Cutting grooves on Al2O3 tube, carbide or diamond?
For some experiments with phosphors, I plan to make a tube furnace from a fused alumina tube (O.D. 26 mm, I.D. 19 mm, 500 mm long) and some nichrome
wire. I'd like to cut a helical groove on the outside of the alumina tube to hold the wire in place (think like the thread of a screw with the wire
coiled around it inside the groove). I might add some refractory mortar on top of that if necessary (e.g. to prevent heating element oxidation).
I'm thinking I'll make a helical mark with a pen on the tube. Then slowly rotate the alumina tube and use a high speed tool (Dremel) to make the
groove. Doens't have to be very deep, maybe 0.5-1 mm.
Now, alumina has a Mohs hardness of 9. So that narrows the choice of tool for the groove to tungsten carbide or diamond. I think a burr would be the
best tool here.
Do you think tungsten carbide would work? It also has a Mohs hardness of 9, so think it won't last long. Would diamond last much longer to justify the
investment?
EDIT:
Btw why do I want to use alumina? It has a very high thermal conductivity for a ceramic: 30 W/(m K).
Compare that to about 1 W/(m K) for glass. Copper is around 400. Lead and stainless steel are at around 30, the same as alumina.
Furthermore, alumina can withstand very high temperatures and has a low coefficient of expansion.
[Edited on 24-2-2019 by Heptylene]
|
|
markx
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 645
Registered: 7-8-2003
Location: Northern kingdom
Member Is Offline
Mood: Very Jolly
|
|
It is not a reasonable practice. You risk breaking the tube in the process and introduce fracture points into the alumina core that very likely shall
contribute to cracking in the process of using the kiln later on.
I would suggest to leave the alumina tube as is and just wind the heating element straigth onto the core. You can secure it with some high temperature
glass fibre material and refractory mortar, surrounded by a close matching case carved from soft fire brick. The heating wire is not going anywhere
and you stand less of a chance to end up with a broken kiln core on first use.
If you still insist on trying to carve grooves into the core tube, then using abrasive diamond tools is the only practical option. They are widely
available and cheap. Carbide tooling shall not be up to the task.
I would also suggest to build some kind of a fixture or jig so you can hold and rotate the workpice and guide the tool securely. Trying to perform
such a operation in freehand mode is likely going to fail.
Exact science is a figment of imagination.......
|
|
andy1988
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 135
Registered: 11-2-2018
Location: NW Americus ([i]in re[/i] Amerigo Vespucci)
Member Is Offline
Mood: No Mood
|
|
See this note on the use of ceramic paper (I hadn't tried myself, but looks relevant).
I'm looking into laser assisted machining on a lathe myself (for ceramics).
|
|
Heptylene
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 319
Registered: 22-10-2016
Member Is Offline
Mood: No Mood
|
|
markx: I hadn't thought about cracking the tube. You're right that could be a big problem. The thing is the wire will be in a rather tightly spaced
coil (maybe 5 mm between wires) and upon heating the coil will expand and I run the risk of shorting adjacent loops of wire. Guess I'll use mortar as
you suggested then.
andy1988: that ceramic paper could be useful. I planned on using silica sleeve such as this, but ceramic paper could be handy.
|
|
Geocachmaster
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 146
Registered: 5-3-2016
Location: Maine, USA
Member Is Offline
Mood: Corroded, just like my spatulas
|
|
I agree with markx, just wrap the wire and use some mortar to hold it in place. I made a tube furnace like this using ~2 mm spacing between wraps and
some Dap high heat mortar to attach it. It worked out just fine.
|
|
Twospoons
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1306
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline
Mood: A trace of hope...
|
|
If you use Kanthal instead of nichrome you have less risk of shorting. On heating Kanthal builds a surface layer of aluminium oxide that protects the
wire from further oxidation and also helps provide turn to turn insulation..
Helicopter: "helico" -> spiral, "pter" -> with wings
|
|