[*] posted on 31-5-2019 at 11:12
NiSO4 storage


Hi.

Are any problems with storage of NiSO4? Can I do experiments with it in closed room? I know it is carcinogenic and I don't want to endanger anyone with bad storage or manipulation.
View user's profile View All Posts By User
CarlSagans_RayGuns
Harmless
*




Posts: 14
Registered: 9-4-2018
Member Is Offline

Mood: No Mood

[*] posted on 31-5-2019 at 12:19


I store mine at room temp in an HDPE jar. You want to make sure you avoid breathing any dust.
View user's profile View All Posts By User
reactofurnace
Hazard to Self
**




Posts: 76
Registered: 17-7-2015
Member Is Offline

Mood: Volatile

[*] posted on 31-5-2019 at 16:26
Heyyy


It should be fine just to store it in a regular glass jar or even a rigid plastic container.

Remember nickel salt are way more of a danger to handle once its dissolved in water. It can easily contact or skin or be over looked and thrown in the drain... which is bad. Sadly i know from experience but i try my best to practice safe chemistry now and learn from my mistakes.

a simple but not full proof way of recovering most transition metal salts is to form the carbonate by using a sodium bicarbonate solution.

Hope this helps. Stay safe.
View user's profile Visit user's homepage View All Posts By User
Amos
International Hazard
*****




Posts: 1406
Registered: 25-3-2014
Location: Yes
Member Is Offline

Mood: No

[*] posted on 31-5-2019 at 17:53


Long-term inhalation is what carcinogenicity is linked to. In other words you're better off keeping it as larger crystals than a fine, dry powder.
View user's profile View All Posts By User
Bedlasky
International Hazard
*****




Posts: 1241
Registered: 15-4-2019
Location: Period 5, group 6
Member Is Offline

Mood: Volatile

[*] posted on 31-5-2019 at 23:40


Quote: Originally posted by Amos  
Long-term inhalation is what carcinogenicity is linked to. In other words you're better off keeping it as larger crystals than a fine, dry powder.


Seller offers this NiSO4. It is small crystals than powder.



Quote: Originally posted by reactofurnace  

a simple but not full proof way of recovering most transition metal salts is to form the carbonate by using a sodium bicarbonate solution.


I thought I might it recover as nickel hydroxide. If I'll precipitate it and later dissolve it in acid there is no aerosol of Ni2+ (unlike carbonate).

But I don't know what I'll do with 1,5kg NiSO4 :(. 200g is enough for me.

[Edited on 1-6-2019 by Bedlasky]
View user's profile View All Posts By User
fusso
International Hazard
*****




Posts: 1922
Registered: 23-6-2017
Location: 4 ∥ universes ahead of you
Member Is Offline


[*] posted on 31-5-2019 at 23:52


Quote: Originally posted by Bedlasky  
But I don't know what I'll do with 1,5kg NiSO4 :(. 200g is enough for me.
Resell the remaining 1.3kg?



View user's profile View All Posts By User
CobaltChloride
Hazard to Others
***




Posts: 239
Registered: 3-3-2018
Location: Romania
Member Is Offline


[*] posted on 1-6-2019 at 01:37


I wouldn't worry about nickel sulfate stored in a closed container, be it plastic or glass (not metal since many metals can be corroded by nickel sulfate). It doesn't have any conceivable way of getting into the air under such circumstances.
View user's profile View All Posts By User
Bedlasky
International Hazard
*****




Posts: 1241
Registered: 15-4-2019
Location: Period 5, group 6
Member Is Offline

Mood: Volatile

[*] posted on 1-6-2019 at 02:24


Thanks all of you :).
View user's profile View All Posts By User