Getting rid of CuCl2 impure junk
I just made Copper chloride and filtered off the junk.
My question is wether I can just wash it down the sink since copper chloride has been known to etch metals
|
|
j_sum1
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 6256
Registered: 4-10-2014
Location: Unmoved
Member Is Online
Mood: Organised
|
|
I always avoid putting Cu down the sink for environmental reasons. Precipitate basic copper carbonate, filter and dispose as solid.
My preferred disposal method is to set into a block of concrete and then discard to landfill.
|
|
Amos
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1406
Registered: 25-3-2014
Location: Yes
Member Is Offline
Mood: No
|
|
How on earth did you make it this way, copper, HCl, and H2O2? I would try adding some hydrochloric acid to both the filtrate and the precipitate and
warming; it looks like you have copper oxychloride forming in your process from atmospheric oxygen, copper metal, and CuCl2 comproportionating.
|
|
lordcookies24
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 78
Registered: 2-1-2019
Location: pluto
Member Is Offline
Mood: curious
|
|
Quote: Originally posted by Amos ![](images/xpblue/lastpost.gif) | How on earth did you make it this way, copper, HCl, and H2O2? I would try adding some hydrochloric acid to both the filtrate and the precipitate and
warming; it looks like you have copper oxychloride forming in your process from atmospheric oxygen, copper metal, and CuCl2 comproportionating.
|
yea i did make it that way, a 1000ml where i added copper, hcl, and h202. when it stopped bubbling that meaned the reaction was over so i filtered it,
then i went to vocation (forgot about this project) and came home to find it completely crystallized, then i re added water to it, swirled it around
and wanted to add it to a mason jar, but some weird stuff at the bottom was not dissolving, so i filtered it(as seen above) and here i am now.
|
|
draculic acid69
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1371
Registered: 2-8-2018
Member Is Offline
|
|
What source of Cu metal did you use? I made CuSO4 from speaker/headphone wire once and there was definitely a grey/black sludge leftover in the blue
solution that wouldn't dissolve. I suspected it to be lead or iron impurities.the sulfuric was clear 98% from chem supply chain.not sure if impurities
were from acid or metal.apparently Cu wire is supposed to be extremely pure.after this experiment im not so sure though.
|
|
fusso
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1922
Registered: 23-6-2017
Location: 4 ∥ universes ahead of you
Member Is Offline
|
|
Why not precipitate the Cu2+ and save for future use? Scrap Cu takes ages to oxidize.
|
|
lordcookies24
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 78
Registered: 2-1-2019
Location: pluto
Member Is Offline
Mood: curious
|
|
Quote: Originally posted by draculic acid69 ![](images/xpblue/lastpost.gif) | What source of Cu metal did you use? I made CuSO4 from speaker/headphone wire once and there was definitely a grey/black sludge leftover in the blue
solution that wouldn't dissolve. I suspected it to be lead or iron impurities.the sulfuric was clear 98% from chem supply chain.not sure if impurities
were from acid or metal.apparently Cu wire is supposed to be extremely pure.after this experiment im not so sure though. |
I bought some very unexpensive copper pipe attackments shown below since I had no scrap
|
|
lordcookies24
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 78
Registered: 2-1-2019
Location: pluto
Member Is Offline
Mood: curious
|
|
I disposed of it by mixing it with aluminium to get the copper then flushing the aluminium chloride down the drain with plenty of water, it might not
be the best for the environment but I had to get use of my beaker again since I don't have much to go around.
|
|
draculic acid69
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1371
Registered: 2-8-2018
Member Is Offline
|
|
I also tried using a piece of. Copper pipe but it seemed like it would take a week to dissolve in boiling h2so4 solution.
|
|