Make Calcium carbonate from calcite


Hi All

I have some Calcite and I wanted to purify calcium carbonate from it. What would you suggest is the best way to do this.

Thanks

Housane
View user's profile View All Posts By User
Foeskes
Hazard to Others
***




Posts: 156
Registered: 25-2-2017
Member Is Offline

Mood: No Mood

[*] posted on 28-11-2018 at 02:52


Well if it's clear or white, then I'd say it's pretty pure especially if it's in the form of large crystals.
View user's profile View All Posts By User
Housane
Hazard to Others
***




Posts: 127
Registered: 3-9-2018
Location: Worcester, England
Member Is Offline

Mood: Let’s make

[*] posted on 28-11-2018 at 10:19


Hi how can I then make it into a powdered form to make calcium hydroxide what would you subject is best. The chunks are rather large
View user's profile View All Posts By User
fusso
International Hazard
*****




Posts: 1922
Registered: 23-6-2017
Location: 4 ∥ universes ahead of you
Member Is Offline


[*] posted on 28-11-2018 at 12:02


Just heat it up to 8xxC to form CaO. The pressure from released CO2 will break the chunks apart.



View user's profile View All Posts By User
Ubya
International Hazard
*****




Posts: 1247
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline

Mood: I'm a maddo scientisto!!!

[*] posted on 28-11-2018 at 12:08


Quote: Originally posted by fusso  
Just heat it up to 8xxC to form CaO. The pressure from released CO2 will break the chunks apart.

then add water and a slurry of calcium hydroxide will form (be careful of the exothermic reaction)





---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------
View user's profile View All Posts By User
Housane
Hazard to Others
***




Posts: 127
Registered: 3-9-2018
Location: Worcester, England
Member Is Offline

Mood: Let’s make

[*] posted on 1-12-2018 at 13:44


Hi Ubya how did you get the part at the bottom
View user's profile View All Posts By User
fusso
International Hazard
*****




Posts: 1922
Registered: 23-6-2017
Location: 4 ∥ universes ahead of you
Member Is Offline


[*] posted on 1-12-2018 at 14:47


Quote: Originally posted by Housane  
Hi Ubya how did you get the part at the bottom
Filtering.



View user's profile View All Posts By User
MrHomeScientist
International Hazard
*****




Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline

Mood: No Mood

[*] posted on 3-12-2018 at 14:09


Well calcite is already calcium carbonate, so smash it with a hammer and you're done!

If you want to ensure purity, probably the easiest way would be:
1) Crush the rock as much as you can with a hammer / mortar & pestle.
2) Dissolve the rock in vinegar. May take a few hours or days; wait until the bubbling stops, then add a bit more vinegar and make sure bubbling doesn't start up again.
3) Filter off any undissolved rock. The solution contains calcium acetate.
4) Add baking soda to the solution. This precipitates the calcium back out as carbonate.
4a) It might be better to first dissolve the baking soda in its own solution, then add that to the acetate solution. This way you know the precipitation is done if you add baking soda solution and no more is observed.
View user's profile Visit user's homepage View All Posts By User