Author: Subject: Is there an alternative to dioxane yet for thermochemical sodium production?
John paul III
Hazard to Others
***




Posts: 110
Registered: 28-4-2018
Member Is Offline

Mood: No Mood

[*] posted on 26-5-2019 at 15:48
Is there an alternative to dioxane yet for thermochemical sodium production?


I've heard of many solvents being discovered as appropriate for the alcohol catalyzed sodium production, but was there ever an alternative found to dioxane for the separation of thermochemically produced sodium?
View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6338
Registered: 4-10-2014
Location: At home
Member Is Offline

Mood: Most of the ducks are in a row

[*] posted on 26-5-2019 at 16:03


Not as far as I am aware. Dioxane seems to just hit the sweet spot.
(Which is a real shame because my dioxane drying and purification abilities suck. My yield is embarrasingly low and the amount of polymeric gunk I have produced is ridiculous.)

[Edited on 27-5-2019 by j_sum1]




View user's profile View All Posts By User
John paul III
Hazard to Others
***




Posts: 110
Registered: 28-4-2018
Member Is Offline

Mood: No Mood

[*] posted on 27-5-2019 at 10:07


I wonder if tetrahydrofuran would work for potassium. It has a very similiar structure to dioxane, and way lower toxicity. lt's lower boiling point would unfortunately make it unsuitable for sodium.
View user's profile View All Posts By User
John paul III
Hazard to Others
***




Posts: 110
Registered: 28-4-2018
Member Is Offline

Mood: No Mood

[*] posted on 27-5-2019 at 10:32


I noticed Potassium/THF and Sodium/dioxane have the same difference between metal melting point and solvent boiling point. I wonder if this proximity could have a favorable effect on surface energy change

[Edited on 27-5-2019 by John paul III]
View user's profile View All Posts By User
clearly_not_atara
International Hazard
*****




Posts: 2801
Registered: 3-11-2013
Member Is Offline

Mood: Big

[*] posted on 27-5-2019 at 16:52


Time might be better spent improving the synthesis protocol for dioxane. I always assumed that its affinity for Mg2+ cations was important here.

I don’t think potassium is a reasonable replacement for sodium. Not only is it dangerous to handle, but I regularly hear people complain about not being able to afford ordinary potassium salts in quantity, much less the hydroxide.




Quote: Originally posted by bnull  
you can always buy new equipment but can't buy new fingers.
View user's profile View All Posts By User
UC235
National Hazard
****




Posts: 565
Registered: 28-12-2014
Member Is Offline

Mood: No Mood

[*] posted on 27-5-2019 at 19:35


I've not found dioxane too hard to make. Buy concentrated walmart brand antifreeze, add sulfuric acid, and distill until it starts getting black and foamy. Yes, there is a ton of dark garbage and polymer that drops out, but everything's pretty cheap.

Potassium hydroxide is only modestly more expensive than NaOH. You just can't buy it at the hardware store. Fortunately soapmaking and biodiesel supply websites both stock it in bulk.
View user's profile View All Posts By User
DavidJR
National Hazard
****




Posts: 908
Registered: 1-1-2018
Location: Scotland
Member Is Offline

Mood: Tired

[*] posted on 28-5-2019 at 03:11


Also, consider using fractional freezing as part of the purification process for dioxane.
View user's profile View All Posts By User
draculic acid69
International Hazard
*****




Posts: 1371
Registered: 2-8-2018
Member Is Offline


[*] posted on 30-5-2019 at 14:28


Already asked that question https://www.sciencemadness.org/whisper/viewthread.php?tid=14...
But it's good to see at least here one is moving the conversation forward.
View user's profile View All Posts By User
draculic acid69
International Hazard
*****




Posts: 1371
Registered: 2-8-2018
Member Is Offline


[*] posted on 30-5-2019 at 17:48


Im still thinking that chelating agents like diglyme or triglyme might be an alternative.where thf was suggested above as useful for K but not sodium one might trytetrahydropyran instead of thf or higher alkylated cyclic ethers.

[Edited on 31-5-2019 by draculic acid69]
View user's profile View All Posts By User
clearly_not_atara
International Hazard
*****




Posts: 2801
Registered: 3-11-2013
Member Is Offline

Mood: Big

[*] posted on 30-5-2019 at 19:32


There is no reason to prefer diglyme to dioxane: it’s harder to make, more expensive, harder to remove and just as carcinogenic.



Quote: Originally posted by bnull  
you can always buy new equipment but can't buy new fingers.
View user's profile View All Posts By User
draculic acid69
International Hazard
*****




Posts: 1371
Registered: 2-8-2018
Member Is Offline


[*] posted on 31-5-2019 at 03:56


Not sure diglyme even works it. Was just a suggestion.nothing so far has been proven to work apart from dioxane.whole point is to discover what works and what doesnt.,figure out alternatives and understand the mechanism and process of how it all works.