Author: Subject: Removing silver from glassware
nitroglycol
Hazard to Self
**




Posts: 56
Registered: 28-10-2005
Location: close to the centre of North America
Member Is Offline

Mood: curious

[*] posted on 27-11-2005 at 18:04
Removing silver from glassware


Recently I came into the possession of a nice 500 mL volumetric flask. Only thing is, it was used to store silver nitrate, and has deposits on the inside surface that I presume to be silver. I suppose given silver's inertness this is more of an aesthetic issue than anything, but I still want to get it clean, and that same inertness makes it darn difficult to do so. Yesterday I filled it with a mix of vinegar and "green" bleach (a hydrogen peroxide solution of unspecified concentration), hoping that this would oxidize the silver, which in turn would allow it to be dissolved by the vinegar. So far, though, no visible changes have occurred. I know nitric acid should work, but finding that would probably be much more difficult than getting a new flask.

Any suggestions?
View user's profile Visit user's homepage View All Posts By User
neutrino
International Hazard
*****




Posts: 1583
Registered: 20-8-2004
Location: USA
Member Is Offline

Mood: oscillating

[*] posted on 27-11-2005 at 18:23


Chloride will form insoluable AgCl percipitates which will block further chemical action.

Hot, concentrated sulfuric acid may work. Otherwise, I suggest to start scrubbing.
View user's profile View All Posts By User
The_Davster
A pnictogen
*******




Posts: 2861
Registered: 18-11-2003
Member Is Offline

Mood: .

[*] posted on 27-11-2005 at 18:47


Do you have acess to potassium permanganate? An acidic solution of it should dissolve silver.



View user's profile View All Posts By User
chochu3
Hazard to Others
***




Posts: 185
Registered: 21-10-2003
Location: South Side Tejas [Cloverland]
Member Is Offline

Mood: Inside looking out

[*] posted on 27-11-2005 at 22:42


Nitric acid will also work. In lab we did some test which made a silver mirror on the bottom of the test tube in organic lab, we then instructed to use nitric acid to remove it.



\"Abiding in the midst of ignorance, thinking themselves wise and learned, fools go aimlessly hither and thither, like blind led by the blind.\" - Katha Upanishad
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5134
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 28-11-2005 at 00:23


Sodium thiosulphate (photographic fixer) might do a useful job of removing any silver salts present.
If there is free silver present (and I expect there will be) you might be able to oxidise it with iodine then disolve the iodide with thiosulphate. You might need to do this a few times if the deposit is thick.
View user's profile View All Posts By User
nitroglycol
Hazard to Self
**




Posts: 56
Registered: 28-10-2005
Location: close to the centre of North America
Member Is Offline

Mood: curious

[*] posted on 28-11-2005 at 02:55


Thanks, unionized! That sounds like the most practical approach (scrubbing is only possible on the outside and the neck- the inside of the main part of the flask is rather hard to reach).
View user's profile Visit user's homepage View All Posts By User
unionised
International Hazard
*****




Posts: 5134
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 28-11-2005 at 12:51


If it doesn't work I recommend scrubbing the inside of the flask using a slurry of lead-shot and salt in water. Used for many years (centuries) by butlers cleaning decanters. Sometimes the old ways are the best.