Check out this video on melting lead - is this "dross" or oxide?
So this guy goes through all kinds of steps trying to purify his lead, placing candle wax into the molten lead (to release the "dross") and then he
keeps scraping the surface (like 40 times) to remove the very thin layer of "dross" (I think it's normal oxide).
Go to about 27:30 in the video, once he removes the obvious dross he then starts dropping in candles and such.
https://www.youtube.com/watch?v=fTRwfyvIbkc
1.5 million views and I'm thinking this wax doesn't remove dross but helps with the oxidation layer which he is calling dross. IIRC, somthing like
sawdust would work as well and would burn slower. Sawdust would work especially if pouring from the bottom of the pan through a spout.
|
|
Ubya
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1247
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline
Mood: I'm a maddo scientisto!!!
|
|
i've heard of people using wax, oil, sawdust and even car tires, just anything that stops oxygen from reaching the molten lead
i have maybe 10kg of "dross" and corroded lead batteries electrodes, i'm planning on turning everything back to lead metal by real smelting (i don't
know why people say "smelting" lead when they are just melting it)
---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------
|
|
Tsjerk
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 20-4-2005
Location: Netherlands
Member Is Offline
Mood: Mood
|
|
Quote: Originally posted by Ubya ![](images/xpblue/lastpost.gif) |
i have maybe 10kg of "dross" and corroded lead batteries electrodes, i'm planning on turning everything back to lead metal by real smelting (i don't
know why people say "smelting" lead when they are just melting it) |
In dutch "smelting" sounds like "smelten", which literally means melting. I don't know why people use the term smelting in English but it might be
because it means something else in other languages.
|
|
fusso
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1922
Registered: 23-6-2017
Location: 4 ∥ universes ahead of you
Member Is Offline
|
|
I'm very sure dross is mixture of Pb oxide+other impurities. He obviously can't distinguish between dirt and oxide. He kept scraping the shiny surface
to make more oxide thus wasting lead and creating more waste just drove me crazy![:mad:](./images/smilies/mad.gif) ![:mad:](./images/smilies/mad.gif) ![:mad:](./images/smilies/mad.gif)
[Edited on 181103 by fusso]
|
|
Fulmen
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1699
Registered: 24-9-2005
Member Is Offline
Mood: Bored
|
|
Wax does separate dross from the metal quite effectively. The oxides sticks to the metal, allowing quite large particles to be caught below the
surface. The wax absorbs into the oxides, breaking the wetting effect.
We're not banging rocks together here. We know how to put a man back together.
|
|
RogueRose
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1590
Registered: 16-6-2014
Member Is Offline
|
|
Quote: Originally posted by fusso ![](images/xpblue/lastpost.gif) | I'm very sure dross is mixture of Pb oxide+other impurities. He obviously can't distinguish between dirt and oxide. He kept scraping the shiny surface
to make more oxide thus wasting lead and creating more waste just drove me crazy![:mad:](./images/smilies/mad.gif) ![:mad:](./images/smilies/mad.gif) ![:mad:](./images/smilies/mad.gif)
[Edited on 181103 by fusso] |
Ok, that is what I thought as well. I didn't know if I had misunderstood what the surface layer was or not. I thought it was oxide but wasn't sure.
|
|
Melgar
Anti-Spam Agent
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2004
Registered: 23-2-2010
Location: Connecticut
Member Is Offline
Mood: Estrified
|
|
Wax protects the surface from oxygen, but also can reduce lead oxide to metallic lead at high enough temperatures. It's also probably the best thing
you can use since it would float on the surface, doesn't catch fire very easily, and is made entirely of hydrogen and carbon. It's also pretty cheap
and easy to remove any residues. Sawdust would leave ash behind, which is mostly silicates and carbonates from groups I and II.
[Edited on 11/4/18 by Melgar]
The first step in the process of learning something is admitting that you don't know it already.
I'm givin' the spam shields max power at full warp, but they just dinna have the power! We're gonna have to evacuate to new forum software!
|
|
fusso
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1922
Registered: 23-6-2017
Location: 4 ∥ universes ahead of you
Member Is Offline
|
|
Quote: Originally posted by Melgar ![](images/xpblue/lastpost.gif) | Sawdust would leave ash behind, which is mostly silicates and carbonates from groups I and II.[Edited on 11/4/18 by Melgar] | Why's there silicate in woodash?!
|
|
kulep
Harmless
Posts: 46
Registered: 19-5-2018
Location: Somewhere below the tropic of Capricorn
Member Is Offline
Mood: Spicy
|
|
stronger and more abrasive plants aren't eaten that easily by pesky animals, grasses usually have high silicates contents tho, I don't know so much
about wood.
rice hulls for example have a veeery high silicate content
"Rice husk was found to have lower extractives content and higher ash content, in comparison with other residues. The high ash content is
associated with a large amount of silica (SiO 2 ); the analysis detected 8.32% of silica."
CHARACTERIZATION OF RESIDUES FROM PLANT BIOMASS FOR
USE IN ENERGY GENERATION
[Edited on 5-11-2018 by kulep]
|
|
Fulmen
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1699
Registered: 24-9-2005
Member Is Offline
Mood: Bored
|
|
Iirc the bark is usually rich in silicates, I suspect it's part of it's fire resistance.