Rooto vs Liquid Fire
Rooto Professional Drain Opener is 60-100% sulfuric acid with no other listed ingredients.
Amazing Liquid Fire is sulphuric acid with rodine 31a.
Rodine 31A msds is attached.
Most of the ingredients boil off at high heat except:
Alkylphenol Ethoxylate which has a boiling point just below sulfuric acid (293-297) for the nonyl variety which is the most commonly available.
I suspect Rooto has similar crud in it.
But from the look of it we can clean these up simply by bringing it to boiling.
Has anyone analyzed the which one of these is best for a home chemist?
Attachment: 1816~v~msds_8256.pdf (35kB) This file has been downloaded 694 times
|
|
MrHomeScientist
International Hazard
   
Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline
Mood: No Mood
|
|
I have never found Rooto where I am, but I do use Liquid Fire. Mine is red/orange, which I assumed was due to dissolved carbon. It might look bad but
it works just fine as-is, at least for my purposes. I've heard that Rooto can be water clear or pitch black; probably depending on the source. Drain
cleaner acid is basically industrial waste, after all. A study of the differences between the brands would be interesting to see.
|
|
CobaltChloride
Hazard to Others
 
Posts: 239
Registered: 3-3-2018
Location: Romania
Member Is Offline
|
|
In Europe they sell Cleamen 420 drain cleaner. The MSDS lists the only ingredient being 98% sulfuric acid. Its color varies from crystal clear to
very, very light brown. The brown color is most probably from the bottle because I've noticed that the clear acid gradually turns very light brown
when stored in its original HDPE bottle.
So far it has worked very well for making esters and HNO3 for me. The ester I made with it (ethyl acetate) didn't have any weird smell at the end
(some people had weird smelling products when using drain acid as a catalyst).
I know this is sold in multiple European states, so you might just be able to find it in the USA, although chances of this being the case are slim
because shipping would cost a lot and be dangerous.
|
|
happyfooddance
National Hazard
  
Posts: 530
Registered: 9-11-2017
Location: Los Angeles, Ca.
Member Is Offline
Mood: No Mood
|
|
Thank you macckone, I had been searching for this msds for a while to no avail, I have a container of Kleenout brand H2SO4 which claims to be "highly
inhibited" by this rodine stuff, but I couldn't find out what it was.
I think at least some of its components might decompose when heated in concentrated acid, because it is crystal clear from the jug, turned caramel to
medium brown when heated in a beaker to boiling, and takes about 20-30 minutes of sustained boiling to completely clear. My acid before heating
titrated @ about 91 percent IIRC (don't have my notes right here).
Or it could be that or a moth flew in the beaker when I wasn't looking as this was done outside (but decently covered).
|
|
RogueRose
International Hazard
   
Posts: 1597
Registered: 16-6-2014
Member Is Offline
|
|
I think you are mistaken on the Rooto. I just found some good SDS/MSDS and I requested the latest from the company (they should email it to me soon I
hope).
Check out the SG and it looks like it is listed as 93.19%, I doubt there is other stuff in it either.
Attachment: Rooto - H2SO4 - 40153573_MSDS.pdf (1.6MB) This file has been downloaded 749 times
Attachment: ROOTO Drain Opener-Sulfuric Acid MSDS.pdf (94kB) This file has been downloaded 831 times
|
|
macckone
Dispenser of practical lab wisdom
   
Posts: 2171
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline
Mood: Electrical
|
|
Happyfooddance:
All of the components should either decompose or evaporate in hot oxygenated sulfuric acid.
RogueRose,
On the first data sheet it lists the composition as 60 - 100% sulfuric acid under section VI at the bottom of the page.
On the second one it lists the sulfuric acid as 92% of the mix but doesn't list what the other 8% is or is not. Nor does it list the strength of the
sulfuric acid that was added.
The Rodine 31A is an inhibitor which also contains sulfuric acid.
Rooto likely contains an inhibitor as well but we don't know what or the quantity.
If it is 92% sulfuric acid with 8% Rodine 31A which is up to 30% acid itself then it could well be 93%.
And given the available data Rooto could range in composition, I don't know how much though. MSDS are usually much more liberal than the actual
composition.
|
|
RogueRose
International Hazard
   
