I would like to perform the reduction of Iron III in hydrogen.
I have seen this done in a "boiling tube". Something like a heavy test tube with a vent at the closed end. I have also seen this done in a "reduction
tube" a narrow version of the same.
In both cases the glass is much thicker than anything I have here, leading me think that creating it from glass I have won't work well.
I've checked out my normal glassware sources, Dr. Bob's spreadsheet, and a done a number of searches.
First time I've been stumped looking for an apparatus, I'm sure it won't be my last. Do any of you know of a source for glassware that might stock
these?
|
|
Ubya
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1247
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline
Mood: I'm a maddo scientisto!!!
|
|
maybe you are looking for something like this
---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------
|
|
JScott
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 51
Registered: 23-8-2018
Member Is Offline
|
|
@Ubya,
That's darned close to a boiling tube, but not heavy enough. The one's I've seen and then read about talk about a large scale test tube with glass
much heavier.
The other, the 'reduction tube' may be very similar to a part used on some rotovaps though I don't know it they are of the same gauge glass either.
If I can find no other, at least that has a port to show hydrogen flame color and size at the sealed end of the tube.
Thanks for getting back to me, and thanks for the new addition to my bookmarks!
[Edited on 9-7-2018 by JScott]
|
|
Dr.Bob
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2689
Registered: 26-1-2011
Location: USA - NC
Member Is Offline
Mood: No Mood
|
|
I have many Ace and Chemglass heavy walled tubes for high pressure reactions, from 10 ml to 250 ml. What I don't have is many caps or top fittings
for them, so if you just want to use a tube (they are all threaded on the top with Ace type threads) and try to find the right fitting for them, let
me know. I do have some fittings, just not sure which are good for what. But the tubes are rated for several atm of pressure ( I thin up to
100-150 psi, maybe higher), assuming that you can seal them properly and such. See the link below for examples:
https://www.aceglass.com/results.php?t=8648
https://www.aceglass.com/seals.php
https://www.aceglass.com%2Fhtml%2F3dissues%2FPressure_Vessel...
Chemglass has some similar products.
|
|
JScott
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 51
Registered: 23-8-2018
Member Is Offline
|
|
@DrBob,
This is what I'm trying to do.
Will your tube fit the bill? I should have written you, but I did check your list first. I don't expect high pressure, but it will be a high
temperature reaction.
One of the those links doesn't work, and one brought me to a tube that was threaded on one end. It is important that the glass be heavy due to direct
exposure to the flame I think.
[Edited on 9-7-2018 by JScott]
[Edited on 9-7-2018 by JScott]
|
|
Ubya
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1247
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline
Mood: I'm a maddo scientisto!!!
|
|
but it's not cheapi understood what you want, the tube is thick walled but if the heat is enough borosilicate will soften, you need fused quartz
---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------
|
|
JScott
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 51
Registered: 23-8-2018
Member Is Offline
|
|
Wow, thank you! I was thinking I would never see one for sale. So much for Goggle and Duck, Duck Go. I guess search engines can only take you so far.
You are right, it's not cheap, but that's what piggy banks are for. Life is short, if you can't break the pig now and again, what's the point?
I also thank you for yet another valuable book mark. I wonder why search engines ignore these sites?
|
|
Ubya
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1247
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline
Mood: I'm a maddo scientisto!!!
|
|
use google images
---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------
|
|
Dr.Bob
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2689
Registered: 26-1-2011
Location: USA - NC
Member Is Offline
Mood: No Mood
|
|
If you want to heat it with a flame or to ridiculous temperatures, quartz is the way to go, the pressure tubes are only rated to about 200-300 C,
depending on type and use. Also, thicker glass is much less resistant to flame heating than thin glass, as the difference between the inside and
outside temperature of thick glass creates stress, so thick glass works much better with gradual and gentle heating.
But quartz can handle heat stress even better. The tubes from Perkin Elmer look made for elemental analyzers, and might be too small, depending on
your scale.
There is a company called prism glass that also does quartz work, which might be more approachable for custom work or dealing with individuals. They
are here in NC, but there are a few other small quartz shops in the US, just google quartz fabricators or the like.
If you have a specific item you want, they might be able to help.
www.prismresearchglass.com/
If anyone is interested in pressure tubes, I can try to make a list sometime, most are in a couple of boxes right now.
[Edited on 8-9-2018 by Dr.Bob]
|
|
JScott
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 51
Registered: 23-8-2018
Member Is Offline
|
|
Dr. Bob,
I will probably spring for that quartz tube you showed me sometime in the near future. That is providing that company will set up an account for an
amateur. Having survived on mostly Chinese glass I haven't had to go through any formalities in the past.
Ubya,
I thought I had used Goggle images, but if you've found one for sale that way I must have bunged it up somehow ;-)
Thanks everyone for your help.
|
|
JScott
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 51
Registered: 23-8-2018
Member Is Offline
|
|
Ah, so close but no cigar! That reduction would have been perfect.
Should anyone else be interested, I haven't been able "shop online" without an account number.
Though I'm sure if I call them in the morning and explain I am home experimenter they will forgo any of the aforementioned formalities. ![;)](./images/smilies/wink.gif)
EDIT:
Then I find this! That is the very item listed on the manufacturer's site.
