at 23:39


But will the smaller oligomer molecules leach out during boiling solvents?



View user's profile View All Posts By User
Deathunter88
National Hazard
****




Posts: 527
Registered: 20-2-2015
Location: Beijing, China
Member Is Offline

Mood: No Mood

[*] posted on 9-9-2019 at 00:02


Quote: Originally posted by fusso  
But will the smaller oligomer molecules leach out during boiling solvents?


Probably wouldn't be too big a deal as I doubt tetrafluoroethane would be very reactive.
View user's profile View All Posts By User
teodor
National Hazard
****




Posts: 928
Registered: 28-6-2019
Location: Netherlands
Member Is Offline


[*] posted on 9-9-2019 at 01:46


I never tried PTFE rods, only pieces of PTFE tapes. I can say PTFE tape is not as effective as porcelain chips (also it is not sitting on the bottom but floating). I use porcelain chips made from a plate - I smashed a thick plate by a hammer. After boiling 85% H2SO4 and constant boiling point HBr with them the glaze was totally dissolved, so I got a totally unglazed chips. They work very well - I forgot about bumping at all.


[Edited on 9-9-2019 by teodor]
View user's profile View All Posts By User
happyfooddance
National Hazard
****




Posts: 530
Registered: 9-11-2017
Location: Los Angeles, Ca.
Member Is Offline

Mood: No Mood

[*] posted on 9-9-2019 at 22:49


Silica gel kitty litter works great and is cheap.

PTFE might look smooth and porous; the naked eye is a poor judge of such properties, however. Silica gel (or aerogels for that matter) look like perfectly smooth glass when carefully prepared, but air passes right throught them and they have more holes than they have solid space :o