Substitute for carbon tetrachloride
Hey guys, I was wondering if anyone knew of a good substitute for carbon tetrachloride? I am making nylon 6,6 through adipoyl chloride, and need
something that help form adipoyl chloride.
Thanks
|
|
EilOr
Harmless
Posts: 20
Registered: 12-12-2017
Member Is Offline
Mood: No Mood
|
|
Carbon tetrachloride can be nearly always be subsitute with Chloroform
If chlorform isn't available, I this case I would use low boiling petrol ether (or pentane/hexane etc.) . I used pentane myself for Nylon 6,6. it also
works good enough.
[Edited on 4-1-2019 by EilOr]
|
|
Ubya
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1247
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline
Mood: I'm a maddo scientisto!!!
|
|
i used dichloromethane and the reaction worked without any problems
---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------
|
|