How to create a gold mirror?
Has anyone ever successfully made a gold mirror in a test tube, much like the silver Tollens reaction does?
I understand that it really depends on your reducing agent as gold will be much more easily reduced. And you can't prepare that soluble ammine complex
like with silver.
I found one description that used AuCl3 in combination with Ethanol / Acetaldehyde and Glucose to get a slow reaction. But it would never
mirror out at all.
Perhaps some of you guys has an idea.
|
|
wg48
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 821
Registered: 21-11-2015
Member Is Offline
Mood: No Mood
|
|
The following Review of Electroless Gold Deposition Processes may be useful to you
Attachment: Review ofElectroless Gold Deposition Processes.pdf (4.4MB) This file has been downloaded 594 times
Borosilicate glass:
Good temperature resistance and good thermal shock resistance but finite.
For normal, standard service typically 200-230°C, for short-term (minutes) service max 400°C
Maximum thermal shock resistance is 160°C
|
|
Chemetix
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 375
Registered: 23-9-2016
Location: Oztrayleeyah
Member Is Offline
Mood: Wavering between lucidity and madness
|
|
What do you actually want to achieve? You can use a flame to vapour deposit gold onto glass or you can use a standard lustre paint to fire it on to
either glass or ceramic. There is electrodeposition onto a suitably prepared surface as well. No point going into details until we get some idea about
the objective you wish to accomplish.
|
|
j_sum1
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 6250
Registered: 4-10-2014
Location: Unmoved
Member Is Offline
Mood: Organised
|
|
I am going to answer that question for myself, Chemetix. I have always fancied samples of Cu, Ag and Au for my element collection: identical test
tubes with the metal mirror inside and ampouled shut to avoud dust and damage.
Ag is well documented. Cu and Ag less so.
|
|