Posts: 1597
Registered: 16-6-2014
Member Is Offline
|
|
Quote: Originally posted by macckone  | Happyfooddance:
All of the components should either decompose or evaporate in hot oxygenated sulfuric acid.
RogueRose,
On the first data sheet it lists the composition as 60 - 100% sulfuric acid under section VI at the bottom of the page.
On the second one it lists the sulfuric acid as 92% of the mix but doesn't list what the other 8% is or is not. Nor does it list the strength of the
sulfuric acid that was added.
The Rodine 31A is an inhibitor which also contains sulfuric acid.
Rooto likely contains an inhibitor as well but we don't know what or the quantity.
If it is 92% sulfuric acid with 8% Rodine 31A which is up to 30% acid itself then it could well be 93%.
And given the available data Rooto could range in composition, I don't know how much though. MSDS are usually much more liberal than the actual
composition. |
it may say 60-100 but look at the SG of 1.8354, which is the correct number for 93.19%. if it is 1.8345g/ml then we are looking at 93-94.5% H2SO4
from my calculations.
again, the seconf one, look at the specific gravity - 1.835 and lists 94%n which is right where I posted it in the paragraph above.
I'm pretty certain that it is pure H2SO4 (plus H2O).
I did contact the company and asked if there was anything other than H2SO4 and asked for the most up to date SDS, MSDS, etc for the product.
We will see when it comes in.
**EDIT - IT's HERE!!
93% H2SO4
7% water
Attachment: Rooto SDS from the manufacturer (2.8MB) This file has been downloaded 629 times
|
|
JJay
International Hazard
   
Posts: 3440
Registered: 15-10-2015
Member Is Offline
|
|
Regardless of what the SDS says, Rooto 1084 definitely has pickling agents and possibly other substances in it. If you boil it off, it leaves a
residue. If you put stainless steel into it, a sticky black coating forms.
|
|
macckone
Dispenser of practical lab wisdom
   
Posts: 2171
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline
Mood: Electrical
|
|
It appears that there are multiple products with the same name but different product numbers. Here we are getting Rooto 1069.
Even the MSDS provided says there may be trace chemicals up to 1% which could include the inhibitors. Which for my purposes 93% with 1% impurities
should be fine. Heat it up and allow water to evaporate with any impurities getting eaten by the hot acid and atmospheric oxygen.
|
|
JJay
International Hazard
   
Posts: 3440
Registered: 15-10-2015
Member Is Offline
|
|
I distill mine if I'm using it for anything where I am really concerned about the purity of the sulfuric acid. For most purposes, that's not
necessary.
|
|
XeonTheMGPony
International Hazard
   
Posts: 1641
Registered: 5-1-2016
Member Is Offline
Mood: No Mood
|
|
I add some 35% H2O2, then reflux to max temp as it burns off any thing that will oxidize, then distill it separating out the fractions (2 in this case
any thing below 3xx and every thing after 3xx)
Weak fraction gets labeled "General purpose sulfuric acid" the concentrated is just called Sulfuric acid.
Upon final distillation I often find clear cubic crystals in the bottom along with the last bits of H2SO4, this is not discarded, it is kept in a
separate container labeled Sulfuric acid dist, dregs.
These dregs is what I used to make SO3 thanks to the max concentration of it and a good way to recycle what would other wise be lost product!
Honestly if you want good reliable results, distill distill and distill again for good measure, sure it is tedious and boring, but it does hone your
skills at distilling and it gets easier with every run (Which ironically makes it even more boring!)
As a warning, sulfuric loves to bump, nothing I do seems to get rid of it, but it is manageable, which means you must be there through the whole run!
|
|
macckone
Dispenser of practical lab wisdom
   
Posts: 2171
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline
Mood: Electrical
|
|
The denser the fluid the worse it bumps. Sulfuric at boiling is well over 1.8 in any decent concentration.
|
|