But, you couldn't order it there it either. The details in the listing don't match the listing header. The photo shows five tubes and there is not
way to pick what one will be sent. There is no place to write the manufacture and we know how well Amazon customer service will do with this.
I could just order it and keep my fingers crossed, but then there is three week wait as well. So, wait three weeks, send it back to Amazon... no, that
won't work either.
Since I've rearranged my search query to include the word quartz I have found a great deal more. So, I'm closing in!
[Edited on 9-19-2018 by JScott]
|
|
JScott
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 51
Registered: 23-8-2018
Member Is Offline
|
|
SO exicited!
Hmmmm, seems as though I may be talking to myself at this point, but if anyone else is looking for a tube like this...
I ordered it, used the item number from the Amazon listing on the manufactures site and it looks like Amazon will ship a tube with the correct
configuration.
Says it will take 3-4 weeks...hmmm. Making them one at a time perhaps? ;-)
Can't wait to post a photo of my newly acquired tube!
|
|
Ubya
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1247
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline
Mood: I'm a maddo scientisto!!!
|
|
happy to see that in the end you succeeded
---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------
|
|
JScott
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 51
Registered: 23-8-2018
Member Is Offline
|
|
I followed the link you sent me Perkin Elmer. They sell through Amazon also.
Thanks for your help!
|
|
Amos
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1406
Registered: 25-3-2014
Location: Yes
Member Is Offline
Mood: No
|
|
What compound of Iron(III) are you trying to reduce? Any salt can be reduced in aqueous solution just by adding metallic iron and stirring.
|
|
morganbw
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 561
Registered: 23-11-2014
Member Is Offline
Mood: No Mood
|
|
@JScott
I bought a few pieces of quartz tubing from deschem. I have a somewhat similar use for the quartz tubes as you. I probably will attempt to make AlCl3
using one of them sometime in the future.
This was the description.
[[[
500mm, Quartz Glass Tube, OD 18mm,1.5mm Thick, Made From Fused Silica,3Pcs/Lot
Total Length is 500mm
Outer Diameter is 18mm
Inner Diameter is 15mm
Thickness is 1.5mm
]]]
Made From Quartz Glass
Quantity:3 pcs/Lot
[Edited on 23-9-2018 by morganbw]
|
|
WGTR
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 971
Registered: 29-9-2013
Location: Online
Member Is Offline
Mood: Outline
|
|
Have you tried using borosilicate tubing yet, just to see if it would work? Also, I don't think you need to go through the trouble of making hydrogen
for this.
For simple (and small-scale) metal oxide reductions, I've used a 2 foot long borosilicate tube that is bent into an "L" shape a few inches from one
end. The tube is mounted at a slight angle in a stand, so that some powder can be placed into the long end of the tube without it sliding down by
itself. The bent end of the tube faces upward. This gives a low spot at the bottom of the "L", and here is placed a few ml of alcohol.
Any kind of inert gas can be bubbled through this; I've used nitrogen before. It evaporates some alcohol and carries the vapor over the oxide to be
reduced. A propane torch can be used to heat the powder. Copper oxide is very simple to reduce this way. You only need 200-300°C to make it work.
Higher temperatures will readily cause the copper powder to sinter together.
I've never tried alcohol for reducing iron oxide. Perhaps there could be some inclusion of carbon into the iron, but otherwise it should reduce it
just fine, although at a higher temperature. Keep in mind that hot iron will react with water to produce hydrogen again. The gasses have to be
absolutely dry. While iron is being reduced water is a product, and this will have to be continually flushed away to bring the reaction to
completion.
[Edited on 9-23-2018 by WGTR]
|
|
JScott
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 51
Registered: 23-8-2018
Member Is Offline
|
|
Sorry, it's been a few days since I checked this post. I'm not getting email notification of the responses, sorry if I was rude.
I watched this video nearly three weeks ago (that got me interested). I can't tell you how frustrated I am that I haven't been able to find it since.
It was the observations of the color of the burning hydrogen at the end of the tube I found most interesting. I wanted to explore this some, just to
satisfy my own personal curiosity. I love watching the videos, sometimes that's enough, there are times when I just say "I have to do that!" I have no
better explanation.
One of the things that fascinates me the most about this hobby are the techniques. I love learning about and performing various laboratory techniques.
In this case I am less interested in the reduction of iron and more interested in the flooded gas environment and what can be done there. I've watched
copper metal formed from copper compounds in a similar manner. It's the technique, not the end result in this case.
I am fairly sure it was hematite. This is NOT the video, but it is now the only one I can find that's even similar. So, I would love to show the video as a reference to what I am
trying to describe, but alas I have lost my way.
On the borosilicate tubing, I guess I just assumed that if the quartz tube got bright orange it would be enough heat to melt normal lab glass. In
fact I have not tried this with borosilicate glass.
Oh, and I did price plain jane quartz tubing but it wasn't much cheaper than this 'made to order' (no kidding) tube.
[Edited on 9-28-2018 by JScott]
[Edited on 9-28-2018 by JScott]
[Edited on 9-28-2018 by JScott]
[Edited on 9-28-2018 by JScott]
|
|
JScott
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 51
Registered: 23-8-2018
Member Is Offline
|
|
Wrong tube sent!
Dammit! After all of that I get sent a plain old quartz tube. I COULD SCREAM! There that's better.
UPS will by in the AM to take it back.
Back where I started!
|
|