Author: Subject: Quenching of bluish fluorescence ...
john_007
Harmless
*




Posts: 5
Registered: 8-1-2019
Member Is Offline


[*] posted on 8-2-2019 at 06:57
Quenching of bluish fluorescence ...


I have the Polyester resin which contains bluish fluorescence.
It is water clear but has bluish ring..of fluorescence.
How can I quench this fluorescence..
Is it possible??
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5126
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 8-2-2019 at 08:09


You might be able to add (or paint on) something which absorbs UV strongly, but doesn't fluoresce.
View user's profile View All Posts By User
Tsjerk
International Hazard
*****




Posts: 3032
Registered: 20-4-2005
Location: Netherlands
Member Is Offline

Mood: Mood

[*] posted on 8-2-2019 at 09:33


Does it have to stay water clear?
View user's profile View All Posts By User
Heptylene
Hazard to Others
***




Posts: 319
Registered: 22-10-2016
Member Is Offline

Mood: No Mood

[*] posted on 9-2-2019 at 02:44


What about adding dibenzylideneacetone? It is used in sunscreen. Slightly yellow but it is non fluorescent.
View user's profile View All Posts By User
john_007
Harmless
*




Posts: 5
Registered: 8-1-2019
Member Is Offline


[*] posted on 9-2-2019 at 22:35


Quote: Originally posted by Tsjerk  
Does it have to stay water clear?

Yes..it is better if it remains.
I thought uv absorber could be helpful..but don't have uv absorber.
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5126
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 10-2-2019 at 06:03


Can you buy sunscreen and see if it helps?
View user's profile View All Posts By User
walruslover69
Hazard to Others
***




Posts: 232
Registered: 21-12-2017
Member Is Offline

Mood: No Mood

[*] posted on 11-2-2019 at 06:05


Potassium iodide is a fairly good quencher for Fluorescein in solution that i have used in the lab before. It would probably work for you
View user's profile View All Posts By User

  Go To Top